journal article·2010-10-01

Creep Behavior of Copper and Cu–0.3Cr–0.1Ag Alloy

A. Akbari-Fakhrabadi, R. Mahmudi, A. Karsaz, A. R. Geranmayeh

Publisher page

Abstract

The creep behavior of Cu–0.3Cr–0.1Ag alloy was investigated by the impression creep testing technique and compared with that of pure copper under constant punching stress in the range 80–550 MPa at temperatures in the range 688–855 K. The enhanced creep resistance of the Cr- and Ag-containing alloys was attributed to the distribution of Cr-rich phase in the copper matrix. Assuming a power-law relationship between the impression stress and velocity, the average stress exponents of 6.0–7.5 and 6.4–8.0 were obtained for pure Cu and CuCrAg, respectively. It was found that the average activation energies were 112.4 kJ mol−1 and 143.5 kJ mol−1 for the pure Cu and CuCrAg alloys, respectively. These activation energies are close to 138 kJ mol−1 for dislocation climb in Cu. This, together with the stress exponents of about 7, suggests that the operative creep mechanism is dislocation climb controlled by dislocation pipe diffusion.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Electronic Packaging and Soldering Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials Engineering, Islamic Azad University, Sirjan Branch, Sirjan, 87185-4563, Iran

School of Metallurgical and Materials Engineering, University of Tehran, PO Box 11155-4563, Tehran, Iran

References (25)

Show source-provided references
1. Processing, Microstructure, and Properties of Ternary High-Strength Cu–Cr–Ag In-Situ Composites10.1016/S0921-5093(00)00981-3 ↗
2. Wear Behavior of Cu–Ag–Cr Alloy Wire Under Electrical Sliding10.1016/j.msea.2005.03.023 ↗
3. Effect of the Amount of Cold Working and Ageing on the Ductility of a Cu–15%Cr–0.2%Ti In-Situ Composite10.1016/S0921-5093(99)00028-3 ↗
4. Study on the Aging Precipitation of the High-Strength and High-Conductivity Dilute Solute Cu-O.1Ag-O.11Cr Alloy
5. Age Hardening Studies in a Cu–4.5Ti–0.5Co Alloy10.1016/S0921-5093(00)01834-7 ↗
6. Analysis of Phases in a Cu–Cr–Zr Alloy10.1016/S1359-6462(02)00353-6 ↗
7. Aging Properties Studies in a Cu–Ag–Cr Alloy10.1016/j.msea.2005.09.118 ↗
8. Creep of Cu–Cr Type Alloys
9. Impression Creep Study of a Cu–0.3Cr–0.1Ag Alloy10.1016/j.msea.2010.01.044 ↗
10. Impression Creep of a Mg-8Zn-4Al-0.5Ca Alloy
11. Impression Creep Behavior of a Cast AZ91 Magnesium Alloy10.1007/s11661-008-9699-7 ↗
12. Impression Creep of Sn–40Pb–2.5Sb Peritectic Solder Alloy10.1179/174328405X46079 ↗
13. Effect of Cooling Rate on the Room-Temperature Impression Creep of Lead-Free Sn–9Zn and Sn–8Zn–3Bi Solders10.1016/j.msea.2007.09.050 ↗
14. Creep of a TiAl Alloy: A Comparison of Indentation and Tensile Testing10.1016/S0921-5093(03)00205-3 ↗
15. Impression Creep of Hypoeutectic Sn–Zn Lead-Free Solder Alloys10.1016/j.msea.2008.01.051 ↗
16. Investigation of Stress Exponent in the Room-Temperature Creep of Sn–40Pb–2.5Sb Solder Alloy10.1016/j.jallcom.2006.04.037 ↗
17. A Comparison of Impression and Compression Creep Behavior of Polycrystalline Sn10.1007/s10853-006-0542-5 ↗
18. Impression Creep Behavior of Cast Pb–Sb Alloys10.1016/j.jallcom.2006.02.053 ↗
19. Impression Creep; A New Creep Test10.1007/BF00552241 ↗
20. Creep Behavior of Copper at Intermediate Temperatures—I. Mechanical Characteristics10.1016/0001-6160(89)90011-4 ↗
21. Identifiying Creep Mechanisms at Low Stresses10.1016/S0921-5093(00)00624-9 ↗
22. Creep Deformation Characteristics of Tin and Tin-Based Electronic Solder Alloys10.1007/s11661-005-0142-z ↗
23. Frost · 21
25. Mechanical Behavior of Crystalline Solids at Elevated Temperature10.1016/0079-6425(68)90024-8 ↗