Bulk AlN crystal growth by direct heating of the source using microwaves
Source abstract
Abstract
Abstract AlN single crystal platelets up to 2×3 mm 2 and needles 1 mm in diameter and 3 mm in length were successfully grown by directly heating the source materials with microwaves. The process temperature was over 2000°C and the pressure was kept constant at 910 Torr. The growth rate was typically 300 μm h −1 in the c -direction. An emission around 5.5 eV was observed in the photoluminescence spectrum probably caused by magnesium impurity. The dislocation density was low, 6×10 3 cm −2 , as determined by both synchrotron white beam X-ray topography and etching in molten potassium hydroxide–sodium hydroxide eutectic alloy. Etching produced hexagonal pits and hexagonal hillocks on the Al- and N-polar surfaces, respectively. Raman spectra, X-ray topograph, and etch pit densities demonstrate that the crystals have good structural quality.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: GaN-based semiconductor devices and materials · Acoustic Wave Resonator Technologies · ZnO doping and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Mukai · J. Phys. Condes. Matter · 2001 · 13 · 708910.1088/0953-8984/13/32/314 ↗
2. Ambacher · J. Phys. D · 1998 · 31 · 265310.1088/0022-3727/31/20/001 ↗
3. 1994
4. Kuball · IEEE Electron Dev. Lett. · 2002 · 23 · 710.1109/55.974795 ↗
5. Slack · J. Crystal Growth · 1976 · 34 · 26310.1016/0022-0248(76)90139-1 ↗
6. Liu · J. Crystal Growth · 2000 · 220 · 24310.1016/S0022-0248(00)00841-1 ↗
7. Katz · Annu. Rev. Mater. Sci. · 1992 · 22 · 15210.1146/annurev.ms.22.080192.001101 ↗
8. Francis · J. Electrochem. Soc. · 1976 · 123 · 43010.1149/1.2132844 ↗
9. Huey · Ceram. Eng. Sci. Proc. · 2000 · 21 · 59910.1002/9780470294635.ch71 ↗
10. Harris · J. Mater. Res. · 1990 · 5 · 176310.1557/JMR.1990.1763 ↗
11. McNeil · J. Am. Ceram. Soc. · 1993 · 76 · 113210.1111/j.1151-2916.1993.tb03730.x ↗
12. Kuokstis · Appl. Phys. Lett. · 2002 · 81 · 275510.1063/1.1510586 ↗
13. Slack · J. Phys. Chem. Solids · 1987 · 48 · 64110.1016/0022-3697(87)90153-3 ↗
14. Tang · Appl. Phys. Lett. · 1998 · 72 · 150110.1063/1.121039 ↗
15. Li · Appl. Phys. Lett. · 2002 · 81 · 336510.1063/1.1518558 ↗
16. Nam · Appl. Phys. Lett. · 2002 · 82 · 169410.1063/1.1559659 ↗
17. Nam · Appl. Phys. Lett. · 2002 · 83 · 87810.1063/1.1594833 ↗
18. Kuball · Surf. Interface Anal. · 2001 · 31 · 98710.1002/sia.1134 ↗
19. Kuball · Appl. Phys. Lett. · 2000 · 77 · 195810.1063/1.1311948 ↗
20. Hayes · Jpn. J. Appl. Phys. · 2000 · 39 · L71010.1143/JJAP.39.L710 ↗
21. Davydov · Phys. Rev. B · 1998 · 58 · 1289910.1103/PhysRevB.58.12899 ↗
22. Weyher · J. Crystal Growth · 2000 · 210 · 15110.1016/S0022-0248(99)00669-7 ↗
23. Kamler · J. Crystal Growth · 2002 · 246 · 2110.1016/S0022-0248(02)01786-4 ↗
24. Weyher · Phys. Stat. Sol. c · 2003 · 0 · 82110.1002/pssc.200306248 ↗
25. Zhuang · MRS Int. J. Nitride Semicond. Res. · 2002 · 7 · 410.1557/S1092578300000302 ↗
26. Shi · MRS Internet J. Nitride Semicond. Res. · 2001 · 6 · 510.1557/S109257830000017X ↗
27. D. Zhuang, J.H. Edgar, B. Strojek, J. Chaudhuri, Z. Rek, J. Crystal Growth 262 (2004) 89.10.1016/j.jcrysgro.2003.10.051 ↗