Crystal growth of the Pr2PdSi3 intermetallic compound
Source abstract
Abstract
Abstract Pr 2 PdSi 3 single crystals were grown by a vertical floating zone method with radiation heating at a zone traveling rate of 3 mm/h. The compound exhibits congruent melting behavior at a liquidus temperature of about 1770 °C. The slightly Pd-depleted composition of the crystal, with respect to the nominal Pr 2 PdSi 3 stoichiometry, led to gradual accumulation of Pd in the traveling zone and to a decreasing operating temperature during the growth process. Thin platelet-like precipitates of a PrSi phase were detected in the crystal matrix. Single crystalline samples exhibit a huge anisotropy due to the crystal electric field effect and order antiferromagnetically below the Neel temperature T N =2.17 K. The [1 1 0] orientation was identified as the magnetic easy axis at room temperature. At lower temperature (∼20 K) magnetic easy and hard axes interchange with each other. Two additional magnetic phase transitions are observed at temperatures below 1 K.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Rare-earth and actinide compounds · Magnetic and transport properties of perovskites and related materials · Magnetic Properties of Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Kotsandis · J. Magn. Magn. Mater. · 1990 · 87 · 19910.1016/0304-8853(90)90215-C ↗
2. Mallik · Solid State Commun. · 1998 · 106 · 16910.1016/S0038-1098(98)00012-X ↗
3. Saha · Phys. Rev. B · 1999 · 60 · 1216210.1103/PhysRevB.60.12162 ↗
4. Saha · Phys. Rev. B · 2000 · 62 · 42510.1103/PhysRevB.62.425 ↗
5. Behr · J. Cryst. Growth · 2002 · 237–239 · 197610.1016/S0022-0248(01)02294-1 ↗
6. Graw · J. Alloys Compd. · 2000 · 308 · 19310.1016/S0925-8388(00)00894-X ↗
7. Behr · Cryst. Res. Technol. · 2000 · 35 · 46110.1002/1521-4079(200004)35:4<461::AID-CRAT461>3.0.CO;2-D ↗
8. Sampathkumaran · Phys. Rev. B · 2002 · 66 · 5240910.1103/PhysRevB.66.052409 ↗
9. Mazilu · J. Cryst. Growth · 2005 · 275 · e10310.1016/j.jcrysgro.2004.10.134 ↗
10. Behr · J. Cryst. Growth · 2008 · 310 · 226810.1016/j.jcrysgro.2007.11.227 ↗
11. Majumdar · Phys. Rev. B · 2000 · 62 · 1420710.1103/PhysRevB.62.14207 ↗
12. Majumdar · Phys. Rev. B · 2001 · 64 · 01241810.1103/PhysRevB.64.012418 ↗
13. Frontzek · J. Magn. Magn. Mater. · 2006 · 301 · 39810.1016/j.jmmm.2005.07.016 ↗
14. Frontzek · Physica B · 2004 · 350 · e18710.1016/j.physb.2004.03.050 ↗
15. Szytula · J. Magn. Magn. Mater. · 1999 · 202 · 36510.1016/S0304-8853(99)00410-2 ↗
16. Jensen · 1991
17. Pearson’s Handbook of Crystallographic Data for Intermetallic Phases
18. Mazilu · J. Alloys Compd. · 2008 · 454 · 22110.1016/j.jallcom.2007.01.044 ↗
19. Souptel · J. Cryst. Growth · 2007 · 300 · 53810.1016/j.jcrysgro.2006.12.042 ↗
20. M. Frontzek, Thesis, Technische Universität Dresden 2009.
21. Frontzek · J. Phys.: Condens. Matter · 2007 · 19 · 14527610.1088/0953-8984/19/14/145276 ↗