Biaxial Thermal Creep of Alloy 617 and Alloy 230 for VHTR Applications
Source abstract
Abstract
In this study, we employed pressurized creep tubes to investigate the biaxial thermal creep behavior of Inconel 617 (alloy 617) and Haynes 230 (alloy 230). Both alloys are considered to be the primary candidate structural materials for very high-temperature reactors (VHTRs) due to their exceptional high-temperature mechanical properties. The current creep experiments were conducted at 900 °C for the effective stress range of 15–35 MPa. For both alloys, complete creep strain development with primary, secondary, and tertiary regimes was observed in all the studied conditions. Tertiary creep was found to be dominant over the entire creep lives of both alloys. With increasing applied creep stress, the fraction of the secondary creep regime decreases. The nucleation, diffusion, and coarsening of creep voids and carbides on grain boundaries were found to be the main reasons for the limited secondary regime and were also found to be the major causes of creep fracture. The creep curves computed using the adjusted creep equation of the form ε=Aσcosh−1(1+rt)+Pσntm agree well with the experimental results for both alloys at the temperatures of 850–950 °C.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Nuclear Materials and Properties · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Nuclear Engineering Division, Argonne National Laboratory, Argonne, IL 60439 e-mail:
Department of Nuclear, Plasma, and Radiological Engineering, University of Illinois at Urbana-Champaign, 104 South Wright Street, Urbana, IL 61801
Institute of Nuclear Energy Research, Atomic Energy Council, Taoyuan 325, Taiwan
Nuclear Engineering Division, Argonne National Laboratory, Argonne, IL 60439;
Department of Nuclear Science and Technology, Xi'an Jiaotong University, Xi'an 710049, China
References (49)
Show source-provided references
1. A Review on Current Status of Alloys 617 and 230 for Gen IV Nuclear Reactor Internals and Heat Exchangers10.1115/1.3121522 ↗
2. A Review Paper on Aging Effects in Alloy 617 for Gen IV Nuclear Reactor Applications10.1115/1.2967885 ↗
3. Inconel Alloy 617—New High-Temperature Alloy
4. Materials Behavior in HTGR Environments
5. Development of a New Nickel-Base Superalloy10.1007/BF03338564 ↗
6. Creep-Rupture Behavior of Candidate Materials for Nuclear Process Heat Applications
7. Oxidation and Creep Failure of Alloy 617 Foils at High Temperature10.1016/j.jnucmat.2008.04.021 ↗
8. Creep Deformation of Alloys 617 and 276 at 750–950 °C10.1016/j.msea.2009.05.029 ↗
9. Creep-Behavior of Materials for High-Temperature Reactor Application
10. Effect of Thermo-Mechanical Processing on Microstructure and Creep Properties of the Foils of Alloy 61710.1016/j.jnucmat.2009.02.029 ↗
11. Influence of Grain Boundary Character on Creep Void Formation in Alloy 61710.1007/s11661-009-0051-7 ↗
12. Precipitate Redistribution During Creep of Alloy 61710.1007/s11661-009-0027-7 ↗
13. Creep Behaviour of as Received, Aged and Cold Worked INCONEL 617 at 850 °C and 950 °C10.1016/j.jnucmat.2010.01.019 ↗
14. Creep Oxidation Behaviour and Creep Strength Prediction for Alloy 61710.1016/j.ijpvp.2010.03.008 ↗
15. Low Cycle Fatigue and Creep-Fatigue Behavior of Alloy 617 at High Temperature10.1115/1.4025080 ↗
16. The Development of Microstructural Damage During High Temperature Creep-Fatigue of a Nickel Alloy10.1016/j.ijfatigue.2012.07.016 ↗
17. Developing Dislocation Subgrain Structures and Cyclic Softening During High-Temperature Creep-Fatigue of a Nickel Alloy10.1007/s11661-013-1737-4 ↗
18. Topologically Close-Packed μ Phase Precipitation in Creep-Exposed Inconel 617 Alloy10.1007/s11661-012-1491-z ↗
19. The Effect of High-Temperature Reactor Primary Circuit Helium on the Formation and Propagation of Surface Cracks in Alloy 800-H and Inconel-61710.1016/0022-3115(84)90553-1 ↗
20. Effect of Trace Impurities in Helium on the Creep Behavior of Alloy 617 for Very High Temperature Reactor Applications10.1016/j.jnucmat.2006.12.028 ↗
21. Microstructural Investigation of Alloy 617 Creep-Ruptured at High Temperature in a Helium Environment10.1016/j.jmst.2013.09.024 ↗
22. Biaxial Thermal Creep of Inconel 617 and Haynes 230 at 850 and 950 °C10.1016/j.jnucmat.2013.12.016 ↗
23. Mechanism of Creep Deformation of Alloy 230 Based on Microstructural Analyses10.1016/j.msea.2010.08.069 ↗
24. Crack-Growth Behavior of Alloy 230 Under Creep-Fatigue Conditions10.1016/j.msea.2010.04.005 ↗
25. A Comparison of the Microstructure and Creep Behavior of Cold Rolled HAYNES® 230 Alloy™ and HAYNES® 282 Alloy™10.1016/j.msea.2011.03.019 ↗
26. Creep Deformation and Mechanisms in Haynes 230 at 800 °C and 900 °C10.1016/j.jnucmat.2013.08.009 ↗
27. High Temperature Fatigue Crack Growth of Haynes 23010.1016/j.matchar.2012.09.012 ↗
28. The Evolved Microstructure Ahead of an Arrested Fatigue Crack in Haynes 23010.1016/j.actamat.2013.06.020 ↗
29. Behavior of Metallic Materials Between 550 and 870 °C in High-Temperature Gas-Cooled Reactor Helium Under Pressures of 2 and 50 Bar
30. Effect of Creep and Oxidation on Reduced Fatigue Life of Ni-Based Alloy 617 at 850 °C10.1016/j.jnucmat.2013.09.030 ↗
31. Experimental and Modeling Results of Creep-Fatigue Life of Inconel 617 and Haynes 230 at 850 °C10.1016/j.jnucmat.2012.08.040 ↗
32. Low Cycle Fatigue and Creep-Fatigue Behavior of Ni-Based Alloy 230 at 850 °C10.1016/j.msea.2012.11.063 ↗
33. Threshold Stress Creep Behavior of Alloy 617 at Intermediate Temperatures10.1007/s11661-014-2244-y ↗
34. Dependence of Irradiation Creep on Temperature and Atom Displacements in 20% Cold Worked Type 316 Stainless Steel10.1016/0022-3115(77)90057-5 ↗
35. Effect of Preinjected Helium on the Response of V-20Ti Pressurized Tubes to Neutron Irradiation10.1016/0022-3115(86)90129-7 ↗
36. Irradiation Creep of Vanadium-Base Alloys10.1016/S0022-3115(98)00211-6 ↗
37. Biaxial Thermal Creep of Inconel 617 and Haynes 230 at 850 and 950 °C10.1016/j.jnucmat.2013.12.016 ↗
38. Creep Deformation of 20 Percent Cold-Worked Type 316 Stainless-Steel10.1115/1.3443428 ↗
39. Biaxial Thermal Creep of Two Heats of V4Cr4Ti at 700 and 800 °C in a Liquid Lithium Environment10.1016/j.jnucmat.2007.03.081 ↗
40. Manufacturing Pressurized Creep Tubes From Highly Purified V–4Cr–4Ti alloys, NIFS-Heat210.1016/j.jnucmat.2004.07.033 ↗
41. Thermal Creep Mechanisms in V–4Cr–4Ti Pressurized Tube Specimens10.1016/j.jnucmat.2007.03.067 ↗
42. Hishinuma, A., Vitek, J., Horak, J., and Bloom, E., 1982, “Effect of Preinjected Helium on Swelling and Microstructure of Neutron Irradiated Pressurized Tubes of Type 316 Stainless Steel,” 11th Conference on Effects of Radiation on Materials, Scottsdale, AZ, June 28–30, ASTM STP 782, pp. 92–10710.1520/STP34340S.
43. Creep Deformation Mechanisms in Modified 9Cr-1Mo Steel10.1016/j.jnucmat.2012.01.005 ↗
44. Creep Behavior of Niobium-Modified Zirconium Alloys10.1016/j.jnucmat.2007.08.019 ↗
45. High Temperature Aging and Corrosion Study on Alloy 617 and Alloy 23010.1115/1.4002819 ↗
46. Mechanism of Plastic Deformation of a Ni-Based Superalloy for VHTR Applications10.1016/j.jnucmat.2013.03.083 ↗
47. Synchrotron Radiation Study on Alloy 617 and Alloy 230 for VHTR Application10.1115/1.4007041 ↗
48. Effect of Orientation on Plastic Deformations of Alloy 617 for VHTR Applications10.1016/j.jnucmat.2013.07.061 ↗
49. Creep Studies on Type 304 Stainless Steel (Heat 8043813) Under Constant and Varying Loads