Quantitative Interfacial Energy Measurements of Adhesion-Promoted Thin Copper Films by Supercritical Fluid Deposition on Barrier Layers
Source abstract
Abstract
A fivefold increase in adhesion energy is observed for poly(acrylic acid) (PAA) modified Cu/TaN interfaces in which the thin copper films are deposited by the hydrogen assisted reduction of bis(2,2,7-trimethyloctane-3,5-dionato) copper in supercritical carbon dioxide. The PAA adhesion layer is sacrificial at the reaction conditions used, and X-ray photoelectron spectroscopy has shown that the Cu/TaN interface is free of contamination following deposition. The resulting average interfacial adhesion energy is just above 5 J/m2, which meets adhesion requirements for integration in Cu interconnects. The adhesion measurements are performed with a custom built four-point bend fracture mechanics testing system. Comparison of the copper film thickness to the measured adhesion energy indicated that there is no effect on the adhesion energy as the film thickness changes.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Copper Interconnects and Reliability · Metal and Thin Film Mechanics · Electronic Packaging and Soldering Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Chemical Engineering, University of Massachusetts Amherst, Amherst, MA 01003
School of Engineering and Applied Science, Harvard University, Cambridge, MA 02138
Department of Polymer Science and Engineering, University of Massachusetts Amherst, Amherst, MA 01003
References (65)
Show source-provided references
1. Adhesion and Reliability of Copper Interconnects With Ta and TaN Barrier Layers10.1557/JMR.2000.0033 ↗
2. Comparative Study of Tantalum and Tantalum Nitrides (Ta2N and TaN) as a Diffusion Barrier for Cu Metallization10.1116/1.588818 ↗
3. Diffusion Barrier Property of TaN Between Si and Cu10.1016/0169-4332(96)00464-3 ↗
4. Comparison of the Diffusion Barrier Properties of Chemical-Vapor-Deposited TaN and Sputtered TaN Between Cu and Si10.1063/1.361518 ↗
5. Chemical Vapor Deposition of Metals: Part 1. An Overview of CVD Processes10.1002/cvde.19950010103 ↗
6. Chemical Vapor Deposition of Metals: Part 2. Overview of Selective CVD of Metals10.1002/cvde.19950010202 ↗
7. Chemical Studies of CVD Cu Deposited on Ta and TaN Barriers Under Various Process Conditions10.1016/S0167-9317(99)00383-4 ↗
8. Adhesion Studies of CVD Copper Metallization10.1016/S0167-9317(99)00326-3 ↗
9. Atomic Layer Deposition of Metal and Nitride Thin Films: Current Research Efforts and Applications for Semiconductor Device Processing10.1116/1.1622676 ↗
10. Evaluation of CVD/PVD Multilayered Seed for Electrochemical Deposition of Cu-Damascene Interconnects10.1109/16.998578 ↗
11. Plasma-Enhanced Atomic Layer Deposition of Tantalum Nitrides Using Hydrogen Radicals as a Reducing Agent10.1149/1.1353160 ↗
12. Plasma-Enhanced Atomic Layer Deposition of Ta and Ti for Interconnect Diffusion Barriers10.1116/1.1305809 ↗
13. Chemical Vapor Deposition of Vanadium, Niobium, and Tantalum Nitride Thin Films10.1021/cm00029a007 ↗
14. Deposition of Conformal Copper and Nickel Films From Supercritical Carbon Dioxide10.1126/science.1064148 ↗
15. Deposition of Gold Films and Nanostructures From Supercritical Carbon Dioxide10.1021/cm034739u ↗
16. Reactive Deposition of Conformal Ruthenium Films From Supercritical Carbon Dioxide10.1021/cm060142d ↗
17. Reactive Deposition of Conformal Metal Oxide Films From Supercritical Carbon Dioxide10.1021/cm070288s ↗
18. Solubility of β-Diketonates, Cyclopentadienyls, and Cyclooctadiene Complexes With Various Metals in Supercritical Carbon Dioxide10.1016/j.supflu.2006.10.011 ↗
19. Solubilities of Copper(II) and Chromium(III) β-Diketonates in Supercritical Carbon Dioxide10.1021/ic00127a015 ↗
20. Solubility of Chelating Agents and Metal-Containing Compounds in Supercritical Fluid Carbon Dioxide10.1016/S0039-9140(96)02008-5 ↗
21. Polyelectrolyte Nanolayers as Diffusion Barriers for Cu Metallization10.1063/1.1618951 ↗
22. Self-Assembled Near-Zero-Thickness Molecular Layers as Diffusion Barriers for Cu Metallization10.1063/1.1365418 ↗
23. Self-Assembled Subnanolayers as Interfacial Adhesion Enhances and Diffusion Barriers for Integrated Circuits10.1063/1.1591232 ↗
24. Interaction of Polymeric Si:C:H Films With Copper Substrates and With Deposited Cu Adatoms10.1016/S0169-4332(01)01028-5 ↗
25. Polymerized C-Si Films on Metal Substrates: Cu Adhesion/Diffusion Barriers for Ultralarge Scale Integration?10.1116/1.581712 ↗
26. Contact Adhesion of Thin Gold Films on Elastomeric Supports: Cold Welding Under Ambient Conditios10.1126/science.253.5021.776 ↗
27. Annealing-Induced Interfacial Toughening Using a Molecular Nanolayer10.1038/nature05826 ↗
28. The Self-Formatting Barrier Characteristics of Cu—Mg/SiO2 and Cu—Ru/SiO2 Films for Cu Interconnects10.1016/j.microrel.2007.12.005 ↗
29. The Effect of Seed Metal on the Surface Morphology of Copper Foil and Adhesion Property
30. Electrical Reliability and Interfacial Adhesion of Cu(Mg) Thin Films for Interconnect Process Adaptability10.1016/j.tsf.2007.08.134 ↗
31. Capacitance-Voltage, Current-Voltage, and Thermal Stability of Copper Alloyed With Aluminum or Magnesium10.1016/S0040-6090(98)00878-5 ↗
32. Alloying of Copper for use in Microelectronic Metallization10.1016/0254-0584(95)01513-2 ↗
33. Stress Effects in Thermal Cycling of Copper (Magnesium) Thin Films10.1063/1.113907 ↗
34. Effects of the Addition of Small Amounts of Al to Copper: Corrosion, Resistivity, Adhesion, Morphology, and Diffusion10.1063/1.356075 ↗
35. Oxidation Resistant High Conductivity Copper Films10.1063/1.111408 ↗
36. Sacrificial Adhesion Promotion Layers for Copper Metallization of Device Structures10.1021/la048731q ↗
37. ASTM Standard D3359-08, 2003, “Standard Test Methods for Measuring Adhesion by Tape Test,” ASTM International, West Conshohocken, PA, www.astm.org.
38. A Review of the Methods for the Evaluation of Coating-Substrate Adhesion10.1016/0921-5093(91)90482-3 ↗
39. Adhesion Measurement of Thin-Films10.1155/APEC.3.21 ↗
40. Adhesion10.1016/0376-4583(81)90005-4 ↗
41. The Scratch Test: Different Critical Load Determination Techniques10.1016/0257-8972(88)90179-X ↗
42. Thin-Film Adhesion – A Review of the Mechanical Methods for Adhesion Assessment
43. A Review of the Mechanical Tests for Assessment of Thin-Film Adhesion10.1116/1.575926 ↗
44. Adhesion Testing by the Scratch Test Method: The Influence of Intrinsic and Extrinsic Parameters on the Critical Load10.1016/0040-6090(87)90377-4 ↗
45. Nanoindentation-Induced Defect—Interface Interactions: Phenomena, Methods and Limitations10.1016/S1359-6454(99)00270-0 ↗
46. A New Indentation Cracking Method for Evaluating Interfacial Adhesion Energy of Hard Films10.1016/S0040-6090(03)00920-9 ↗
47. Effect of Residual Stress on Delamination From Interface Edge Between Nano-Films10.1016/S0013-7944(02)00254-0 ↗
48. Quantitative Adhesion Measures of Multilayers Films: Part I. Indentation Mechanics10.1557/JMR.1999.0404 ↗
49. Quantitative Adhesion Measures of Multilayers Films: Part II. Indentation of W/Cu, W/W, Cr/W10.1557/JMR.1999.0405 ↗
50. Adhesion Evaluation of Immersion Plating Copper Films on Silicon by Microindentation Measurements10.1016/S0040-6090(03)00469-3 ↗
51. A Test Specimen for Determining the Fracture Resistance of Bimaterial Interfaces10.1115/1.3176069 ↗
52. Adhesion and Debonding of Multi-Layer Thin Film Structures10.1016/S0013-7944(98)00052-6 ↗
53. The Effect of Residual Stresses on the Debonding of Coatings—I. A Model for Delamination at a Bimaterial Interface10.1016/0956-7151(94)90223-2 ↗
54. Four-Point Bend Adhesion Measurements of Copper and Permalloy Systems10.1016/S0013-7944(03)00100-0 ↗
55. A Four Point Bending Technique for Studying Subcritical Crack Growth in Thin Films and at Interfaces10.1557/JMR.1997.0122 ↗
56. Crack Penetration and Deflection at a Bimaterial Interface in a Four-Point Bend Test10.1557/JMR.2004.0376 ↗
57. Interfacial Adhesion of Copper-Low k Interconnects
58. The Effect of Residual Stresses on the Debonding of Coatings—II. An Experimental Study of a Thermally Sprayed System10.1016/0956-7151(94)90224-0 ↗
59. Vapor Deposition of Ruthenium From an Amidinate Precursor10.1149/1.2789294 ↗
60. Nucleation and Adhesion of ALD Copper on Cobalt Adhesion Layers and Tungsten Nitride Diffusion Barriers10.1149/1.1924929 ↗
61. Outstanding Meeting Paper: Constraint Effects on Thin Film Channel Cracking Behavior10.1557/jmr.2005.0317 ↗
62. Fracture of Organosilicate Glass Thin Films: Environmental Effects10.1016/j.msea.2004.08.070 ↗
63. Zong, Y. , 2004, “Chemical Engineering,” Ph.D. thesis, University of Massachusetts Amherst, Amherst, MA.
64. Deposition of Copper by the H2-Assisted Reduction of Cu(tmod)2 in Supercritical Carbon Dioxide: Kinetics and Reaction Mechanism10.1021/cm048665d ↗
65. Calculated Elastic Constants for Stress Problems Associated With Semiconductor Devices10.1063/1.1661935 ↗