Abstract

Abstract The formation of 1:5H phase in Sm (Co, Fe, Cu, Zr)z melt-spun ribbons with high iron content has been investigated. The precipitation of the Zr-rich 2:7R phase is restrained in the boundaries of 2:17H grains for the as-spun ribbon. After aging treatment, only 2:17R phase with planar 1:3R phase occurs, which results in a lower coercivity of around 1.03kOe. After solid solution treatment of the as-spun ribbon, 2:17R phase with lower ordered state together with minor 2:17H phase is obtained. In addition, the ribbon after solid solution consists of large numbers of 2:17R nanotwins. When different twin variants with various stacking sequence encounter each other, those areas which are rich in Sm will act as the nucleation centers of 1:5H phase during aging. The pinning strength for the magnetic domain walls is enhanced, thus leading to a much higher coercivity of 6.16 kOe. These results may provide guidance for high performance 2:17R SmCo permanent magnets with high iron content.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Magnetic properties of thin films · Hydrogen Storage and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Hard magnetic materials: a perspective, magnetics10.1109/TMAG.2011.2166975 ↗
2. Magnetic materials and devices for the 21st century: stronger, lighter, and more energy efficient10.1002/adma.201002180 ↗
3. Magnetic anisotropy—How much is enough for a permanent magnet?10.1016/j.scriptamat.2015.09.021 ↗
4. Effect of ball milling process on coercivity of nanocrystalline SmCo5 magnets10.1016/j.jmmm.2017.09.012 ↗
5. Strategy for high-coercivity Nd–Fe–B magnets10.1016/j.scriptamat.2012.06.038 ↗
6. A new class of Sm-TM magnets for operating temperatures up to 550 °C10.1109/20.908807 ↗
7. Sm2(Co, Fe, Cu, Zr)17 magnets for use at temperature≥400 °C10.1063/1.367937 ↗
8. Magnetic Properties of the Intermetallic Phases Sm2(Co, Fe)1710.1063/1.2946980 ↗
9. Permanent magnet properties of Sm2(Co, Fe)1710.1109/TMAG.1975.1058832 ↗
10. Sm2(Co, Fe, Cu, Zr)17 magnets with higher Fe content10.1109/20.42433 ↗
11. Effects of solution treated temperature on the structural and magnetic properties of iron-rich Sm(CoFeCuZr)z sintered magnet10.1109/TMAG.2013.2247576 ↗
12. Effect of pre-aging treatment on the microstructure and magnetic properties of Sm(Co, Fe, Cu, Zr)7.8 sintered magnets10.2320/matertrans.MBW201325 ↗
13. Influence of intermediate-heat treatment on the structure and magnetic properties of iron-rich Sm(CoFeCuZr)z sintered magnets10.1063/1.4906757 ↗
14. The high squareness Sm-Co magnet having Hcb = 10.6 kOe at 150°C10.1063/1.4976334 ↗
15. Evolution of magnetic domain structures and coercivity in high-performance SmCo 2:17-type permanent magnets10.1016/j.actamat.2005.10.026 ↗
16. Attractive-domain-wall-pinning controlled Sm-Co magnets overcome the coercivity-remanence trade-off10.1016/j.actamat.2018.10.046 ↗
17. Microstructure and magnetic properties of Sm(CobalFexCu0. 128Zr0. 02)7.0 magnets with Fe substitution10.1016/S0304-8853(00)00508-4 ↗
18. Atomic structure and domain wall pinning in samarium-cobalt-based permanent magnets10.1038/s41467-017-00059-9 ↗
19. The evolution of phase constitution and microstructure in iron-rich 2:17-type Sm-Co magnets with high magnetic performance10.1038/s41598-018-27487-x ↗
20. Microstructures of precipitation-hardened SmCo permanent magnets10.1063/1.330867 ↗
21. Metallurgical behavior of Sm(Co, Fe, Cu, Zr)z alloys10.1063/1.333575 ↗
22. L. Rabenberg, R. Mishra, G. Thomas, Development of the cellular microstructure in the SmCo7.4-type magnets, Proc. 6th Inter workshop on REPM (1982) 599.
23. Fast development of high coercivity in melt-spun Sm (Co, Fe, Cu, Zr)z magnets10.1063/1.1450253 ↗
24. Microchemistry and magnetization reversal mechanism in melt-spun 2: 17-type Sm-Co magnets10.1063/1.1611641 ↗
25. Mechanism of phase transformation in 2:17 type SmCo magnets investigated by phase stabilization10.1016/j.scriptamat.2015.10.041 ↗
26. An electron microscope study of Sm-Co-Cu–based magnetic materials with the Sm2Co17 structure10.1063/1.323958 ↗
27. Twinning structure in Sm (Co, Fe, Cu, Zr)z permanent magnet10.1016/j.intermet.2010.02.008 ↗
28. Long-period antiphase boundary structures in the ordered alloy Au4Zn II. Growth mechanism of the LPAPB structure10.1002/pssa.2210500104 ↗
29. The coercivity mechanism of sintered Sm(CobalFe0.245Cu0.07Zr0.02)7.8 permanent magnets with different isothermal annealing time10.1016/j.physb.2015.03.009 ↗