journal article·2026-06-07

High-Reliability Cu-Cu3Sn Composite Bonding for Power Electronics in Harsh Environments

Huan Hu, YiShu Wang, Qiang Jia, Xu Gao, BoLong Zhou, Limin Ma, Guisheng Zou, Fu Guo

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Electrical Contact Performance and Analysis · 3D IC and TSV technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Y. Zhao, Y.T. Zhou, R. Ramaraghavulu, and G. Wang, Cu particle-reinforced Sn58Bi filler for soldering SiC to Cu at a temperature below 200°C. J. Mater. Sci. 60, 10898 (2025). https://doi.org/10.1007/s10853-025-11088-x.10.1007/s10853-025-11088-x ↗
2. G.D. Nuzzo, M. Tuellmann, T. Methfessel, and S. Rzepka, Condition monitoring indicators for Si and SiC power modules. Microelectron. Reliab. 138, 114614 (2022). https://doi.org/10.1016/j.microrel.2022.114614.10.1016/j.microrel.2022.114614 ↗
3. C.H. Yin, K. Wumaeraili, Y. Zhang, Y.C. Wu, J.H. Zhang, W. Guo, Y. Zhu, X.G. Song, Q. Jia, and H.Q. Zhang, Novel Ag-Cu foam sheet with multi-layer composite structure for high performance joining of SiC power chips. Mater Charact 209, 113696 (2024). https://doi.org/10.1016/j.matchar.2024.113696.10.1016/j.matchar.2024.113696 ↗
4. H.B. Jin, J.H. Wang, Y.Y. Yao, S.Q. Wang, and Y.A. Shen, Effect of thermal aging on joint with eutectic Sn-In solder by TLP bonding. Mater. Sci. Semicond. Process. 185, 108878 (2025). https://doi.org/10.1016/j.mssp.2024.108878.10.1016/j.mssp.2024.108878 ↗
5. H. Zhang, W. Zhou, X.L. Ji, and X.Y. Li, Growth kinetics and mechanical properties of the Cu20Sn6 phase transited from the full Cu3Sn joint during high temperature aging process. J. Mater. Sci. 34, 1309 (2023). https://doi.org/10.1007/s10854-023-10643-z.10.1007/s10854-023-10643-z ↗
6. P. Liu, J. Ren, and M.L. Huang, Microstructure and reliability of full (Cu,Ni)6Sn5 IMC interconnects fabricated by current driven bonding method with Sn-5Cu-5Ni composite solder. J. Mater. Sci. 36, 585 (2025). https://doi.org/10.1007/s10854-025-14635-z.10.1007/s10854-025-14635-z ↗
7. G.L. Yang, X.Y. Li, E.H. Ren, and S.S. Li, Morphology evolution and grain orientations of intermetallic compounds during the formation of full Cu3Sn joint. Intermetallics 145, 107555 (2022). https://doi.org/10.1016/j.intermet.2022.107555.10.1016/j.intermet.2022.107555 ↗
8. O. Golim, V. Vuorinen, T. Wernicke, M. Pawlak, and P.K. Mervi, Low-temperature wafer-level bonding with Cu-Sn-In solid liquid interdiffusion for microsystem packaging. Microelectron. Eng. 286(1), 112140 (2024). https://doi.org/10.1016/j.mee.2024.112140.10.1016/j.mee.2024.112140 ↗
9. H. Jiang, S. Robertson, S.B. Liang, Z.X. Zhou, L.G. Zhao, and C.Q. Liu, Microstructural and mechanical characteristics of Cu-Sn intermetallic compound interconnects formed by TLPB with Cu-Sn nanocomposite. Mater. Today Commun. 33, 104623 (2022). https://doi.org/10.1016/j.mtcomm.2022.104623.10.1016/j.mtcomm.2022.104623 ↗
10. P. Yao, X.Y. Li, X.B. Liang, and B. Yu, Investigation of soldering process and interfacial microstructure evolution for the formation of full Cu3Sn joints in electronic packaging. Mater. Sci. Semicond. Process. 58, 39 (2017). https://doi.org/10.1016/j.mssp.2016.11.019.10.1016/j.mssp.2016.11.019 ↗
11. Satyanarayan and K.N. Prabhu, Reactive wetting, evolution of interfacial and bulk IMCs and their effect on mechanical properties of eutectic Sn-Cu solder alloy. Adv. Colloid Interface Sci. 166(1–2), 87 (2011). https://doi.org/10.1016/j.cis.2011.05.005.10.1016/j.cis.2011.05.005 ↗
12. L. Zhu, J. Ren, and M.L. Huang, Ultrasonic-assisted rapid fabrication of Cu foam/Cu-Sn IMC composite interlayers for high-temperature die-attach applications. Mater Charact 224, 115100 (2025). https://doi.org/10.1016/j.matchar.2025.115100.10.1016/j.matchar.2025.115100 ↗
13. H.H. Zhang, H.Y. Xu, X. Liu, and J. Xu, Fabrication of Cu@Sn TLPS joint for high temperature power electronics application. RSC Adv. 12(45), 29063 (2022). https://doi.org/10.1039/d2ra04606g.10.1039/d2ra04606g ↗
14. H.W. Niu, H. Bian, X. Liu, X.G. Song, and H.Y. Zhao, Asymmetric growth of Cu6Sn5 intermetallic compound in Cu/Sn/Cu bonding system under the vertical ultrasonic vibration. Intermetallics 170, 108337 (2024). https://doi.org/10.1016/j.intermet.2024.108337.10.1016/j.intermet.2024.108337 ↗
15. H.B. Li, K.X. Shang, J. Shen, D.J. Luo, and Q. Chen, Mechanics and thermal behavior of Cu-Sn solder reinforced by skeleton intermetallic compounds: Insights from molecular dynamics and experiments. Mater. Today Commun. 49, 114065 (2025). https://doi.org/10.1016/j.mtcomm.2025.114065.10.1016/j.mtcomm.2025.114065 ↗
16. L. Zhu, J. Ren, F.F. Huang, and M.L. Huang, High-performance full IMC/Cu foam composite joints prepared by transient liquid phase soldering for high temperature application. Mater. Chem. Phys. 343, 131045 (2025). https://doi.org/10.1016/j.matchemphys.2025.131045.10.1016/j.matchemphys.2025.131045 ↗
17. L. Sun, M.H. Chen, L. Zhang, P. He, and L.S. Xie, Recent progress in SLID bonding in novel 3D-IC technologies. J. Alloys Compd. 818, 152825 (2020). https://doi.org/10.1016/j.jallcom.2019.152825.10.1016/j.jallcom.2019.152825 ↗
18. Q. Jia, Z.Y. Deng, L. Liu, H.Q. Zhang, W.G. Wang, L.M. Ma, F. Guo, and G.S. Zou, Interface enhancing strategy for low-temperature bonding of Ag-based nanoalloy. Mater. Lett. 339, 134050 (2023). https://doi.org/10.1016/j.matlet.2023.134050.10.1016/j.matlet.2023.134050 ↗
19. B.L. Zhou, Q. Jia, Y.S. Wang, D. Li, H.Q. Zhang, H.A. Hu, L.M. Ma, G.S. Zou, and F. Guo, Preparation of Ag-Cu nanoparticle film using a dual-beam pulsed laser deposition for power electronic packaging. J. Laser Appl. 36, 022010 (2024). https://doi.org/10.2351/7.0001321.10.2351/7.0001321 ↗
20. H.A. Hu, Q. Jia, Y.S. Wang, B.L. Zhou, H.Q. Zhang, M.A. Zhang, L.M. Ma, G.S. Zou, and F. Guo, Facile synthesis of Cu-Sn nanoparticle film and its bonding mechanism for power electronic packaging. J. Mater. Process. Technol. 329, 118438 (2024). https://doi.org/10.1016/j.jmatprotec.2024.118438.10.1016/j.jmatprotec.2024.118438 ↗
21. L. Sun, M.H. Chen, and L. Zhang, Microstructure evolution and grain orientation of IMC in Cu-Sn TLP bonding solder joints. J. Alloys Compd. 786, 677 (2019). https://doi.org/10.1016/j.jallcom.2019.01.384.10.1016/j.jallcom.2019.01.384 ↗
22. X. Zhao, Z. Deng, W. Zhao, B. Feng, M. Wang, and M. Huang, Nanoporous silver by pulsed laser deposition for high-performance oxygen reduction reaction and hydrogen peroxide sensing. Nanoscale 12(37), 19413 (2020). https://doi.org/10.1039/D0NR05395C.10.1039/D0NR05395C ↗
23. J.B. Xin, X.C. Lv, Y. Gao, L. Yang, S.S. Liu, and K. Li, Failure modes competition and long-term reliability in the isothermal aging of sintered Cu joints. Microelectron. Reliab. 168, 115717 (2025). https://doi.org/10.1016/j.microrel.2025.115717.10.1016/j.microrel.2025.115717 ↗
24. M.L. Li, L. Zhang, L. Gao, X. Wang, X. Chen, and X. Lu, Interfacial structures and mechanical properties of Cu/Sn/Cu containing SiC nanowires under transient liquid phase bonding. Intermetallics 148, 107641 (2022). https://doi.org/10.1016/j.intermet.2022.107641.10.1016/j.intermet.2022.107641 ↗
25. M. Shang, J.Y. Yao, J.J. Wang, Y.P. Wang, H. Ma, and H.R. Ma, Direct formation of Cu3Sn at Sn-Bi/Cu interfaces: a thermodynamic and kinetic perspective. Appl. Surf. Sci. 716(30), 164522 (2026). https://doi.org/10.1016/j.apsusc.2025.164522.10.1016/j.apsusc.2025.164522 ↗
26. X.W. Peng, Y. Wang, W.L. Wang, Z. Ye, J. Yang, and J.H. Huang, Kinetics of Cu6Sn5 and Cu3Sn intermetallic compounds growth and isothermal solidification during Cu-Sn transient liquid phase sintering process. J. Alloys Compd. 949(15), 169631 (2023). https://doi.org/10.1016/j.jallcom.2023.169631.10.1016/j.jallcom.2023.169631 ↗
27. H.A. Hu, Y.S. Wang, Q. Jia, B.L. Zhou, R.C. Liu, and F. Guo, Rapid in-situ formation of Cu-Sn full intermetallic compound films and their joint strengthening mechanisms. Mater. Des. 256, 114241 (2025). https://doi.org/10.1016/j.matdes.2025.114241.10.1016/j.matdes.2025.114241 ↗
28. Q.Y. Yin, F. Gao, Z.Y. Gu, J.R. Wang, E.A. Stach, and G.W. Zhou, In situ imaging of the soldering reactions in nanoscale Cu/Sn/Cu and Sn/Cu/Sn diffusion couples. J. Appl. Phys. 123, 024302 (2018). https://doi.org/10.1063/1.4995314.10.1063/1.4995314 ↗
29. J.X. Liu, W.H. Lv, Y. Mou, Y. Peng, F.L. Zhu, and M.X. Chen, Sn-enhanced high-temperature reliability of Cu/Nano-Ag/Cu joint via transient-liquid-phase bonding. J. Mater. Sci. 58, 10870 (2023). https://doi.org/10.1007/s10853-023-08702-1.10.1007/s10853-023-08702-1 ↗