Two-dimensional BMD, BSF, ring-OISF and COP distributions in a dislocation-free ingot grown by the NOC method
Source abstract
Abstract
The noncontact crucible (NOC) method has a large and deep low-temperature region in Si melt to grow a uniform large Si single ingot. The theoretical simulation pointed out that the lowest vacancy or interstitial Si atom area appears in the region with the smaller ratio between temperature gradients at melt surface and growing interface. The growth condition to obtain this region is suitable for the NOC method. The quality of a NOC ingot was first evaluated by determining the distribution of bulk micro defect (BMD), bulk stacking fault (BSF), oxidation induced stacking fault (OISF) and crystal originated particle (COP) in the cross section of the dislocation-free ingot. A ring-OISF or BSF can be clearly observed on the cross section cut from the middle and tail parts of the ingot. BMD can be observed inside and outside the ring-OISF. By estimated comparison to the none-doping case, CV (= CI) at cross point clearly has a trend to increase for the high B-doing case (5 × 10 19 cm −3), where C V and C I are concentration of vacancy and interstitial Si atom, respectively. Nevertheless, in comparison with the distribution of COP in Cz and NOC ingots, COP cannot be detected inside the ring-OISF in the NOC wafer under the same etching process as many COP can be observed in the Cz wafer. This may be a unique feature for NOC growth.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Silicon and Solar Cell Technologies · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Nakajima · J. Crystal Growth · 2012 · 344 · 610.1016/j.jcrysgro.2012.01.051 ↗
2. Nakajima · J. Crystal Growth · 2012 · 355 · 3810.1016/j.jcrysgro.2012.06.034 ↗
3. Nakajima · J. Crystal Growth · 2013 · 372 · 12110.1016/j.jcrysgro.2013.03.024 ↗
4. Nakajima · Jpn. J. Appl. Phys. · 2014 · 53 · 025501-110.7567/JJAP.53.025501 ↗
5. Nakajima · J. Crystal Growth · 2014 · 389 · 11210.1016/j.jcrysgro.2013.12.006 ↗
6. Nakajima · J. Crystal Growth · 2014 · 405 · 4410.1016/j.jcrysgro.2014.07.024 ↗
7. Nakajima · Jpn. J. Appl. Phys. · 2015 · 54 · 015504-1
8. Nakajima · J. Electron. Materials · 2016 · 45 · 283710.1007/s11664-016-4463-z ↗
9. Nakajima · J. Crystal Growth · 2017 · 468 · 70510.1016/j.jcrysgro.2016.10.039 ↗
10. Nakajima · J. Crystal Growth · 2018 · 499 · 5510.1016/j.jcrysgro.2018.07.031 ↗
11. Nakajima · J. Crystal Growth · 2019 · 52410.1016/j.jcrysgro.2019.125160 ↗
12. Czochralski · Zeitschrift Physikalische Chem. · 1917 · 92 · 219
13. Nakajima · J. Crystal Growth · 2020 · 54710.1016/j.jcrysgro.2020.125810 ↗
14. Nakajima · J. Crystal Growth · 2022 · 59210.1016/j.jcrysgro.2022.126721 ↗
15. ScienceDirect10.1016/j.egypro.2016.07.075 ↗
16. Kern · J. Electrochem. Sci. · 1990 · 137 · 188710.1149/1.2086825 ↗
17. K. Nakamura, Doctoral thesis for Tohoku University, “Study of Diffusion of Point Defects in a Single Crystal of Silicon during Growth Process and Formation of Secondary Defects”, 2002.10.1016/S0022-0248(01)02323-5 ↗
18. Ohashi · Shin-Nittetsu Technical Report · 2000 · 373 · 2
19. Voronkov · J. Appl. Phys. · 1999 · 86 · 597510.1063/1.371642 ↗
20. Voronkov · J. Appl. Phys. · 2000 · 87 · 412610.1063/1.373040 ↗
21. K. Nakamura, R. Suewaka, T. Saishoji, J. Tomioka, Proceedings of the Forum on the Science and Technology of Silicon Materials 2003, Nov. 25-27, Japan, p.161 (2003).