Fatigue-Crack Propagation Behavior of Incoloy 800 at Elevated Temperatures
Source abstract
Abstract
Linear-elastic fracture mechanics techniques were used to characterize the fatigue-crack propagation behavior of Incoloy 800 in an air environment over the temperature range 75 to 1200 deg F (24 to 649 deg F). Crack growth rates were measured over the range 5×10−7 to 5×10−5 in./cycle. Material Grades 1 and 2 were found to exhibit essentially the same behavior over this range. In general, crack growth rates increased with increasing test temperature, although the increases were less then previously noted for austenitic stainless steels. This difference is probably related to the superior oxidation resistance of Incoloy 800.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Fatigue and fracture mechanics · Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Westighouse Hanford Co., Richland, Wash.
References
Reference metadata was not supplied for this record.