Reducing Residual Stress in 7050 Aluminum Alloy Die Forgings by Heat Treatment
Source abstract
Abstract
Aerospace aluminum alloy forgings can have the residual stresses arising from heat treatment reduced by modification to the quench cooling rates and subsequent aging treatments. A series of propeller hubs usually made from the alloy 2014 have been closed die forged from the less quench sensitive alloy 7050. These forgings have been subjected to various quenching and aging treatments in an attempt to improve the balance of mechanical properties with the residual stress magnitudes. These forgings were not amenable to stress relieving by cold compression or stretching. Warm water (60°C) and boiling water quenches are investigated in addition to quenching into molten salt (200°C) and uphill quenching from −196°C. Various dual aging treatments including retrogression and reaging have been evaluated in an attempt to optimize low residual stress magnitudes with mechanical properties. Residual stresses determined by the center hole-drilling strain-gauge method are reported in addition to electrical conductivity, stress corrosion cracking, fracture toughness, initiation fatigue, and tensile mechanical property variations. It was found that quenching into boiling water and salt at 200°C did substantially reduce the residual stress but had only a small detrimental effect on the majority of the properties measured. However, the influence of quench rate on fracture toughness was much more significant. This is attributed to both coarse grain boundary precipitation and heterogeneous precipitation of η on Al3Zr dispersoids within the grains, which promotes easier crack propagation.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Welding Techniques and Residual Stresses · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials Science and Technology, University of Limerick, Limerick, Ireland
Department of Manufacturing and Operations Engineering, Materials and Surface Science Institute, University of Limerick, Limerick, Ireland
References (22)
Show source-provided references
1. Heat Treating of Aluminum Alloys
2. Polmear
3. U.S. Department of Defense, 2003, “Metallic Materials and Elements for Aerospace Vehicle Structures,” Document No. MIL-HDBK-5J.
4. Aluminum Alloys for Aircraft Structures
5. Uphill Quenching of Aluminum: Rebirth of a Little-Known Process
6. Effect of Retrogression and Reaging Treatments on the Microstructure of Al-7075-T651
7. Thirty Years of Retrogression and Re-Aging (RRA)
8. The Effect of Heating Shot Peened Sheets and Thin Plates of Aluminium Alloys10.1007/BF00582488 ↗
9. Development of Large High Strength Aluminium Alloy Component for Spacecraft
10. U.S. Department of Defense, 1991, “Heat Treatment of Aluminum Alloys,” Document No. MIL-H-6088G.
11. A Contribution to the Optimisation of the 7075 Heat Treatment10.1016/0025-5416(80)90200-1 ↗
12. Society of Automotive Engineers (SAE), 1992, “Aluminum Alloy Die Forgings 6.2ZN-2.3CU-2.2MG-0.12ZR (7050-T74) Solution Heat Treated and Overaged,” Document No. AMS 4107D.
13. Henry
14. Fatigue Crack Growth Rate Measurements in Aluminium Alloy Forgings: Effects of Residual Stress and Grain Flow
15. Grain Boundary Ductile Fracture in Precipitation Hardened Aluminium Alloys10.1016/0001-6160(87)90001-0 ↗
16. Influence of Quench and Heating Rates on the Ageing Response of an Al-Zn-Mg-(Zr) Alloy
17. Nature and Distribution of Quench-Induced Precipitation in an Al-Zn-Mg-Cu Alloy10.1016/S1359-6462(98)00357-1 ↗
18. On the Relationship Between Microstructure, Strength and Toughness in AA7050 Aluminum Alloy
19. Characterisation of Precipitation Microstructures in Aluminium Alloys 7040 and 7050 and Their Relationship to Mechanical Behaviour10.1179/026708304225016662 ↗
20. The Thermal Mechanical Method for Relieving Residual Quench Stresses in Aluminum Alloys
21. Pellman, M. A., Kilhefner, P. T., Baxter, W. J., and Hahn, T. S., 1990, “Vapor Phase Uphill Quenching of Metal Alloys Using Fluorochemicals,” U.S. Patent No. 4,968,358.
22. Thermal Stress Relief in 7050 Aluminum Forgings by Uphill Quenching