Abstract
Fatigue crack growth behavior of two typical solders 63Sn-37Pb and 95Pb-5Sn has been investigated under room temperature (20°C) and frequency of 10 Hz. Fatigue crack growth behavior of the 63Sn-37Pb specimen tested at stress ratios up to 0.5 and the 95Pb-5Sn specimen tested at stress ratios up to 0.7 were dominantly cyclic dependent. Intergranular crack growth was observed for the 63Sn-37Pb specimen tested at stress ratio of 0.7, which indicates that a crack grows under influence of creep. The difference of effect of stress ratio on crack growth behavior between two solders may results from the difference of homologous temperature. Fatigue crack growth mechanisms for solder materials are summarized as follows: A crack propagates in a transgranular manner at low homologous temperature and low stress ratio, while it propagates along eutectic grain boundaries at high homologous temperature and high stress ratio under influence of creep. At the intermediate homologous temperatures, a crack propagates in a transgranular manner with some region of intergranular fracture.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Fatigue and fracture mechanics · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. S. Vaynman, G. Ghosh and M. E. Fine, J. Electron. Mater. 27, 1223 (1998).10.1007/s11664-998-0073-8 ↗
2. G. Ghosh, J. Electron. Mater. 27, 1154 (1998).10.1007/s11664-998-0064-9 ↗
3. R. Sandstrom, J.-O. Osterberg, and M. Nylen, Mater. Sci. and Technol. 9, 811 (1993).
4. J. K. Tien, B. C. Hendrix, and A. I. Attarwala, IEEE Trans. CHMT 12, 502 (1989).
5. S. Vaynman, M. E. Fine, and D. A. Jeannotte, Metall. Trans. A 19, 1051 (1988).10.1007/BF02628389 ↗
6. R. Berriche M. E. Fine, and D. A. Jeannotte, Metall. Trans. A 22, 357 (1991).10.1007/BF02656804 ↗
7. D. R. Frear, J. B. Posthill, and J. W. Morris Jr., Metall. Trans. A 20, 1325 (1989).10.1007/BF02665491 ↗
8. D. Frear, D. Grivas, and J. W. Morris, Jr., J. Electron. Mater. 17, 171 (1988).10.1007/BF02652148 ↗
9. W. A. Logsdon, P. K. Liaw, and M. A. Burke, Eng. Fracture Mechan. 36, 183 (1990).10.1016/0013-7944(90)90001-W ↗
10. H. D. Solomon, The Mechanics of Solder Alloy Interconnects, ed. D. R. Frear et al. New York: Van Nostrand Reinhold, 1994), p.199.
11. H. D. Solomon, Solder Joint Reliability, ed. J. H. Lau New York: Van Nostrand Reinhold, 1991), p. 406.10.1007/978-1-4615-3910-0_14 ↗
12. Z. Guo and H. Conrad, J. Electron. Pkg. 115, 159 (1993).
13. W. H. Cubberly et al., Metals Handbook Ninth Edition, Vol. 2 Metals Park OH: ASM, 1979), pp. 500, 617.
14. G. A. Clarke and J. D. Landes, J. Testing and Eval., 7, 264 (1979).10.1520/JTE10222J ↗
15. G. R. Irwin, Fracture, Handbuch der Physik VI, ed. S. Flugge (Berlin: Springer, 1958), pp.551–590.
16. D. S. Dugdale, J. Mechs. and Phys of Solids 8, 100 (1960).10.1016/0022-5096(60)90013-2 ↗
17. V. Raman and T. C. Reiley, Scripta Metall. 20, 1343 (1986).10.1016/0036-9748(86)90092-X ↗
18. V. Raman and T. C. Reiley, Metall. Trans.A 19A, 1533 (1988).10.1007/BF02674027 ↗
19. D. Tribula, D. Grivas, D. R. Frear, and J. W. Morris, Jr., J. Electron. Pkg. 111, 83 (1989).
20. Z. Mei, J. W. Morris, Jr., M. C. Shine, and T. S. E. Summers, J. Electron. Mater. 20, 599 (1991).10.1007/BF02669524 ↗
21. D. Hardwick, C. M. Sellars, and W. J. McG. Tegart, J. Inst. Metals 90, 21 (1961–62).