Effect of Coated Rutile TiO2 and Disazopyrazolone Dye Additives on Unvulcanized Styrene Butadiene Rubber During Photo-Ageing
Source abstract
Abstract
The effect of coated rutile titanium dioxide (TiO2) and a disazopyrazolone dye (azo dye) on the mechanism and the kinetic of photo-oxidation of unvulcanized styrene butadiene rubber (SBR) composites under accelerated UV-visible irradiation (λ > 290 nm at 35 °C) has been investigated using several techniques such as infrared spectroscopy, UV-visible spectrophotometry, and gel fraction measurements. Different photo-products resulting from the photo-ageing such as alcohol, ketone, or acids as well as cross-linked network were identified. The incorporation of TiO2 rutile and an azo dye into the matrix did not modify the mechanism of photo-oxidation. However, they have a significant effect on the kinetic of photoproducts accumulation. Both fillers protect the matrix from photo-oxidation. TiO2 rutile, thanks to its inorganic coating at the surface, dissipates part of the UV-visible radiation received by the polymer. The activity mechanism of azo dye consisting of a combination of its function as an antioxidant and light absorber, presents a better stabilizing effect compared with TiO2 rutile.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Polymer Nanocomposites and Properties · Epoxy Resin Curing Processes · Photopolymerization techniques and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Advanced Materials and Structures, CRP Henri Tudor, 66 rue de Luxembourg, L-4002 Esch-sur-Alzette, Luxembourg; Institut Jean Lamour - UMR CNRS 7198, Ecole des Mines de Nancy, Parc de Saurupt, F-54042 Nancy cedex, France
Department of Advanced Materials and Structures, CRP Henri Tudor, 66 rue de Luxembourg, L-4002 Esch-sur-Alzette, Luxembourg
Institut Jean Lamour - UMR CNRS 7198, Ecole des Mines de Nancy, Parc de Saurupt, F-54042 Nancy cedex, France
References (41)
Show source-provided references
1. Characterization Of Photodegradation of Polybutadiene and Polyisoprene: Chronology of Crosslinking and Chain-Scission10.1016/j.polymertesting.2010.02.008 ↗
2. Photooxidation of Polybutadiene at Long Wavelengths (λ > 300 nm)10.1016/0141-3910(96)00093-6 ↗
3. Characterization of Photodegradation of Polybutadiene and Polyisoprene: Chronology of Crosslinking and Chain-Scission10.1016/j.polymdegradstab.2004.02.013 ↗
4. Photo-, Thermal and Natural Ageing of Ethylene–Propylene–Diene Monomer (EPDM) Rubber Used in Automotive Applications. Influence of Carbon Black, Crosslinking and Stabilizing Agents10.1016/S0141-3910(99)00147-0 ↗
5. New Insights into Crosslinking of Elastomers Through Photo-Oxidation10.1016/S0141-3910(02)00232-X ↗
6. A Review of Rubber Oxidation10.5254/1.3547889 ↗
7. Gardette, J. L., Baba, M., Mailhot, B., Morlat-Thérias, S., and Rivaton, A., 2008, “Photodégradation des Matériaux Polymères,” L’Actualité Chimique, n°317, pp. 25–30.
8. Polymer Weathering: Photo-Oxidation10.1023/A:1021148205366 ↗
9. Photo-Oxidative Degradation Mechanisms in Styrene–Ethylene–Butadiene–Styrene (SEBS) Triblock Copolymer10.1016/j.polymdegradstab.2005.06.017 ↗
10. Bousquet, J. A., Fouassier, J. P., 1987, “Photo-oxidation of a Random Styrene-Butadiene Copolymer: Role of Hydroperoxides and Behaviour of Butenyl Segments,” Eur. Polym. J., 23(5), pp. 367–376.10.1016/0014-3057(87)90165-010.1016/0014-3057(87)90165-0 ↗
11. Photo-Oxidation of Elastomeric Materials. Part 1-Photo-Oxidation of Polybutadienes10.1016/0141-3910(89)90091-8 ↗
12. Photo-Oxidation Of Elastomeric Materials: Part IV-Photo-Oxidation of 1,2-Polybutadiene10.1016/0141-3910(90)90042-6 ↗
13. The Chemical Effects of Photo-Oxidation on Butadiene Rubber10.1016/0014-3057(83)90145-3 ↗
14. Mechanistic Studies on the Photo-Oxidation of Commercial poly(butadiene)10.1016/0014-3057(74)90167-0 ↗
15. Photo-Oxidation of Elastomeric Materials: Part II-Photo-Oxidation of Styrene-Butadiene Copolymer10.1016/0141-3910(89)90079-7 ↗
16. Boutamdja, M. , 2006, “Synthesis and Characterization of UV Absorber: 2-Hydroxy-4′-Vinyl Benzophenone,” Ph.D. thesis, University of Hadj Lakhdar de Batna, Batna, Algeria.
17. Chemical Modifications, Mechanical Properties and Surface Photo-Oxidation of Films of Polystyrene (PS)10.1016/j.polymertesting.2003.10.001 ↗
18. The Photo-Oxidation of EPDM Rubber: Part V-Mechanical Properties Degradation of Vulcanized Filled Samples10.1016/0141-3910(92)90021-V ↗
19. Chemistry of the Vulcanization and Protection of Elastomers: A Review of the Achievements10.1002/app.v87:1 ↗
20. Influence of Copper-Phthalocyanine on The Photodegradation of Polycarbonate10.1016/j.polymdegradstab.2006.06.004 ↗
21. Influence of Pigments on The Light Stability of Polymers: A Critical Review10.1016/0144-2880(83)90042-8 ↗
22. Photofading And Light Stability of Dyed and Pigmented Polymers10.1016/0141-3910(94)90095-7 ↗
23. Photo- and Thermal Ageing of Polychloroprene: Effect of Carbon Black and Crosslinking10.1016/0141-3910(96)00097-3 ↗
24. The Influence of CB Loading on Thermal Aging Resistance of SBR and NBR Rubber Compounds Under Different Aging Temperature10.1016/j.matdes.2008.05.065 ↗
25. NMR Study of Styrene-Butadiene Rubber (SBR) and Tio2 Nanocomposites10.1016/j.polymertesting.2009.03.011 ↗
26. Photo-Oxidation of Commercial Polyethylene Containing Titanium Dioxide (rutile)/Antioxidant Systems10.1007/BF00540845 ↗
27. Stabiliser Interactions in the Thermal and Photooxidation of Titanium Dioxide Pigmented Polypropylene films10.1016/S0141-3910(97)00143-2 ↗
28. An Influence of Micron and Nano-Particle Titanium Dioxides on the Efficiency of Antioxidant Irganox 1010 in a Model Oxidative Reaction10.1016/j.polymdegradstab.2004.03.017 ↗
29. Thermal Ageing of Acrylonitrile-Butadiene Copolymer10.1016/S0141-3910(00)00035-5 ↗
30. Silicone Rubbers Filled With Tio2: Characterization and Photocatalytic Activity10.1016/j.matchemphys.2008.07.104 ↗
31. Degradation Of Carboxylated Styrene Butadiene Rubber Based Water Born Paints. Part 1: Effect of Talc Filler and Titania Pigment on UV Stability10.1016/j.polymdegradstab.2007.04.016 ↗
32. Influence of Sio2 Fillers on the Irradiation Ageing of Silicone Rubbers10.1016/S0032-3861(01)00470-0 ↗
33. Influence of Copper-Phthalocyanine on the Photodegradation of Polycarbonate10.1016/j.polymdegradstab.2006.06.004 ↗
34. Light Protective Action of Azo Compounds in Polydienes10.1016/0144-2880(84)90061-7 ↗
35. Structure of Azo Compounds and Effectiveness of Their Light-Screening Effect in Elastomers
36. N-Phenyl-3-Substituted 5 Pyrazolone Derivatives as Organic Stabilizers for Rigid Poly(vinyl chloride) Against Photodegradation10.1002/app.v101:3 ↗
37. Organic Thermal Stabilizers For Rigid Poly(Vinyl Chloride). Part XII: N-Phenyl-3-Substituted-5-Pyrazolone Derivatives10.1016/j.polymdegradstab.2005.05.031 ↗
38. The Effect of Environmental Conditions on Electron Beam Cross-linked Agricultural Polyethylene Films
39. Thermal Degradation of Polystyrene, Poly(1,4-butadiene) and Copolymers of Styrene and 1,4-Butadiene Irradiated Under Air or Argon With 60Co-γ-rays10.1016/S0141-3910(98)00114-1 ↗
40. Zweifel
41. FTIR Imaging of Oxidation of Polyisoprene 2. The Role of N-Phenyl-N′-Dimethyl-Butyl-p-Phenylenediamine antioxidant10.1016/S0141-3910(03)00109-5 ↗