journal article·2020-05Open access

Photo-oxidative degradation of injection molded sepiolite/polyamide66 nanocomposites

C. Fernández-Barranco, A. Yebra-Rodríguez, J. Jiménez-Millán, F.J. Navas-Martos, A. Yebra, A.E. Koziol, M.D. La Rubia

Abstract

Every day clay/polymer nanocomposites are included in more industrial applications, due to its high performance. Because of this, nanocomposites may be submitted to extreme conditions of work, which could degrade it. Exposure to solar radiation in the presence of oxygen (photo-degradation) represents one of the major problems of the Clay/Polymer anocomposites. In this study, samples of neat polyamide 66 (PA66-S-0) and reinforced nanocomposites with 1, 3, 5, 7 and 9 wt% organophilized sepiolite (PA66-S-1, PA66-S-3, PA66-S-5, PA66-S-7 and PA66-S-9 samples) are analysed after UV exposure, following the standard accelerated degradation method UNE-EN-ISO 4892-2. The aim of this study is to establish the effect of UV exposure on the mechanical, optical and crystallographic properties of the new material. Tensile tests show a reduction in the ductility and an embrittlement after degradation process. In addition, an increase of transparency is confirmed with the UV exposure. The carbonyl index in the samples containing sepiolite is lower than in neat PA66 whereas the yellowness index is not affected by degradation. Sepiolite has an inhibitor effect on the formation of C=O bonds. These results indicate that breaking of chains of PA66 starts in the amorphous region and that it is lower in the nanocomposites due to the low diffusion of oxygen induced by the sepiolite. This affirmation is corroborated by the obtained diffraction patterns.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Polymer Nanocomposites and Properties · biodegradable polymer synthesis and properties · Polymer Nanocomposite Synthesis and Irradiation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Polylactic acid and polylactic acid-based nanocomposite photooxidation10.1021/bm1006773 ↗
2. The crystal structures of two polyamides (“nylons”)
3. Influence of functional nanoparticles on the photostability of polymer materials: recent progress and further applications10.1016/j.polymdegradstab.2013.06.009 ↗
4. Poly(vinyl alcohol)/chitosan/montmorillonite nanocomposites for food packaging applications: Influence of montmorillonite content10.1177/0954008315617231 ↗
5. MALDI investigation of the photooxidation of nylon6610.1021/ma049521n ↗
6. New vistas in the photo-oxidation of nylon 610.1021/ma0344137 ↗
7. Sepiolite based materials for the photo- and thermal stabilization of pesticides10.1016/S0169-1317(01)00030-8 ↗
8. Thermal-oxidative degradation of polyamide 6,6 containing metal salts10.1016/j.polymdegradstab.2010.08.014 ↗
9. Comparision of photo-oxidative degradation of polyamide 6,6 films stabilized with HALS and CuCl2 + KI mixtures10.1016/j.polymer.2005.03.065 ↗
10. CIE Publication 15:1970 · 1970
11. CIE Publication 15:1986 · 1986
12. CIE · 2004
13. Photo-oxidation behaviour of polyethylene/polyamide 6 blends filled with organomodified clay: Improvement of the photo-resistance through morphology modification10.1016/j.polymdegradstab.2009.12.021 ↗
14. Influence of temperature on the thermo-oxidative degradation of polyamide 6 films10.1016/j.polymdegradstab.2010.02.030 ↗
15. Mechanical and crystallographic properties of injection-molded polyamide 66/sepiolite nanocomposites with different clay loading10.1002/pc.23146 ↗
16. Study of spatial distribution of sepiolite in polyamide 66/sepiolite nanocomposites10.1016/j.clay.2016.04.015 ↗
17. Structural characterization of sepiolite/polyamide6,6 nanocomposites by means of static and dynamic thermal methods10.1016/j.clay.2017.12.025 ↗
18. Color difference thesholds in dental ceramics10.1016/j.jdent.2010.07.008 ↗
19. Polymer nanocomposites from modified clays: recent advances and challenges10.1016/j.progpolymsci.2015.10.001 ↗
20. Melt crystallized polyamide 6.6 and its copolymers, part I. Melting point – Lamellar thickness relations in the homopolymer10.1016/j.eurpolymj.2007.01.051 ↗
21. Thermal decomposition of aliphatic nylons10.1002/(SICI)1097-0126(199907)48:7<532::AID-PI214>3.0.CO;2-R ↗
22. On the pho-oxidation of aliphatic polyamides
23. Clay–polymer nanocomposites: Progress and challenges for use in sustainable water treatment10.1016/j.jhazmat.2019.121125 ↗
24. Twenty years of polymer-clay nanocomposites10.1002/mame.200600260 ↗
25. Effect of UV irradiation on thermal properties of nanocomposites based on polylactide10.1007/s10973-014-4103-x ↗
26. An overview on the degradability of polymer nanocomposites10.1016/j.polymdegradstab.2004.09.013 ↗
27. Usefulness of cathode ray tube color displays in chromaticity–discrimination experiments10.1364/AO.39.004021 ↗
28. Nanocomposites: industrial opportunity or challenge?10.1016/j.polymdegradstab.2009.11.019 ↗
29. The influence of interlayer cations on the photo-oxidative degradation of polyethylene/montmorillonite composites10.1002/polb.20068 ↗
30. Photo-oxidative degradation of polypropylene/montmorillonite nanocomposites10.1016/j.polymer.2005.01.087 ↗
31. Photo-oxidation of polystyrene/clay nanocomposites under accelerated UV exposure: effect on the structure and molecular weight10.1002/app.29806 ↗
32. Preparation and characterization of poly(vinyl alcohol)/modified clay electrospun nanocomposite nanofibrous mats for microbial protection
33. Photo-oxidative degradation of nylon 66 under accelerated weathering10.1016/S0032-3861(97)10390-1 ↗
34. Photo-irradiation induced morphological changes in nylon 6610.1016/S0032-3861(00)00374-8 ↗
35. Torikai · J. Appl. Polym. Sci. · 1999 · 40 · 163710.1002/app.1990.070400919 ↗
36. Advances in 3d Printing of Thermoplastic Polymer Composites and Nanocomposites10.1016/j.progpolymsci.2019.101162 ↗
37. Crystalline properties of injection molded polyamide-6 and polyamide-6/montmorillonite nanocomposites10.1016/j.clay.2008.07.010 ↗
38. Thermooxidative degradation of injection molded sepiolite/polyamide66 nanocomposites10.1180/minmag.2014.078.5.09 ↗
39. Effect of natural weather on the structure and properties of polylactide/cloisite 30B nanocomposites10.1016/j.polymdegradstab.2010.05.014 ↗