Low Temperature Bonding of Alumina/Alumina and Alumina/Copper in Air Using Sn3.5Ag4Ti(Ce,Ga) Filler

S.Y. Chang, T.H. Chuang, C.L. Yang

Journal of Electronic Materials· Volume 36· Issue 9
Publisher page

Abstract

Sn3.5Ag4Ti(Ce,Ga) active filler was used for joining alumina with alumina and alumina with copper at 250°C in air. The joining process was done without flux and without the need for pre-metallization of alumina or a protective atmosphere. After mechanical activation of the bonding surfaces of alumina and copper, the filler showed good wetting on both alumina and copper and led to a strong bond between alumina and copper. Through tensile testing, a bonding strength of 23.7 MPa was found in the alumina/copper joint region. The shear strengths for alumina/alumina, copper/copper and alumina/copper joints were 13.5, 14.3, and 10.2 MPa, respectively. The affinity of cerium for oxygen protects titanium from oxidation, giving rise to the reaction of titanium with alumina at such a low temperature. Electron probe microanalyzer (EPMA) elemental mapping revealed that titanium segregates effectively at the alumina/solder interfaces. After aging tests at 200°C and 150°C, a double layer of Cu3Sn and Cu6Sn5 intermetallic compound was formed at the solder/copper interfaces. With an increase of aging periods, the amount of brittle compound in the joints increased and resulted in decreases in the shear strengths of the alumina/copper joints.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. Y. Yoshino and T. Shibata, J. Am. Ceram. Soc., 75(10), 2756 (1992).10.1111/j.1151-2916.1992.tb05500.x ↗
2. J. Glazer, Int. Mater. Rev. 40, 65 (1995).10.1179/095066095790151115 ↗
3. H. Pulfrich, U.S. Patent 2,163,407 (1939)10.1093/english/2.12.407 ↗
4. H.J. Nolte, U.S. Patent 2,667,432 (1954)
5. A.J. Chick and L.J. Speck, U.S. Patent. 2,708,787 (1955)
6. A.J. Moorhead, Adv. Ceram. Mater. 2(2), 159 (1987).10.1111/j.1551-2916.1987.tb00073.x ↗
7. H. Mizuhara and K. Mally, Weld. J., 64(10), 27 (1985).
8. W. Weise, W. Malikowski, and W. Bohm, Verbinden von Keramik mit Keramic oder Metall durch Aktivloten under Argon oder Vakuum, Firmenschrift Degussa Hanau AG., Hanau, Germany
9. Y.H. Chai, W.P. Weng, and T.H. Chuang, Ceram. Int. 24, 273 (1998).10.1016/S0272-8842(97)00009-6 ↗
10. T.H. Chuang, M.S. Yeh, and Y.H. Chai, Metall. Mat. Trans. A 31A, 1591 (2000).10.1007/s11661-000-0169-0 ↗
11. F. Hillen, D. Pickart-Castillo, I.J. Rass, and E. Lugscheider, Weld. Cutting 52(8), E162 (2000)
12. R.W. Smith, Weld. J. 10, 30 (2001).
13. S.Y. Chang, L.C. Tsao, M.J. Chiang, C.N. Tung, G.H. Pan, and T.H. Chuang, J. Mater. Eng. Perform. 12(4), 383 (2003).10.1361/105994903770342890 ↗
14. S.Y. Chang, M.H. Lu, L.C. Tsao, and T.H. Chuang, Weld. J., 4, 81 (2006).
15. M. Halvarsson, V. Langer, and S. Vuorinen, Surf. Coat. Technol., 76–77, 358 (1995).10.1016/0257-8972(95)02558-8 ↗
16. S-Bond Technologies, LLC, Bulletin No. 14.01.05, http://www.s-bond.com (2002)