Constitutive Behavior for Quenching of Al–Cu–Mg Alloy With Consideration of Precipitation
Source abstract
Abstract
The deformation behavior of as-quenched 2024 Al–Cu–Mg alloy has been experimentally studied. The experiments are designed to cool specimens to the desired temperature with a constant cooling rate, i.e., 5 K/s. Isothermal tensile tests are performed over a range of 573–723 K temperature and (0.01, 0.1, and 1 s−1) strain rates to find out the flow stresses and microstructures after deformation. Due to the nonuniform deformation mechanisms (solid solution versus solid solution and precipitation), two types of Arrhenius model are established for the temperature range of 573–673 K and 673–723 K, respectively. For temperature between 573 and 673 K, the activation energy is dependent on temperature and strain rate, and the value of activation energy decreases with the increases of temperature and strain rate. Compared with the ideal variation trend with no consideration of precipitation, the largest difference of activation energy is found at the temperature of 623 K which is the nose temperature of 2024 alloy.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Metallurgy and Material Forming · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Mechanical Engineering, Northwestern Polytechnical University, 127 West Youyi Road, Xi'an 710072, China e-mail:
School of Mechanical Engineering, Northwestern Polytechnical University, Xi'an 710072, China e-mail:
Funding
National Natural Science Foundation of China
References (35)
Show source-provided references
1. Recent Developments in Advanced Aircraft Aluminium Alloys10.1016/j.matdes.2013.12.002 ↗
2. Analytical and Computational Methodology for Modeling Spray Quenching of Solid Alloy Cylinders10.1016/j.ijheatmasstransfer.2010.06.055 ↗
3. An Experimental Study of Heat Transfer in Aluminum Castings During Water Quenching10.1016/j.jmatprotec.2010.07.026 ↗
4. Quench Induced Residual Stress Prediction in Heat Treatable 7xxx Aluminium Alloy Thick Plates Using Gleeble Interrupted Quench Tests10.1016/j.jmatprotec.2015.03.029 ↗
5. Chobaut, N., 2015, “Measurements and Modelling of Residual Stresses During Quenching of Thick Heat Treatable Aluminium Components in Relation to Their Precipitation State,” Ph.D. thesis, Swiss federal Institute of Technology, Lausanne, Switzerland.https://infoscience.epfl.ch/record/205768?ln=en
6. 50th Anniversary Article: The Origin and Management of Residual Stress in Heat-Treatable Aluminum Alloys10.1111/str.12091 ↗
7. Constitutive Behaviour of A356 During the Quenching Operation10.1016/j.msea.2004.06.004 ↗
8. Hot Compressive Deformation Behavior of the As-Quenched A357 Aluminum Alloy10.1016/j.mseb.2012.02.020 ↗
9. Constitutive Behavior of As-Quenched Al–Cu–Mn Alloy10.1142/S0217984913410364 ↗
10. Characterisation of Precipitation Upon Cooling of an AA2618 Al–Cu–Mg Alloy10.1016/j.jallcom.2015.09.113 ↗
11. Temperature-Dependent Constitutive Behavior With Consideration of Microstructure Evolution for As-Quenched Al–Cu–Mn Alloy10.1016/j.msea.2016.09.090 ↗
12. Continuous Cooling Precipitation Diagram of Aluminium Alloy AA7150 Based on a New Fast Scanning Calorimetry and Interrupted Quenching Method10.1016/j.matchar.2016.08.016 ↗
13. Continuous Cooling Precipitation Diagrams of Al–Mg–Si Alloys10.1016/j.msea.2012.04.033 ↗
14. Development of Continuous Cooling Precipitation Diagrams for Aluminium Alloys AA7150 and AA702010.1016/j.jallcom.2013.09.014 ↗
15. Schloth, P., 2015, “Precipitation in the High Strength AA7449 Aluminum Alloy: Implications on Internal Stresses on Different Length Scales,” Ph.D. thesis, Swiss federal Institute of Technology in Lausanne, Switzerland.https://infoscience.epfl.ch/record/208831?ln=en
16. Analysis of Residual Strain and Stress States Due to Heat Treatment and Thermal Processing10.1243/03093247JSA418 ↗
17. A Critical Review of Experimental Results and Constitutive Descriptions for Metals and Alloys in Hot Working10.1016/j.matdes.2010.11.048 ↗
18. Fribourg, G., 2009, “Precipitation and Plasticity Couplings in a 7xxx Aluminum Alloy: Application to Thermo-Mechanical Treatments for Distortion Correction of Aerospace Components,” Ph.D. thesis, Institute National Polytechnique de Grenoble, France.
19. Strain Hardening Behavior of a Friction Stir Welded Magnesium Alloy10.1016/j.scriptamat.2007.08.001 ↗
20. Tensile Properties and Strain-Hardening Behavior of Double-Sided Arc Welded and Friction Stir Welded AZ31B Magnesium Alloy10.1016/j.msea.2010.01.031 ↗
21. Effects of Aluminum Content and Strain Rate on Strain Hardening Behavior of Cast Magnesium Alloys During Compression10.1016/j.msea.2013.11.078 ↗
22. Effect of Strain Rate Upon Plastic Flow of Steel10.1063/1.1707363 ↗
23. Strength and Structure Under Hot-Working Conditions10.1179/mtlr.1969.14.1.1 ↗
24. Constitutive Equations for High Temperature Flow Stress of Aluminium Alloys10.1179/mst.1997.13.3.210 ↗
25. Constitutive Analysis in Hot Working10.1016/S0921-5093(01)01117-0 ↗
26. Evolution of Activation Energy During Hot Deformation of AA7150 Aluminum Alloy10.1016/j.msea.2013.01.080 ↗
27. Modeling Quench Sensitivity of Aluminum Alloys for Multiple TEM PERS and Properties: Application to AA202410.1007/s11661-010-0359-3 ↗
28. Huang: Hot Deformation Behavior of 7150 Aluminum Alloy During Compression at Elevated Temperature10.1016/j.matchar.2008.12.012 ↗
29. 2011 · 205
30. Characterization of Hot Workability in AA 7050 Aluminum Alloy Using Activation Energy and 3-D Processing Map10.1016/j.jmatprotec.2015.05.018 ↗
31. Hardening of an Al–Cu–Mg Alloy Containing Types I and II S Phase Precipitates10.1016/j.matdes.2009.12.048 ↗
32. Influence of Pre-Deformation and Aging of an Al–Zn–Mg Alloy—II: Modeling of Precipitation Kinetics and Yield Stress10.1016/S1359-6454(98)00296-1 ↗
33. Solute Strengthening From First Principles and Application to Aluminum Alloys10.1016/j.actamat.2012.03.037 ↗
34. Work Hardening Descriptions in Simulation of Sheet Metal Forming Tailored to Material Type and Processing10.1016/j.ijplas.2015.11.002 ↗
35. Early Cluster Formation During Rapid Cooling of an Al–Cu–Mg Alloy: In Situ Small-Angle X-Ray Scattering10.1016/j.scriptamat.2015.06.015 ↗