Correlation between ordered solid solution and cellular structure of Sm2Co17 type magnets with high iron content

Cheng Xu, Hui Wang, Bingjie Liu, Hao Xu, Tianli Zhang, Jinghua Liu, Chengbao Jiang

Publisher page

Abstract

Abstract The ordering transformation of solid solution and the insufficient 1:5H boundary phase in the final magnets challenge the realization of high performance in Sm2Co17 magnets with high iron content. The investigation correlates the ordering degree of solid solutions to the cellular structure of the final magnets with the composition of Sm(CobalFexCu0.06Zr0.02)7.8 in which x ranges from 0.30 to 0.36. The ordering tendency of solid solution increases with increasing iron content. Rietveld structure refinement demonstrates that increasing iron content reduces the occupancy of Sm at Co-Co dumbbell sites in 2:17R, as well as Zr solubility on Sm 6c sites, leading to higher ordering degree and less Z planar phase formation separately. Antiphase boundaries (APBs) arising from the different 2:17R variants with the same or different directions were frequently observed in solid solutions, which facilitate the nucleation and formation of 1:5H phase during aging treatment. With increasing Fe content, the width of nanotwins increases and thus the APB density decreases in the solid solution. Furthermore, overlapping zones appear in solid solutions with higher Fe content, which will retain and enlarge as the twins grow during aging treatment, inhibiting the formation of 1:5H boundary phase. In addition, the density of Z phase declines and more defective platelet phases occur in x = 0.36 magnets, which depress the element diffusion and re-distribution during slow cooling. The above correlation between solid solution and cellular structure well explain the structure origin for the deterioration of magnetic performance with higher Fe content, which may provide guidance for further performance improvement in Sm2Co17 type magnets with higher iron content.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Hydrogen Storage and Materials · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Perspective and prospects for rare earth permanent magnets
2. Initial irreversible losses and enhanced high-temperature performance of rare-earth permanent magnets
3. Evolution of magnetic domain structures and coercivity in high-performance SmCo 2:17-type permanent magnets10.1016/j.actamat.2005.10.026 ↗
4. Hard magnetic materials: a perspective10.1109/TMAG.2011.2166975 ↗
5. Magnetic materials and devices for the 21st century: stronger, lighter, and more energy efficient10.1002/adma.201002180 ↗
6. Correlation of microstructure and magnetic properties in Sm(CobalFe0.1Cu0.1Zr0.033)6.93 magnets solution-treated at different temperatures10.1007/s12598-018-1182-z ↗
7. Identification of the cell boundary phase in the isothermally aged commercial Sm(Co0.725Fe0.1Cu0.12Zr0.04)7.4 sintered magnet10.1016/j.scriptamat.2005.12.009 ↗
8. Effect of Cu redistribution in grain boundary on magnetic properties of Sm(Co0.665Fe0.25Cu0.06Zr0.025)7 permanent magnets10.1016/j.jallcom.2018.01.164 ↗
9. Attractive-domain-wall-pinning controlled Sm-Co magnets overcome the coercivity-remanence trade-off10.1016/j.actamat.2018.10.046 ↗
10. Grain boundary modification induced magnetization reversal process and giant coercivity enhancement in 2:17 type SmCo magnets10.1016/j.jallcom.2019.01.217 ↗
11. Optimization of both coercivity and knee-point magnetic field of Sm2Co17-type magnets via solid solution process
12. Development of high-coercivity state in high-energy and high-temperature Sm-Co-Fe-Cu-Zr magnets upon step cooling
13. Atomic structure and domain wall pinning in samarium-cobalt-based permanent magnets10.1038/s41467-017-00059-9 ↗
14. The evolution of phase constitution and microstructure in iron-rich 2: 17-type Sm-Co magnets with high magnetic performance10.1038/s41598-018-27487-x ↗
15. Influence mechanism of Fe content on the magnetic properties of Sm2Co17-type sintered magnets: microstructure and microchemistry
16. The formation mechanism of 1: 5H phase in Sm(Co, Fe, Cu, Zr)z melt-spun ribbons with high iron content10.1016/j.jmmm.2019.165939 ↗
17. Effect of pre-aging treatment on the microstructure and magnetic properties of Sm(Co, Fe, Cu, Zr)7.8 sintered magnets10.2320/matertrans.MBW201325 ↗
18. Crystalline and magnetic microstructures of iron-rich Sm(Co0.65Fe0.26Cu0.07Zr0.02)7.8 sintered magnets: isothermal aging effect10.1016/j.jmmm.2018.06.047 ↗
19. Genesis of the cell microstructure in the Sm(Co, Fe, Cu, Zr) permanent magnets with 2: 17 type10.1002/pssa.2211400104 ↗
20. Micromagnetic analysis of pinning-hardened nanostructured, nanocrystalline Sm2Co17 based alloys10.1016/S1359-6462(02)00177-X ↗
21. Metallurgical behavior of Sm(Co, Fe, Cu, Zr)z alloys10.1063/1.333575 ↗
22. Variation of lattice parameters with composition of the RCo5 permanent magnets10.1002/pssa.2210210106 ↗
23. On the crystal structures of the R2Co17 intermetallic compounds10.1107/S0567740873006928 ↗
24. Structural effect of Zr substitution in the Sm2Co17 phase10.1016/S0925-8388(96)03023-X ↗
25. A new nanoscale metastable iron phase in carbon steels10.1038/srep15331 ↗
26. {1 1 2}< 1 1 1> Twinning during ω to body-centered cubic transition10.1016/j.actamat.2013.09.040 ↗
27. On the activation of alternated stacking fault pair twinning mechanism in a very large-grained Fe–29Mn–2.4 Al steel10.1016/j.scriptamat.2019.11.035 ↗
28. Role of nanoscale interfacial defects on magnetic properties of the 2: 17-type Sm–Co permanent magnets
29. Mechanism of phase transformation in 2:17 type SmCo magnets investigated by phase stabilization10.1016/j.scriptamat.2015.10.041 ↗
30. Coercivity kinetics upon step annealing of sintered Sm(Co0.88–xFexCu0. 09Zr0. 03)7 magnets10.1016/j.jre.2019.04.009 ↗
31. Rare earth cobalt compounds with the A2B17 structure10.1107/S0365110X66003451 ↗
32. A study of dissociated antiphase boundaries in Ni3Mo10.1002/pssa.2210180105 ↗