Abstract

With miniaturization and heterogeneous integration in packaging, there has been a drive toward developing lower temperature solders. Sn-58Bi eutectic solder provides an attractive alternative with its meting point at 138°C. Due to the lower melting temperature of Sn-Bi solder, Bi coarsening may occur even at room temperature. In this paper, the microstructural evolution in Sn-58Bi joints was observed during room temperature storage. Room temperature aging induced the dissolution and coarsening of Bi phases in the solder matrix, especially in the primary Sn phases and Sn-Bi dendrites. The mechanical properties of individual Sn-rich and Bi-rich phases were measured by nanoindentation. The results showed that the Sn-rich phases had higher Young’s modulus and hardness than Bi-rich phases in aged solder joints due to solution strengthening. Bi phases were more compliant and had lower hardness than Sn.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Intermetallics and Advanced Alloy Properties · 3D IC and TSV technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. S. Cheng, C.-M. Huang, and M. Pecht, A review of lead-free solders for electronic applications Micron. Reliab. 75, 77 (2017).10.1016/j.microrel.2017.06.016 ↗
2. L. Zhang, and K.N. Tu, Structure and properties of lead-free solders bearing micro and nano particles Mater. Sci. Eng. R. 82, 1 (2014).10.1016/j.mser.2014.06.001 ↗
3. D.A. Shnawah, M.F. Sabri, and I.A. Badruddin, A review on thermal cycling and drop impact reliability of SAC solder joint in portable electronic products Microelectron. Reliab. 52, 90 (2012).10.1016/j.microrel.2011.07.093 ↗
4. F. Wang, H. Chen, Y. Huang, L. Liu, and Z. Zhang, Recent progress on the development of Sn-Bi based low-temperature Pb-free solders J. Mater. Sci.-Mater. Electron. 30, 3222 (2019).10.1007/s10854-019-00701-w ↗
5. H.R. Kotadia, P.D. Howes, and S.H. Mannan, A review: on the development of low melting temperature Pb-free solders Micron. Reliab. 54, 1253 (2014).10.1016/j.microrel.2014.02.025 ↗
6. Binary Alloy Phase Diagrams, edited by T. Massalski (ASM, International, Materials Park, OH, 1986)
7. A.A. El-Daly, A.M. El-Taher, and S. Gouda, Development of new multicomponent Sn-Ag-Cu-Bi lead-free solders for low-cost commercial electronic assembly J. Alloys Compd. 627, 268 (2015).10.1016/j.jallcom.2014.12.034 ↗
8. A.A. El-Daly, A.M. El-Taher, and S. Gouda, Novel Bi-containing Sn-1.5Ag-0.7Cu lead-free solder alloy with further enhanced thermal property and strength for mobile products Mater. Design. 65, 796 (2015).10.1016/j.matdes.2014.10.006 ↗
9. M. He, S.N. Ekpenuma, and V.L. Acoff, Microstructure and creep deformation of Sn-Ag-Cu-Bi/Cu solder joints J. Electron. Mater. 37, 300 (2008).10.1007/s11664-007-0368-1 ↗
10. M. Celikin, M. Maalekian, and M. Pekguleryuz, Effect of Bi additions on the creep behavior of SAC solder alloys J. Electron. Mater. 47, 5842 (2018).10.1007/s11664-018-6458-4 ↗
11. S. Liu, S. McDonald, K. Sweatman, and K. Nogita, The effects of precipitation strengthening and solid solution strengthening on strain rate sensitivity of lead-free solders Microelectron. Reliab. 84, 170 (2018).10.1016/j.microrel.2018.03.038 ↗
12. S.A. Belyakov, J. Xian, G. Zeng et al., Precipitation and coarsening of bismuth plates in Sn-Ag-Cu-Bi and Sn-Cu-Ni-Bi solder joints J. Mater. Sci.-Mater. Electron. 30, 378 (2019).10.1007/s10854-018-0302-8 ↗
13. P.J. Shang, Z.Q. Liu, D.X. Li, and J.K. Shang, Directional growth of Cu3Sn at the reactive interface between eutectic SnBi solder and (100) single crystal Cu Scripta Mater. 59, 317 (2008).10.1016/j.scriptamat.2008.03.031 ↗
14. C.Z. Liu, and W. Zhang, Bismuth redistribution induced by intermetallic compound growth in SnBi/Cu microelectronic interconnect J. Mater. Sci. 44, 149 (2009).10.1007/s10853-008-3118-8 ↗
15. F. Wang, H. Chen, Y. Huang, and C. Yan, Interfacial behavior and joint strength of Sn-Bi solder with solid solution compositions J. Mater. Sci. Mater. Electron. 29, 11409 (2018).10.1007/s10854-018-9233-7 ↗
16. T.Y. Kang, Y.Y. Xiu, C.Z. Liu, L. Hui, J.J. Wang, and W.P. Tong, Bismuth segregation enhances intermetallic compound growth in SnBi/Cu microelectronic interconnect J. Alloys. Compd. 509, 1785 (2011).10.1016/j.jallcom.2010.10.040 ↗
17. P.L. Liu, and J.K. Shang, Interfacial embrittlement by bismuth segregation in copper/tin-bismuth Pb-free solder interconnect J. Mater. Res. 16, 1651 (2001).10.1557/JMR.2001.0229 ↗
18. O. Mokhtari, and H. Nishikawa, Correlation between microstructure and mechanical properties of Sn-Bi-X solders Mater. Sci. Eng. A. 651, 831 (2016).10.1016/j.msea.2015.11.038 ↗
19. Y. Yanaka, Y. Kariya, H. Watanabe, H. Hokazono, Plastic deformation behavior and mechanism of bismuth single crystals in principal axes. Mater. Trans. MD201503 (2016)10.1299/jsmemecj.2016.J0120102 ↗