journal article·2017-02

Effects of supersaturation on pore shape in solid

P.S. Wei, S.Y. Hsiao

Publisher page

Abstract

Abstract The shape of a pore resulting from a bubble entrapped by a solidification front with different supersaturation ratios is predicted in this work. Supersaturation ratio, representing the ratio between solute concentration and saturation solute concentration, determines nucleation of a bubble and development of the pore shape in the early stage. Pore formation and its shape in solid influence contemporary issues of biology, engineering, foods, geophysics and climate change, etc. This work extends and combines previous models accounting for realistic mass and momentum transport, and physico-chemical equilibrium of solute gas across the bubble cap to self-consistently determine shape of the bubble cap beyond the solidification front and the pore shape in solid. The study also deal with that pore formation can be resulted from three different mechanisms, depending on the directions and magnitude of solute gas transport across the bubble cap. Case 1 is subject to solute transport from the pore across the cap into the surrounding liquid in the early stage. Cases 2a and 2b indicate opposite direction of solute transport. In contrast to Case 2b, the effect of solute transport on solute gas pressure in the pore in Case 2a is stronger than that of pore volume expansionin the last stage. The results find that an increase in supersaturation ratio decreases pore radius and time for bubble entrapment in Case 1. The bubble cannot be entrapped in Case 2. The predicted pore shape in solid agrees with experimental data. Understanding, prediction and control of the growth of the pore shape have therefore been obtained.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Pickering emulsions and particle stabilization · Calcium Carbonate Crystallization and Inhibition · Heat and Mass Transfer in Porous Media

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Kou · 1987
2. Artificial dispersal of void patterns in unidirectional freezing10.1080/08916159308946466 ↗
3. Effect of welding variables and solidification substructure on weld metal porosity10.1007/BF02652328 ↗
4. Current issues and problems in laser welding of automotive aluminum alloys10.1179/095066099101528298 ↗
5. Study of the gas inclusions in Al2O3/Y3Al5O12 and Al2O3/Y3Al5O12/ZrO2 eutectic fibers grown by laser floating zone10.1016/j.jcrysgro.2007.02.042 ↗
6. Modification and enhancement of cryogenic quenching heat transfer by a nanoporous surface10.1016/j.ijheatmasstransfer.2014.09.056 ↗
7. Solidification researches using transparent model materials - a review10.1007/s11431-011-4689-1 ↗
8. Microstructure characteristics of the model spring steel 51CrV4
9. The effect of Ar and N2 shielding gas on laser weld porosity in steel, stainless steels, and nickel
10. Fabrication, properties and application of porous metals with directional pores10.1016/j.pmatsci.2006.09.001 ↗
11. Influence of ultrasonic agitation on pore formation and growth during unidirectional solidification of water-carbon dioxide solution10.2320/matertrans.47.2183 ↗
12. Gas-storage ice grown form water containing mircobubbles10.1016/j.ijrefrig.2008.08.008 ↗
13. Frozen ponds: production and storage of methane during the arctic winter in a lowland tundra landscape in northern Siberia, Lena River Delta10.5194/bg-12-977-2015 ↗
14. Exact solution of the problem of gas segregation in the process of crystallization10.1016/S0017-9310(02)00349-6 ↗
15. Nucleation of bubbles on a solidification front-experiment and analysis10.1007/s11663-003-0078-x ↗
16. A stochastic model for nucleation in the boundary layer during solvent freeze-concentration10.1021/cg401172z ↗
17. Evaluation of porosity in lotus-type porous magnesium fabricated by metal/gas eutectic unidirectional solidification10.1016/j.msea.2005.03.107 ↗
18. Effect of transference velocity and hydrogen pressure on porosity and poremorphology of lotus-type porous copper fabricated by a continuous casting technique10.1016/j.actamat.2007.06.022 ↗
19. Formation of pores during unidirectional solidification of water containing carbon dioxide10.2320/matertrans.43.2582 ↗
20. Growth of spherical and cylindrical oxygen bubbles at an ice-water interface10.1021/cg070251k ↗
21. Particle capture in binary solidification10.1017/S0022112008005570 ↗
22. Air bubbles in ice10.1088/0370-1328/77/3/327 ↗
23. Evaluation of porosity in porous copper fabricated by unidirectional solidification under pressurized hydrogen10.1016/S0921-5093(01)01263-1 ↗
24. Metal/gas eutectic growth during unidirectional solidification10.1007/BF02586119 ↗
25. Evaluation of porosity in lotus-type porous Cu fabricated with GASAR process
26. A comprehensive model of ordered porosity formation10.1016/j.actamat.2007.08.008 ↗
27. Modelling of structural formation in ordered porosity metal materials10.1088/0965-0393/14/4/009 ↗
28. Shape of a pore trapped in solid during solidification10.1016/S0017-9310(99)00134-9 ↗
29. An analytical self-consistent determination of a bubble with a deformed cap trapped in solid during solidification10.1007/s11663-002-0089-z ↗
30. On the shape of small sessile and pendant drops by singular perturbation techniques10.1017/S0022112091000587 ↗
31. The cycle of bubble production from a gas cavity in a supersaturated solution10.1016/S0001-8686(98)00075-X ↗
32. Effect of step-wise change in processing pressure on isolated pore growth during controlled directional solidification in small channels10.1016/j.jcrysgro.2008.11.055 ↗
33. Evolution of elongated pores at the melt-solid interface during controlled directional solidification10.1016/j.actamat.2013.03.006 ↗
34. Microbubble or pendant drop control described by a general phase diagram10.1016/j.ijheatmasstransfer.2008.08.021 ↗
35. Growths of bubble/pore sizes in solid during solidification -an in situ measurement and analysis10.1016/j.jcrysgro.2004.06.039 ↗
36. Pore shape development from a bubble captured by a solidification front10.1016/j.ijheatmasstransfer.2012.08.054 ↗
37. Pore formation from bubble entrapment by a solidification front