Orientational control of CeO2 films on sapphire substrates grown by magnetron sputtering

S. Yamamoto, M. Sugimoto, H. Koshikawa, T. Hakoda, T. Yamaki

Abstract

Abstract The effect of deposition temperature and post-annealing on the crystallographic orientation of cerium dioxide (CeO 2 ) films on sapphire (α-Al 2 O 3 ) substrates were investigated. CeO 2 films, with thickness of 17 nm, were grown on c-plane and r-plane sapphire substrates by radiofrequency (rf) magnetron sputtering. Deposition temperatures between 150 and 500 °C were used with a sintered CeO 2 target in an Ar–O 2 gas mixture. The post-annealing treatment was performed in air at various temperatures ranging from 400 to 1000 °C. The films were characterized by X-ray diffraction, atomic force microscopy, and Rutherford backscattering spectroscopy. X-ray diffraction studies revealed that the orientation of the CeO 2 films changed from (001) to mixed (001)/(111) and then to (111), with increasing deposition temperatures on both the c-plane and r-plane sapphire substrates. Post-annealing at 1000 °C improved the degree of crystallinity of the films, and formed rectangular grains. The results suggest that control of the deposition and post-annealing temperatures provides orientation-controlled CeO 2 films on c- and r-plane sapphire substrates.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Catalytic Processes in Materials Science · ZnO doping and properties · Gas Sensing Nanomaterials and Sensors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Large-area epitaxial CeO2 buffer layers on sapphire substrates for the growth of high quality YBa2Cu3O7 films10.1016/0040-6090(93)90040-V ↗
2. Epitaxial CeO2 buffer layers for YBa2Cu3O7−δ films on sapphire10.1063/1.354650 ↗
3. High crystalline quality CeO2 buffer layers epitaxied on (1102) sapphire for YBa2Cu3O7 thin films10.1016/S0022-0248(97)00857-9 ↗
4. Cerium oxide (CeO2) buffer layers for preparation of high-Jc YBCO films on large-area sapphire substrates (30cm×10cm) by coating pyrolysis10.1016/j.physc.2004.01.164 ↗
5. Defect induced magnetic transition in Co doped CeO2 sputtered thin films10.1016/j.ceramint.2016.04.091 ↗
6. Room temperature ferromagnetism of Ni doped cerium oxide single crystalline thin Films deposited by using rf magnetron sputtering10.1016/j.matlet.2015.09.102 ↗
7. Enhancement of room temperature ferromagnetic behavior of rf sputtered Ni-CeO2 thin films10.1016/j.apsusc.2016.08.166 ↗
8. Role of cerium oxide in the enhancement of activity for the oxygen reduction reaction at Pt-CeOx nanocomposite electrocatalyst - An in situ electrochemical X-ray absorption fine structure study10.1021/jp301509t ↗
9. Defect structure analysis of heterointerface between Pt and CeOx promoter on Pt electro-catalyst10.1021/am507754w ↗
10. Growth and recrystallization of CeO2 thin films deposited on R-plane sapphire by off-axis RF sputtering10.1016/S0022-0248(00)00585-6 ↗
11. Pulsed laser deposition of epitaxial buffer layers on LiNbO3
12. Heteroepitaxial growth of CeO2(001) films on Si(001) substrates by pulsed laser deposition in ultrahigh vacuum10.1143/JJAP.30.L1136 ↗
13. Deposition of CeO2 films including areas with the different orientation and sharp border between them10.1016/0040-6090(95)08201-8 ↗
14. Crystalline quality and surface morphology of (100) CeO2 thin films grown on sapphire substrates by solid source metalorganic chemical vapor deposition10.1016/0022-0248(95)00253-7 ↗
15. The influence of substrate temperature on the optical and micro structural properties of cerium oxide thin films deposited by10.1016/j.spmi.2015.05.041 ↗
16. Effect of rf power on the properties of magnetron sputtered CeO2 thin films10.1007/s10854-015-2761-5 ↗
17. Epitaxial growth of cerium oxide thin film buffer layers deposited by d.c. magnetron sputtering10.1016/S0040-6090(01)00839-2 ↗
18. Growth of CeO2 films on sapphire and MgO by rf magnetron sputtering10.1111/j.1151-2916.1995.tb08920.x ↗
19. Fabrication and characterization of a CeO2 buffer layer on c-plane and tilt-c-plane sapphire substrates10.1016/S0921-4534(03)00993-6 ↗
20. Influence of growth rate on the epitaxial orientation and crystalline quality of CeO2 thin films grown on Al2O3(0001)10.1063/1.3525558 ↗
21. Growth of epitaxial CeO2 thin films on r-cut sapphire by molecular beam epitaxy10.1016/j.physc.2003.08.007 ↗
22. How r-plane Al2O3 surface modifications impact the growth of epitaxial (001) CeO2 thin films10.1007/s11664-009-0864-6 ↗
23. Growth and characterization of CeO2 films on sapphire substrates by sputtering process10.1143/JJAP.35.5805 ↗
24. (001) and (111) single-oriented highly epitaxial CeO2 thin films on r-cut sapphire substrates10.1007/s11664-015-3728-2 ↗
25. Growth of high-quality YBa2Cu3O7−x films on CeO2 buffer of mixed (001)/(111) orientation on sapphire10.1063/1.114305 ↗
26. Comparative studies of nanostructural and morphological evolution of CeO2 thin films induced by high-temperature annealing10.1088/0957-4484/18/16/165605 ↗
27. Nie · Physica C · 2007 · 460–462 · 135310.1016/j.physc.2007.04.023 ↗