Low temperature homoepitaxy of GaN structures by Vapor Liquid Solid transport
Source abstract
Abstract
Abstract Low temperature (500–800 °C) homoepitaxy of not intentionally doped GaN structures on GaN(0 0 0 1)/Si(1 1 1) seed has been investigated by Vapor-Liquid-Solid (VLS) approach. The growth sequence consists in the metalorganic chemical vapor deposition of a network of submicrometric liquid Ga droplets, followed by their nitridation under flowing ammonia diluted either in H 2 or Ar. When nitridation is performed under Ar carrier gas, GaN growth is very difficult to control due to too high N supersaturation within the droplets, despite very low NH 3 flows. Nucleation and growth at the droplets periphery are always favored and, in most cases, high growth rates induce a crust-like growth, forming hollow GaN gangues. The use of H 2 as carrier gas is detrimental to GaN (seed and grown material) stability, for nitridation temperatures ≥700 °C. But, compared to Ar atmosphere, a pronounced decrease of N supersaturation is demonstrated, allowing a better control of the growth mode. This is probably a consequence of a lower thermal decomposition efficiency of NH 3 at the droplets surface. Optimal growth conditions are found at relatively low temperature (600 °C) and NH 3 flow (20 sccm) for which a network of well-separated and faceted epitaxial GaN dots or rings is obtained. The growth mechanisms allowing these results are discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: GaN-based semiconductor devices and materials · Semiconductor materials and devices · Ga2O3 and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Tournier · Adv. Mater. Res. · 2011 · 324 · 4610.4028/www.scientific.net/AMR.324.46 ↗
2. Perez · IEEE Trans. Electron Dev. · 2005 · 52 · 230910.1109/TED.2005.856805 ↗
3. Heera · Appl. Surf. Sci. · 2001 · 184 · 30710.1016/S0169-4332(01)00510-4 ↗
4. Van de Walle · J. Cryst. Growth · 1998 · 189 · 50510.1016/S0022-0248(98)00340-6 ↗
5. Kucheyev · Mater. Sci. Eng. · 2001 · 33 · 5110.1016/S0927-796X(01)00028-6 ↗
6. Nagae · J. Cryst. Growth · 2011 · 324 · 8810.1016/j.jcrysgro.2011.04.022 ↗
7. Lin · J. Cryst. Growth · 2011 · 318 · 45010.1016/j.jcrysgro.2010.10.195 ↗
8. Kato · J. Cryst. Growth · 1994 · 144 · 13310.1016/0022-0248(94)90448-0 ↗
9. Song · J. Appl. Phys. · 2008 · 104 · 06430910.1063/1.2978382 ↗
10. Vézian · J. Cryst. Growth · 2011 · 323 · 32610.1016/j.jcrysgro.2010.10.160 ↗
11. Chen · J. Cryst. Growth · 2011 · 322 · 1510.1016/j.jcrysgro.2011.03.007 ↗
12. Cordier · Mater. Sci. Semcond. Proc. · 2009 · 12 · 1610.1016/j.mssp.2009.07.003 ↗
13. Vo-Ha · Thin Solid Films · 2013 · 548 · 12510.1016/j.tsf.2013.09.030 ↗
14. Jacquier · Phys. Stat. Sol. (c) · 2005 · 2 · 126510.1002/pssc.200460423 ↗
15. H. Baker, H. Okamoto, ASM Handbook Volume 3 Alloy Phase Diagrams 1, ASM International, 1992, p. 148.
16. Suski · Mater. Sci. Eng., B · 1999 · 59 · 110.1016/S0921-5107(98)00402-4 ↗
17. Schupp · J. Cryst. Growth · 2010 · 312 · 323510.1016/j.jcrysgro.2010.07.049 ↗
18. Hu · Appl. Phys. Lett. · 2003 · 82 · 288910.1063/1.1570000 ↗
19. Buckmaster · Microelectron. J. · 2005 · 36 · 45610.1016/j.mejo.2005.02.046 ↗
20. Debnath · J. Cryst. Growth · 2009 · 311 · 338910.1016/j.jcrysgro.2009.04.025 ↗
21. Otsubo · Phys. Status Solidi (c) · 2007 · 4 · 232210.1002/pssc.200674921 ↗
22. Kondo · Phys. Status Solidi (a) · 2006 · 203 · 170010.1002/pssa.200565212 ↗
23. Gherasimova · Appl. Phys. Lett. · 2004 · 85 · 234610.1063/1.1793343 ↗
24. Wu · Appl. Phys. Lett. · 2004 · 85 · 207110.1063/1.1787947 ↗
25. Soueidan · Cryst. Growth Des. · 2008 · 8 · 105110.1021/cg701146m ↗
26. Jacob · Mat. Res. Bull. · 1976 · 11 · 44510.1016/0025-5408(76)90094-5 ↗
27. Koleske · J. Cryst. Growth · 2001 · 223 · 46610.1016/S0022-0248(01)00617-0 ↗
28. Pisch · J. Cryst. Growth · 1998 · 187 · 32910.1016/S0022-0248(98)00006-2 ↗
29. Gerlach · J. Appl. Phys. · 2012 · 111 · 11352110.1063/1.4728166 ↗
30. Cochran · J. Electrochem. Soc. · 1962 · 109 · 14410.1149/1.2425347 ↗
31. Remy · 1960 · 18
32. Imade · Mater. Lett. · 2005 · 59 · 402610.1016/j.matlet.2005.07.063 ↗
33. Sidorenko · Surf. Sci. · 2007 · 601 · 452110.1016/j.susc.2007.04.190 ↗