Abstract

The appearance of cut-pile carpets deteriorates due to foot traffic and long term heavy loadings. This deterioration is generally seen as a fuzzy appearance due to loose fibers and fuzz on the carpet surface or as thickness loss. The fiber fineness has important effects on a number of yarn properties including cohesion, evenness, strength, stiffness and luster. In this study, three acrylic yarns with different fiber finenesses at the same yarn linear density were used to produce cut-pile carpet samples. The effects of fiber linear density on the amount of loose fibers and fuzz on the carpet surface, thickness loss under prolonged heavy static and dynamic loadings and compression recovery after loading-unloading were investigated. The carpet produced with finest fibers yarns had the lowest amount of loose fibers due to higher cohesion. The carpet samples with the finest fibers exhibited the highest resiliency and lowest thickness loss under static loading. However, the carpet samples with the coarsest fibers showed the least thickness loss under dynamic loading and higher compression recovery after loading-unloading.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Textile materials and evaluations · Ergonomics and Musculoskeletal Disorders · Color perception and design

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Gaziantep University Textile Engineering Department, Gaziantep TURKEY

References (27)

Show source-provided references
1. Crawshaw G. H. · 2002
2. Goswami K. K. · 2009
3. Demey S · Textinfo · 2011 · 1
4. 10.1080/00405000.2014.91278410.1080/00405000.2014.912784 ↗
5. 10.1080/00405000.2013.87615110.1080/00405000.2013.876151 ↗
6. Özdil N. · Tekstil ve Konfeksiyon · 2014 · 3 · 203
7. 10.1080/00405000.2012.68555810.1080/00405000.2012.685558 ↗
8. 10.1080/0040500080254224210.1080/00405000802542242 ↗
9. Dubinskaite K. · Fibres & Textiles in Eastern Europe · 2008 · 16 · 47
10. 10.1080/0040500080237616110.1080/00405000802376161 ↗
11. Celik N. · Fibres & Textiles in Eastern Europe · 2010 · 18 · 54
12. Celik N. · Fibres & Textiles in Eastern Europe · 2007 · 15 · 87
13. Koc E. · Fibres & Textiles in Eastern Europe · 2005 · 13 · 56
14. 10.1177/004051750606103610.1177/0040517506061036 ↗
15. Celik N. · Association of Textile, Apparel and Material Professionals · 2009 · 43
16. Saville B. P. · 1999
17. NPTEL; E-Learning Courses from The IITs & IISc; http://nptel.ac.in/courses/116102029/14, 2015.
18. Sheikhi H. · FIBRES & TEXTILES in Eastern Europe · 2012 · 20 · 77
19. ISO 139: 2005 (en) Textiles-Standard atmospheres for conditioning and testing.
20. DD ISO/PAS 11856:2003 Textile floor covering-Test methods for the determination of fibre bind-Determination of mass loss by hexapod tumbler test.
21. ISO 8543:1998 Textile floor coverings. Methods for determination of mass.
22. ISO 3416:1986(en) Textile floor coverings — Determination of thickness loss after prolonged, heavy static loading.
23. ISO 1765:1986(en) Machine-made textile floor coverings — Determination of thickness.
24. BS ISO 2094:1999 Textile floor coverings. Determination of thickness loss under dynamic loading.
25. BS 4098:1975 Method for the determination of thickness, compression and recovery characteristics of textile floor coverings.
26. 10.1007/BF0287567110.1007/BF02875671 ↗
27. Gokarneshan N. · Indian Journal of Fibre & Textile Research · 2008 · 33 · 203