Effects of substrate temperature on the physical properties of strained BaTiO3/LaNiO3 artificial superlattices
Source abstract
Abstract
Abstract An artificially layered perovskite composed of dielectric BaTiO 3 (BTO) and conductive LaNiO 3 (LNO) was grown on a LaNiO 3 -coated SrTiO 3 (0 0 1) single crystal substrate by a radio-frequency magnetron sputtering system. The cross-sectional image of transmission electron microscopy confirmed the formation of BTO/LNO superlattice structure. Moreover, the clearly main feature and satellite features from the (0 0 L ) Bragg reflection of X-ray indicate the high quality of the BTO/LNO superlattice structure was formed on a LaNiO 3 -coated SrTiO 3 substrate. All the superlatttice films deposited at 300–550 °C show a significant enhancement of dielectric constant relative to the BTO single epilayer of the same effective thickness; the higher is the deposition temperature, the larger is the dielectric constant of the films present.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Dielectric properties of ceramics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Tabata · Jpn. J. Appl. Phys. Part 1 · 1995 · 34 · 54410.1143/JJAP.34.544 ↗
2. Liang · J. Appl. Phys. · 2004 · 96 · 58410.1063/1.1759074 ↗
3. Kim · Appl. Phys. Lett. · 2002 · 80 · 358110.1063/1.1477934 ↗
4. Wang · Appl. Phys. Lett. · 2002 · 82 · 288010.1063/1.1569658 ↗
5. Tsurumi · Jpn. J. Appl. Phys. · 1994 · 33 · 519210.1143/JJAP.33.5192 ↗
6. Tsurumi · J. Appl. Phys. · 2002 · 91 · 228410.1063/1.1433180 ↗
7. Tabata · Appl. Phys. Lett. · 1997 · 70 · 32110.1063/1.118202 ↗
8. Wang · J. Electrochem. Soc. · 2000 · 147 · 461510.1149/1.1394111 ↗
9. Koebernik · Thin Solid Films · 2004 · 449 · 8010.1016/j.tsf.2003.10.031 ↗
10. Visinoiu · J. Appl. Phys. · 2002 · 91 · 1015710.1063/1.1478800 ↗
11. Park · Jpn. J. Appl. Phys. Part I · 1996 · 35 · 154810.1143/JJAP.35.1548 ↗
12. Zhang · Jpn, J. Appl. Phys. · 1997 · 362 · 76
13. Matsuoka · J. Appl. Phys. · 1994 · 76 · 176810.1063/1.357694 ↗
14. Wu · Mater. Lett. · 1997 · 33 · 9710.1016/S0167-577X(97)00083-9 ↗
15. Yamada · Appl. Phys. Lett. · 2002 · 81 · 479310.1063/1.1530734 ↗
16. Wakiya · Thin Solid Films · 2002 · 410 · 11410.1016/S0040-6090(02)00238-9 ↗
17. Liang · Thin Solid Films · 2004 · 469–470 · 50010.1016/j.tsf.2004.06.195 ↗
18. Liang · J. Crystal Growth · 2005 · 279 · 11410.1016/j.jcrysgro.2005.02.047 ↗
19. Yang · Appl. Phys. Lett. · 1995 · 66 · 264310.1063/1.113111 ↗
20. Lee · J. Mater. Res. · 1997 · 12 · 316510.1557/JMR.1997.0413 ↗
21. Lin · J. Mater. Res. · 2000 · 15 · 11510.1557/JMR.2000.0020 ↗
22. Liang · J. Electrochem. Soc. · 2005 · 152 · F12910.1149/1.1992387 ↗
23. Shimuta · J. Appl. Phys. · 2002 · 91 · 229010.1063/1.1434547 ↗
24. Li · Appl. Phys. Lett. · 2005 · 97 · 094103
25. Lee · Appl. Phys. Lett. · 2002 · 81 · 47510.1063/1.1489082 ↗
26. Wu · Jpn. J. Appl. Phys. · 1997 · 36 · 116410.1143/JJAP.36.1164 ↗
27. Fuchs · J. Appl. Phys. · 2002 · 91 · 528810.1063/1.1461897 ↗
28. Tabata · Appl. Phys. Lett. · 1994 · 65 · 197010.1063/1.112837 ↗
29. Neaton · Appl. Phys. Lett. · 2003 · 82 · 158610.1063/1.1559651 ↗