Experimental Investigation and Constitutive Modeling for Hot Deformation Behavior of 2219 Al-Alloy Microalloyed With Silver
Source abstract
Abstract
2219Al and 2219Al + 0.1 wt % Ag alloys were processed by casting route. The hot compression tests were carried out at constant true strain rates and temperatures in the range of 10−3 to 101 s−1 and 300–500 °C, respectively. Flow stress of the alloy decreases with the addition of silver. The flow stress of both alloys increases with the decrease in deformation temperature and the increase in strain rates. Constitutive models correlating the peak flow stress with deformation temperature and strain rates for the two alloys were developed using hyperbolic–sine relationship. The activation energy for hot deformation of 2219 Al alloy decreases with the addition of silver. Comparison of the predicted and experimental values of peak flow stress reveals that 92% of the data could be predicted within a deviation error of ±10% indicating good predictive capability for the developed constitutive relationships.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metallurgy and Material Forming · Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Mechanical Engineering, Indian Institute of Technology Guwahati, Guwahati 781039, India e-mail:
References (35)
Show source-provided references
1. Studies on Squeeze Casting of Al 2124 Alloy and 2124-10% SiCp Metal Matrix Composite10.1016/j.msea.2008.01.054 ↗
2. Effect of Different Aging Processes on the Microstructure and Mechanical Properties of a Novel Al–Cu–Li Alloy10.1016/j.jmst.2016.01.018 ↗
3. Effect of Pre-Deformation on Microstructure and Mechanical Properties of 2219 Aluminum Alloy Sheet by Thermomechanical Treatment10.1016/S1003-6326(12)61733-6 ↗
4. Influence of Deformation Ageing Treatment on Microstructure and Properties of Aluminum Alloy 261810.1016/j.matchar.2007.08.007 ↗
5. Hot Deformation Behavior and Microstructural Evolution of Ag-Containing 2519 Aluminum Alloy10.1016/j.matdes.2009.10.061 ↗
6. Classification of the Role of Microalloying Elements in Phase Decomposition of Al Based Alloys10.1016/S1359-6454(99)00475-9 ↗
7. Mechanical Properties and Microstructure of Aluminum Alloy 2618 With Al3(Sc, Zr) Phases10.1016/j.msea.2003.09.092 ↗
8. Microstructure and High Temperature Stability of Age Hardenable AA2219 Aluminium Alloy Modified by Sc, Mg and Zr Additions10.1016/j.msea.2007.01.144 ↗
9. Effect of Trace Additions of Sn on Microstructure and Mechanical Properties of Al–Cu–Mg Alloys10.1016/j.matdes.2010.03.012 ↗
10. Influence of Indium Trace Addition on the Precipitation Behavior in a 357 Cast Aluminum Alloy10.1007/s11665-007-9086-3 ↗
11. Constitutive Equation and Processing Maps of an Al–Mg–Si Aluminum Alloy: Determination and Application in Simulating Extrusion Process of Complex Profiles10.1016/j.matdes.2015.12.113 ↗
12. Constitutive Modeling of Deformation in High Temperature of a Forging 6005A Aluminum Alloy10.1016/j.matdes.2013.08.037 ↗
13. Constitutive Behavior of Aluminum Alloy in a Wide Temperature Range From Warm to Semi-Solid Regions10.1016/j.jallcom.2016.02.254 ↗
14. Hot Deformation of the Extruded Mg–10Li–1Zn Alloy: Constitutive Analysis and Processing Maps10.1016/j.jallcom.2016.12.087 ↗
15. Dynamic Recrystallization and Precipitation Behavior of Mn-Cu-V Weathering Steel10.1016/S1005-0302(12)60008-5 ↗
16. High Temperature Deformation Behavior of Al–Cu–Mg Alloys Micro-Alloyed With Sn10.1016/j.msea.2010.01.052 ↗
17. Processing Maps for Hot Working Behavior of a PM TiAl Alloy10.1016/S1005-0302(11)60161-8 ↗
18. Flow Behavior and Microstructure Evolution of 6A82 Aluminium Alloy With High Copper Content During Hot Compression Deformation at Elevated Temperatures10.1016/S1003-6326(16)64154-7 ↗
19. Characterization of Hot Deformation Behavior of as-Homogenized Al–Cu–Li–Sc–Zr Alloy Using Processing Maps10.1016/j.msea.2014.07.031 ↗
20. Difference in the Hot Compressive Behavior and Processing Maps Between the as-Cast and Homogenized Al–Zn–Mg–Cu (7075) Alloys10.1016/j.jmst.2016.04.006 ↗
21. Deformation Behavior and Microstructure Evolution of 7050 Aluminum Alloy During High Temperature Deformation10.1016/j.msea.2007.10.051 ↗
22. General Expression of the Zener–Hollomon Parameter as a Function of the Chemical Composition of Low Alloy and Microalloyed Steels10.1016/1359-6454(95)00151-0 ↗
23. Modeling High-Temperature Stress-Strain Behavior of Cast Aluminum Alloys10.1007/s11661-999-0201-y ↗
24. Deformation Behavior of a 2219 Al Alloy10.1016/S0921-5093(01)01777-4 ↗
25. Hot Deformation Behavior of AA7085 Aluminum Alloy During Isothermal Compression at Elevated Temperature10.1016/j.msea.2013.12.012 ↗
26. Prediction of Hot Deformation Behavior of Al–5.9% Cu–0.5% Mg Alloys With Trace Additions of Sn10.1007/s10853-011-5873-1 ↗
27. Constitutive Analysis in Hot Working10.1016/S0921-5093(01)01117-0 ↗
28. Flow Behavior and Microstructural Evolution of Al–Cu–Mg–Ag Alloy During Hot Compression Deformation10.1016/j.msea.2008.09.028 ↗
29. Evolution of Activation Energy During Hot Deformation of AA7150 Aluminum Alloy10.1016/j.msea.2013.01.080 ↗
30. Effect of Zr Addition on Hot Deformation Behavior and Microstructural Evolution of AA7150 Aluminum Alloy10.1016/j.msea.2013.12.057 ↗
31. Effects of Zr and V Micro-Alloying on Activation Energy During Hot Deformation of 7150 Aluminum Alloys
32. Nucleation of Precipitates in Aged Al–Cu–Mg–(Ag) Alloys With High Cu:Mg Ratios10.1016/1359-6454(95)00314-2 ↗
33. Strain-Compensated Arrhenius-Type Constitutive Model for Flow Behavior of Al-12Zn-2.4 Mg-1.2 Cu Alloy10.1016/S1875-5372(16)30009-1 ↗
34. Effect of Initial Microstructure on the Hot Compression Deformation Behavior of a 2219 Alumnum Alloy10.1016/j.matdes.2011.07.061 ↗
35. Hot Deformation Behavior of 2026 Aluminum Alloy During Compression at Elevated Temperature10.1016/j.msea.2009.09.042 ↗