journal article·2019-01-01Open access

Mechanical Behavior of Silicon Carbide Under Static and Dynamic Compression

D. Zhang, L. G. Zhao, A. Roy

Abstract

This paper compared the mechanical behavior of 6H SiC under quasi-static and dynamic compression. Rectangle specimens with a dimension of 3 × 3 × 6 mm3 were used for quasi-static compression tests under three different loading rates (i.e., 10−5/s, 10−4/s, and 10−3/s). Stress–strain response showed purely brittle behavior of the material which was further confirmed by scanning electron microscopy (SEM)/transmission electron microscopy (TEM) examinations of fractured fragments. For dynamic compression, split Hopkinson pressure bar (SHPB) tests were carried out for cubic specimens with a dimension of 6 × 6 × 4 mm3. Stress–strain curves confirmed the occurrence of plastic deformation under dynamic compression, and dislocations were identified from TEM studies of fractured pieces. Furthermore, JH2 model was used to simulate SHPB tests, with parameters calibrated against the experimental results. The model was subsequently used to predict strength and plasticity-related damage under various dynamic loading conditions. This study concluded that, under high loading rate, silicon carbide (SiC) can deform plastically as evidenced by the development of nonlinear stress–strain response and also the evolution of dislocations. These findings can be explored to control the brittle behavior of SiC and benefit end users in relevant industries.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-Velocity Impact and Material Behavior · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Wolfson School of Mechanical, Electrical and Manufacturing Engineering, Loughborough University, Loughborough LE11 3TU, UK

Wolfson School of Mechanical, Electrical and Manufacturing Engineering, Loughborough University, Loughborough LE11 3TU, UK e-mail:

References (35)

Show source-provided references
1. Mechanical Properties of 3C-SiC Films for MEMS Applications10.1557/PROC-1049-AA03-06 ↗
2. Silicon Carbide as a New MEMS Technology10.1016/S0924-4247(99)00335-0 ↗
3. Inductively-Coupled Plasma-Enhanced Chemical Vapour Deposition of Hydrogenated Amorphous Silicon Carbide Thin Films for MEMS10.1016/j.sna.2016.05.042 ↗
4. Research of CMC Application to Turbine Components
5. Friction and Surface Fracture of a Silicon Carbide Ceramic Brake Disc Tested against a Steel Pad10.1016/j.jeurceramsoc.2015.07.009 ↗
6. Ballistic Performance of Bilayer Alumina Aluminium and Silicon Carbide Aluminium Armours10.1016/j.proeng.2016.12.141 ↗
7. Characterisation, Significance and Detection of Manufacturing Defects in Reaction Sintered Silicon Carbide Armour Materials10.1016/j.ceramint.2015.06.083 ↗
8. Investigations on Hydrobromination of Silicon in the Presence of Silicon Carbide Abrasives as a Purification Route of Kerf Loss Waste10.1016/j.seppur.2012.10.031 ↗
9. Mechanisms Responsible for Strain-Rate-Dependent Compressive Strength in Ceramic Materials10.1111/j.1151-2916.1981.tb09570.x ↗
10. Strain-Rate Effect on Brittle Failure in Compression10.1016/0956-7151(94)90295-X ↗
11. Dynamic Compressive Strength of Silicon Carbide Under Uniaxial Compression10.1016/S0921-5093(01)01172-8 ↗
12. Dynamic Strength of Reaction-Sintered Silicon Carbide Ceramics10.3103/S0025654414060028 ↗
13. The Influence of Mechanical and Microstructural Properties on the Rate-Dependent Fracture Strength of Ceramics in Uniaxial Compression10.1016/j.ijimpeng.2015.02.007 ↗
14. The Rate-Dependent Fracture Toughness of Silicon Carbide- and Boron Carbide-Based Ceramics10.1016/j.jeurceramsoc.2015.08.027 ↗
15. Prismatic Slip of Al2O3 Single Crystals below 1000 °C in Compression Under Hydrostatic Pressure10.1111/j.1151-2916.1981.tb10314.x ↗
16. Temperature-Strain Rate Dependance of Compressive Strength and Damage Mechanisms in Aluminium Oxide10.1007/BF02396874 ↗
17. Effect of Stress State and Microstructural Parameters on Impact Damage of Alumina-Based Ceramics10.1007/BF01174523 ↗
18. Static and Dynamic Compressive Behavior of Aluminum Nitride Under Moderate Confinement10.1111/j.1151-2916.1996.tb07913.x ↗
19. High-Strain-Rate Superplasticity in Nanocrystalline Silicon Nitride Ceramics Under Compression10.1016/j.scriptamat.2015.02.028 ↗
20. Standard Test Method for Monotonic Compressive Strength of Advanced Ceramics at Ambient Temperature
21. An Investigation of Mechanical Properties of Material at Very High Rates of Loading10.1088/0370-1301/62/11/302 ↗
22. A Split Hopkinson Pressure Bar Technique to Determine Compressive Stress-Strain Data for Rock Materials10.1007/BF02323102 ↗
23. Cronin, D. S., Bui, K., Kaufmann, C., Mcintosh, G., Berstad, T., and Cronin, D., 2003, “Implementation and Validation of the Johnson-Holmquist Ceramic M Aterial Model in LS-DYNA,” Fourth European LS-DYNA Users Conference, Ulm, Germany, May 23–24, pp. 47–60.
24. ‘A Computational Constitutive Model for Brittle Materials Subjected to Large Strains, High Strain Rates and High Pressures’
25. An Improved Computational Constitutive Model for Brittle Materials10.1063/1.46199 ↗
26. Microstructure and Mechanical Properties of Silicon Carbide Processed by Spark Plasma Sintering (SPS)10.1016/j.ceramint.2012.05.003 ↗
27. Experiments and Modelling of the Compressive Behaviour of Two SiC Ceramics10.1016/S0167-6636(02)00321-6 ↗
28. Damage Evolution in Dynamic Deformation of Silicon Carbide10.1016/S1359-6454(99)00409-7 ↗
29. Mechanisms of Dynamic Deformation and Dynamic Failure in Aluminium Nitride10.1016/j.actamat.2012.03.011 ↗
30. Dynamic Failure and Fracture Mechanism in Alumina Ceramics: Experimental Observations and Finite Element Modelling10.1016/j.ceramint.2015.06.110 ↗
31. Synthesis and Structure–Property Relationships of a New Family of Layered Carbides in Zr-Al(Si)-C and Hf-Al(Si)-C Systems10.1016/j.jeurceramsoc.2013.05.020 ↗
32. Defects in Silicon Carbide10.1007/BF00761949 ↗
33. Defects in Plastically Deformed 6H-SiC Single Crystal Studied by Transmission Electron Microscopy10.1080/01418618808214408 ↗
34. 1992 · 98
35. Response of Silicon Carbide to High Velocity Impact Response of Silicon Carbide to High Velocity Impact10.1063/1.1468903 ↗