An ATR-FTIR and ESEM study on magnetic tapes for the assessment of the degradation of historical audio recordings

Federica Bressan, Roberta Bertani, Claudio Furlan, Fabio Simionato, Sergio Canazza

Publisher page

Abstract

Abstract This article presents some approaches for chemical and physical characterization of materials (ATR-FTIR and ESEM) applied to a specific category of cultural material, magnetic tapes. Analogue recording on magnetic tape has been the main technique for capturing sound for about five decades in the past century. Most of our collective memory is therefore stored on this type of medium, which is unfortunately degrading very fast. The past twenty years have witnessed a true rush to digitization in order to save the information stored on tape, but many aspects of the physical recovery of damaged carriers are still performed without solid scientific knowledge, leaving space for improvised treatments with unexpected ill effects. The main motivations for this study are that the preservation of sound recordings is an urgent matter that belongs to the field of Intangible Cultural Heritage preservation, the scientific literature on the subject is scarce and little known by the non-scientific archival world, and the documented approaches to tapes recovery are currently fragmented and do not provide an exhaustive reference for the operators in this field. The analyses presented in this article aim at paving the way for the establishment of a scientific protocol for the safe recovery of damaged tapes.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Diverse Musicological Studies · Conservation Techniques and Studies · Non-Destructive Testing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Camras · 1988
2. Archives in motion: concrete steps towards the digital disclosure of audiovisual content10.1016/j.culher.2011.04.004 ↗
3. Audiovisual production, restoration and content management methods to preserve local tradition and folkloric heritage10.1016/j.culher.2013.05.003 ↗
4. Magnetic tape for data storage: an enduring technology10.1109/JPROC.2008.2004311 ↗
5. Boston · 1998
6. Bogart · 1995
7. Aging of magnetic tape10.1109/TMAG.1980.1060652 ↗
8. Tape degradation factors and challenges in predicting tape life
9. Analysis of audio magnetic tapes with sticky shed syndrome by ATR-FTIR10.1002/app.38364 ↗
10. The safeguard of audio collections: a computer science based approach to quality control in the archive of the Arena di Verona
11. IASA TC-03 · 2005
12. Bigourdan · 2006
13. Rusch · 1963
14. Kinetics of the humid aging of magnetic recording tape10.1109/TMAG.1982.1061957 ↗
15. Degradation of magnetic tape: support and binder stability10.1016/0141-3910(93)90097-3 ↗
16. Casey · 2008
17. Medeiros · 1993
18. Honey, I burnt the tapes! A study on thermal treatment for the recovery of magnetic tapes affected by sticky shed syndrome
19. Temperature dependence of long-term magnetization stability for data storage tapes prepared from ultrafine particles10.1016/j.phpro.2011.06.108 ↗
20. Polyester and acetate for magnetic recording tape backings
21. Correlation between creep, shrinkage, and dynamic mechanical characteristics of magnetic tape materials10.1002/app.33032 ↗
22. ATR-FTIR spectroscopy for the characterization of magnetic tapes materials
23. Pressure-dependent Fourier transform infrared spectroscopy of a poly(ester urethane)10.1016/S1386-1425(02)00173-7 ↗
24. Infrared analysis of the photochemical behavior of segmented polyurethanes: 1. Aliphatic poly(ester-urethane)10.1016/S0032-3861(96)00984-6 ↗
25. FTIR investigation of the influence of diisocyanate symmetry on the morphology development in model segmented polyurethanes10.1016/j.polymer.2006.02.027 ↗
26. Time-resolved infrared spectroscopy studies of poly(ethylene terephalate) deformation10.1021/ma0610459 ↗
27. In situ ATR-FTIR spectroscopy of poly(ethylene terephalate) subjected to high-temperature methanol10.1002/masy.200850521 ↗
28. Hydrogen bonding and polyurethane morphology. II. Spectroscopic, thermal and crystallization behavior of polyether blends with 1,3-dimethylurea and a model urethane compound10.1016/S0032-3861(02)00566-9 ↗
29. Characterization of U-matic videotape deterioration by size exclusion chromatography and pyrolysis gas chromatography/mass spectrometry and the role of adipic acid10.1016/j.culher.2008.04.010 ↗
30. Degradation of a poly(ester urethane) elastomer. III. Estane 5703 hydrolysis: experiments and modeling10.1002/pola.10656 ↗
31. Kinetics of hydrolytic aging of polyester urethane elastomers10.1021/ma60074a009 ↗
32. Phase separation of diamine chain-extended poly(urethane) copolymers: FTIR spectroscopy and phase transitions10.1016/S0032-3861(03)00165-4 ↗
33. Effects of hydrolysis-induced molecular weight changes on the phase separation of a polyester polyurethane10.1016/j.polymdegradstab.2006.05.019 ↗
34. Lifetime expectancy of polyurethane binder as magnetic recording media10.1016/S0143-7496(96)00015-2 ↗
35. Recent developments in binder design for advanced media10.1016/S0304-8853(98)00755-0 ↗
36. Dynamical mechanical analysis of barium ferrite magnetic tapes with aramid and poly(ethylene naphtalate) substrates10.1002/app.41478 ↗