journal article·2008-05

Solidification behavior of falling germanium droplets produced by pulsated orifice ejection method

Satoshi Masuda, Kenta Takagi, Wei Dong, Kenta Yamanaka, Akira Kawasaki

Journal of Crystal Growth· Volume 310· Issue 11
Publisher page

Abstract

In order to clarify containerless solidification mechanism of falling semiconductor microdroplets, the monosized droplets of germanium in the size range from 200 to 500 μm were ejected by pulsated orifice ejection apparatus method. The density of grains in the resultant particles was dramatically reduced by decreasing the ejection temperature, i.e. initial temperature. A surface observation and orientation imaging microscopy analysis proposed that such microstructural transition was derived from the dependency of preferred growth direction on the undercooling level: the initial temperature determined the solidification undercooling. Numerical calculation with the classical nucleation theory was performed to discuss this phenomenon, but could not sufficiently elucidate the effect of initial temperature obtained experimentally.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Solidification and crystal growth phenomena · Material Dynamics and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. A. Ishikawa, Spherical shaped semiconductor integrated circuit, United States Patent, No. 5,955,776, September 21, 1999.
2. N. Takeda, in: Proceedings of the MEMS2000, Miyazaki, Japan, 2000, p. 11.
3. Minemoto · Jpn. J. Appl. Phys. · 2005 · 7A · 482010.1143/JJAP.44.4820 ↗
4. Omae · Sol. Energy Mater. Sol. Cells · 2006 · 90 · 361410.1016/j.solmat.2006.06.056 ↗
5. Kuzuoka · J. Crystal Growth · 2007 · 304 · 48710.1016/j.jcrysgro.2007.02.030 ↗
6. Li · J. Mater. Sci. · 1997 · 32 · 143710.1023/A:1018593615171 ↗
7. Nagashio · Jpn. J. Appl. Phys. · 2006 · 45 · 62310.1143/JJAP.45.L623 ↗
8. Kawasaki · 2001
9. Takagi · Mater. Trans. · 2006 · 47 · 138010.2320/matertrans.47.1380 ↗
10. Nagashio · Acta Mater. · 2005 · 53 · 302110.1016/j.actamat.2005.03.022 ↗
11. Aoyama · Acta Mater. · 2000 · 48 · 373910.1016/S1359-6454(00)00164-6 ↗
12. Aoyama · Mater. Sci. Eng. A · 2001 · 304–306 · 23110.1016/S0921-5093(00)01494-5 ↗
13. Nagashio · Metall. Mater. Trans. A · 2005 · 36A · 340710.1007/s11661-005-0014-6 ↗
14. Devaud · Acta Metall. · 1987 · 35 · 76510.1016/0001-6160(87)90202-1 ↗
15. Brandon · Acta Metall. · 1966 · 14 · 147910.1016/0001-6160(66)90168-4 ↗
16. Lin · Scripta Metall. · 1997 · 36 · 114510.1016/S1359-6462(97)00010-9 ↗
17. Hirth · Metall. Trans. A · 1978 · 9A · 40110.1007/BF02646391 ↗
18. 1993
19. 2000
20. Turnbull · Contemp. Phys. · 1969 · 10 · 47310.1080/00107516908204405 ↗
21. Iida · 1988
22. Li · Europhys. Lett. · 1996 · 34 · 42310.1209/epl/i1996-00473-7 ↗
23. Markov · 2003
24. Sato · High Temp. High Pressure · 2000 · 32 · 25310.1068/htwu265 ↗
25. Willnecker · Mater. Sci. Eng. · 1988 · 98 · 8510.1016/0025-5416(88)90132-2 ↗
26. Thompson · Acta Metall. · 1983 · 31 · 202110.1016/0001-6160(83)90019-6 ↗
27. Fujino · ISIJ Int. · 1997 · 37 · 110710.2355/isijinternational.37.1107 ↗