Review of Fe-6.5 wt%Si high silicon steel—A promising soft magnetic material for sub-kHz application
Source abstract
Abstract
To meet the growing need for energy efficiency in power electronics and electric machines, a number of new soft magnetic materials are being investigated. Among them, high silicon Fe-Si alloy has been recognized as a promising candidate for low-to-medium-frequency applications. Compared to the currently most widely used 3 wt% silicon steel, the steel containing 6.5 wt% Si possesses more favorable properties, including high electrical resistivity, good saturation magnetization, and near-zero magnetostriction. However, the high silicon content facilitates the formation of ordered phases, resulting in severe brittleness that prohibits mass production using the economical conventional processing methods. A number of new processing routes have been investigated and inspiring progress has been made. Prototypes of motors and transformers using high silicon steel have been demonstrated with improved efficiency and power density. If the processing cost and limitations of size and shape are properly addressed, high silicon steel is expected to be widely adopted by the industries. Among all the investigated processing techniques, rapid solidification appears to be the most cost-effective method for mass producing thin sheet of high silicon steel. This paper reviews the current state-of-the-art of the Fe-Si based soft magnetic materials including their history, structure, properties, processing, and applications.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Magnetic Properties and Applications · Magnetic Properties of Alloys · Metallic Glasses and Amorphous Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. Cullity · 2008
2. U.S. Department of Energy, Premium Efficiency Motor Selection and Application Guide. https://www.energy.gov/sites/prod/files/2014/04/f15/amo_motors_handbook_web.pdf, 2014, (accessed 11/28/2018).
3. Teknomotor Product Catalog http://www.teknomotor.com/pdf/catalogo.pdf, (accessed 11/28/2018).
4. The Scale up of Wide Bandgap Power Semiconductor Technology and Power Electronics. https://www.nist.gov/document-2981, (accessed 11/28/2018).
5. Influence of deformation process on the improvement of non-oriented electrical steel10.1016/S0304-8853(02)00965-4 ↗
6. Fiorillo · 2004
7. Iron and silicon-iron alloys10.1109/TMAG.1971.1066998 ↗
8. Recent development of non-oriented electrical steel sheets10.1016/0304-8853(82)90116-0 ↗
9. Super CoreTM Electrical steel sheets for high-frequency application, JFE Steel Corporation. http://www.jfe-steel.co.jp/en/products/electrical/catalog/f1e-002.pdf, (accessed 11/28/2018).
10. S. Constannides, Energy Savings with Thin Gauge Silicon-Iron, Arnold Magnetic Technologies. http://www.arnoldmagnetics.com/wp-content/uploads/2017/10/Energy-Savings-with-Thin-Gauge-Silicon-Iron-thingagesife_100213c_final-ppr.pdf, (accessed 11/28/2018).
11. Y. Chen, V.G. Harris, Magnetic grain boundary engineered ferrite core materials, Google Patents, 2015.
12. Recent development of low-loss grain-oriented silicon steel10.1016/S0304-8853(02)00933-2 ↗
13. Effect of grain size and magnetic texture on iron-loss components in NO electrical steel at different frequencies10.1016/j.jmmm.2018.07.073 ↗
14. Evidence for the effectiveness of stress coatings in improving the magnetic properties of high permeability 3% Si-Fe10.1109/TMAG.1979.1060469 ↗
15. The influence of compressive stress applied by hard coatings on the power loss of grain oriented electrical steel sheet10.1016/j.jmmm.2011.02.044 ↗
16. Effects of applied stress on the magnetic-properties of high permeability silicon-iron10.1109/TMAG.1979.1060392 ↗
17. L. Kestens, S. Jacobs, Texture Control During the Manufacturing of Nonoriented Electrical Steels, Texture, Stress, and Microstructure 2008(Article ID 173083), 2008. p. 9.10.1155/2008/173083 ↗
18. Influence of the manufacturing process on the magnetic properties of non-oriented electrical steels10.1016/S0304-8853(00)00070-6 ↗
19. Electrical conductivity and magnetic permeability of various alloys of Fe
20. Permalloy, a new magnetic material of very high permeability10.1002/j.1538-7305.1923.tb03595.x ↗
21. J.L. Snoek, Magnetic Core, 1948.
22. Amorphous ferromagnetic phase in iron-carbon-phosphorus alloys10.1063/1.1709084 ↗
23. Rapidly quenched ribbon-form silicon-iron alloy with high silicon concentration10.1016/0304-8853(80)90352-2 ↗
24. New Fe-based soft magnetic alloys composed of ultrafine grain structure10.1063/1.342149 ↗
25. Coey · 2010
26. Soft magnetic materials for a sustainable and electrified world10.1126/science.aao0195 ↗
27. Ferrite devices and materials10.1109/22.989957 ↗
28. Recent advances in processing and applications of microwave ferrites10.1016/j.jmmm.2009.01.004 ↗
29. Nonoriented electrical steels10.1007/s11837-012-0356-7 ↗
30. Soft magnetic material status and trends in electric machines10.1109/TIE.2016.2613844 ↗
31. Amorphous and nanocrystalline materials for applications as soft magnets10.1016/S0079-6425(99)00002-X ↗
32. Modern soft magnets: amorphous and nanocrystalline materials10.1016/j.actamat.2012.10.040 ↗
33. Development of new amorphous and nanocrystalline magnetic materials for use in energy-efficient devices10.1557/adv.2017.552 ↗
34. R.M. Bozorth, Ferromagnetism, Van Nostrand, New York, 1951.
35. Magnetic properties and workability of 6.5% Si steel sheet10.1016/0304-8853(96)00128-X ↗
36. Herzer · 2007
37. Magnetic materials and devices for the 21st century: stronger lighter, and more energy efficient10.1002/adma.201002180 ↗
38. Structure and magnetic properties of (Fe0.5Co0.5)88Zr7B4Cu1 nanocrystalline alloys10.1063/1.369007 ↗
39. Nanocrystalline soft magnetic Fe-Si-B-P-Cu alloys with high B of 1.8–1.9T contributable to energy saving10.1109/TMAG.2011.2175210 ↗
40. Jiles · 2015
41. Trade studies for a manganese bismuth based surface permanent magnet machine
42. E. Gumlich, D.I.P. Goerens, Magnetic properties of iron-carbon and iron-silicon alloys, 1912.10.1039/tf9120800098 ↗
43. On the magnetic properties of silicon iron (Stalloy) in alternating magnetic fields of low value10.1088/1478-7814/32/1/325 ↗
44. Beckley · 2002
45. Core loss reduction in electrical steels through materials processing10.1063/1.369134 ↗
46. Si-steel thin-strip prepared by twin-roll continuous casting10.1142/S0218625X11014515 ↗
47. Magnetostriction and applications of 6.5% Si steel sheet10.1063/1.348028 ↗
48. Effect of microstructure on the magnetic properties of 6.5% Si Fe alloy10.1016/0304-8853(92)91149-N ↗
49. Ribbon-form silicon-iron alloy containing around 6.5 percent silicon10.1109/TMAG.1980.1060560 ↗
50. Effect of wheel speed on magnetic and mechanical properties of melt spun Fe-6.5 wt.% Si high silicon steel10.1063/1.5006481 ↗
51. Fabrication of Fe-6.5 wt%Si ribbons by melt spinning method on large scale10.1155/2015/296197 ↗
52. Formation and electronic state of Do3-type ordered structure in sputtered Fe-Si thin-films10.1063/1.351091 ↗
53. Effect of composition on the loss of non-oriented medium silicon electric steels10.1016/0304-8853(84)90135-5 ↗
54. Effect of silicon on the loss separation and permeability of laminated steels10.1016/S0304-8853(96)00268-5 ↗
55. Magnetic properties of roller-quenched high silicon steel ribbons10.1016/0304-8853(82)90133-0 ↗
56. New magnetic materials10.1109/JRPROC.1942.232364 ↗
57. Ordering-disordering phenomena and micro-hardness characteristics of B2 phase in Fe-(5–6.5%)Si alloys10.1016/j.msea.2005.07.012 ↗
58. The B2 and DO3 ordering reactions in iron-silicon alloys in the vicinity of the curie temperature10.1179/030634575790445279 ↗
59. Order in Fe-Si alloys: a neutron diffraction study10.1016/j.physb.2006.05.364 ↗
60. Dieter · 1961
61. Effects of precipitated phase and order degree on bending properties of an Fe-6.5 wt%Si alloy with columnar grains10.1557/jmr.2011.136 ↗
62. Effect of ordering on magnetic properties of 6.5-percent silicon-iron alloy10.1109/TMAG.1979.1060174 ↗
63. The nature of dislocations and effect of order in rapidly solidified Fe–(5.5–7.5)wt.%Si alloys10.1016/0921-5093(93)90432-E ↗
64. Effect of quench cooling rate on residual stress, microstructure and mechanical property of an Fe-6.5Si alloy10.1016/j.msea.2011.10.013 ↗
65. Thermodynamic and kinetic analysis of the melt spinning process of Fe-6.5 wt.% Si alloy10.1016/j.jallcom.2018.08.293 ↗
66. Study of the brittle behaviour of annealed Fe-6.5 wt%Si ribbons produced by planar flow casting10.1016/0921-5093(96)10188-X ↗
67. Effect of cooling rate on order degree of 6.5 wt.% Si electrical steel after annealing treatment10.1109/TMAG.2015.2449899 ↗
68. Strain-softening behavior of an Fe–6.5 wt%Si alloy during warm deformation and its applications10.1016/j.msea.2010.10.093 ↗
69. Soft magnetic Ni-Fe and Co-Fe alloys – some physical and metallurgical aspects10.1016/0304-8853(80)90592-2 ↗
70. Grain size dependence of coercivity and permeability in nanocrystalline ferromagnets10.1109/20.104389 ↗
71. On the law of hysteresis10.1109/T-AIEE.1892.5570437 ↗
72. Calculation of losses in ferro- and ferrimagnetic materials based on the modified Steinmetz equation10.1109/28.936396 ↗
73. L. Jieli, T. Abdallah, C.R. Sullivan, Improved calculation of core loss with nonsinusoidal waveforms, in: Conference Record of the 2001 IEEE Industry Applications Conference. 36th IAS Annual Meeting (Cat. No.01CH37248), 2001, vol. 4. pp. 2203–2210.10.1109/IAS.2001.955931 ↗
74. K. Venkatachalam, C.R. Sullivan, T. Abdallah, H. Tacca, Accurate prediction of ferrite core loss with nonsinusoidal waveforms using only Steinmetz parameters, 2002 IEEE Workshop on Computers in Power Electronics, 2002. Proceedings, 2002, pp. 36–41.10.1109/CIPE.2002.1196712 ↗
75. Soft, magnetic materials10.1109/5.56909 ↗
76. Physical origin of losses in conducting ferromagnetic materials (invited)10.1063/1.330306 ↗
77. Calculation of the energy loss in magnetic sheet materials using a domain model10.1063/1.1723212 ↗
78. Effect of texture and grain size on the magnetic flux density and core loss of cold-rolled high silicon steel sheets10.1016/j.jmmm.2015.06.032 ↗
79. Investigation of total losses of non-oriented electrical steels
80. The optimum grain size for minimizing energy losses in iron10.1016/j.jmmm.2005.06.014 ↗
81. The effects of sulfur on magnetic properties of non-oriented electrical steel sheets10.1016/S0304-8853(02)00866-1 ↗
82. A new non-oriented silicon-steel with texture of [100] (Ovw)10.1016/0304-8853(80)90554-5 ↗
83. Newly developed electrical steel for high-frequency use10.1016/S0304-8853(01)01164-7 ↗
84. The effect of boron content on the processing for Fe–6.5wt% Si electrical steel sheets10.1016/j.jmmm.2003.11.012 ↗
85. N.P. Goss, Electrical sheet and method and apparatus for its manufacture and test, Google Patents, 1934.
86. Production and properties of melt-spun Fe-6.5wt.%Si ribbons10.1016/0025-5416(88)90295-9 ↗
87. Solidification structure and crystallographic texture of strip casting 3wt% Si non-oriented silicon steel10.1016/j.matchar.2011.02.010 ↗
88. Microstructure, texture and magnetic properties of strip casting Fe–6.2wt%Si steel sheet10.1016/j.jmatprotec.2012.04.015 ↗
89. Improvement of magnetic properties of an Fe-6.5 wt % Si alloy by directional recrystallization10.1063/1.3026742 ↗
90. Directional recrystallization and microstructures of an Fe-6.5 wt%Si alloy10.1557/jmr.2009.0303 ↗
91. Improvement of magnetic properties of an Fe–6.5 wt.% Si alloy by directional solidification10.1016/j.matlet.2011.02.020 ↗
92. Effect of magnetic annealing on the properties of (110) [001] oriented 3 14% silicon-iron strip10.1063/1.2185845 ↗
93. Heat treatment of magnetic materials in a magnetic field – I. Survey of iron-cobalt-nickel alloys
94. Iron-silicon alloys heat treated in a magnetic field10.1063/1.1700079 ↗
95. Magnetic-properties of commercially produced Fe-6.5wt-percent Si sheet10.1007/BF02833761 ↗
96. Grain oriented silicon steel sheet with a ceramic film characterized by ultra-low iron loss10.1016/0042-207X(96)00082-6 ↗
97. Laser processing for reducing core loss of grain oriented silicon steel10.1063/1.330828 ↗
98. Heatproof domain refining method using combination of local strain and heat-treatment for grain oriented 3-percent Si-Fe10.1088/0031-8949/1988/T24/005 ↗
99. Recent development of non-oriented electrical steel sheet for automobile electrical devices10.1016/j.jmmm.2008.03.054 ↗
100. A desirable material for transformer cores10.1007/BF02833762 ↗