Controlling the composition, microstructure, electrical and magnetic properties of LiFe5O8 powders synthesized by sol gel auto-combustion method using urea as a fuel
Source abstract
Abstract
Abstract Nanocrystalline lithium ferrite LiFe 5 O 8 powders were synthesized by the sol gel auto-combustion method from the corresponding metal nitrates using urea as a fuel. DTA results showed that the LiFe 5 O 8 phase started to form at temperature around 385 °C. X-ray diffraction analysis indicates that all compositions were formed in a single-phase cubic spinel structure at different annealing temperatures from 400 to 800 °C for 2 h. The lattice parameter was found to decrease whereas the particle size was increased with annealing temperature. The frequency exponent “ s ” of lithium ferrite lies in the range 0.5≤ s ≤1, which confirmed the electron hopping between Fe 2+ and Fe 3+ ions. The electron mobility in LiFe 5 O 8 samples ranged from 0.05 to 0.29 eV, which clearly indicated that the present lithium ferrites have semiconductor-like behavior. The saturation magnetization was increased on increasing the annealing temperature up to 800 °C. High saturation magnetization ( Ms =51.9 emu/g) was achieved for the ferrite powders produced at annealing temperature 800 °C for 2 h.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties and Synthesis of Ferrites · Advancements in Battery Materials · Electromagnetic wave absorption materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Mazen · Ceram. Int. · 2014 · 40 · 1122910.1016/j.ceramint.2014.03.167 ↗
2. Srivastava · J. Alloys Compd. · 2014 · 591 · 17410.1016/j.jallcom.2013.12.180 ↗
3. Mohanty · J. Mater. Sci. Technol. · 2014 · 30 · 33510.1016/j.jmst.2013.10.028 ↗
4. Teixeira · J. Non-Cryst. Solids · 2012 · 358 · 192410.1016/j.jnoncrysol.2012.06.003 ↗
5. Arjunwadkar · J. Alloys Compd. · 2014 · 611 · 27310.1016/j.jallcom.2014.05.054 ↗
6. Teixeira · Mater. Sci. Eng.: B · 2014 · 186 · 8310.1016/j.mseb.2014.03.008 ↗
7. Srivastava · Mater. Sci. Eng.: B · 2010 · 175 · 1410.1016/j.mseb.2010.06.005 ↗
8. Hessien · J. Magn. Magn. Mater. · 2008 · 320 · 280010.1016/j.jmmm.2008.06.018 ↗
9. Hankare · J. Magn. Magn. Mater. · 2010 · 322 · 262910.1016/j.jmmm.2010.03.005 ↗
10. Li · Solid State Ion. · 1999 · 120 · 25110.1016/S0167-2738(98)00556-6 ↗
11. Zeng · RSC Adv. · 2014 · 4 · 2314510.1039/c4ra02957g ↗
12. Singhal · J. Electromagn. Appl. Anal. · 2010 · 2 · 51
13. Barriga · J. Solid State Chem. · 1988 · 77 · 13210.1016/0022-4596(88)90100-4 ↗
14. Abdullah Dar · J. Alloys Compd. · 2012 · 523 · 3610.1016/j.jallcom.2012.01.083 ↗
15. Mohamed · J. Magn. Magn. Mater. · 2010 · 322 · 205810.1016/j.jmmm.2010.01.034 ↗
16. Rasly · J. Magn. Magn. Mater. · 2013 · 337–338 · 5810.1016/j.jmmm.2013.02.038 ↗
17. Rashad · Sci. Mater. Electron. · 2013 · 24 · 328410.1007/s10854-013-1244-9 ↗
18. Rashad · J. Mater. Sci. Mater. Electron. · 2012 · 23 · 88210.1007/s10854-011-0513-8 ↗
19. Bahadur · J. Chem. Sci. · 2006 · 118 · 1510.1007/BF02708761 ↗
20. Ramesh · J. Alloys Compd. · 2012 · 513 · 28910.1016/j.jallcom.2011.10.038 ↗
21. Kadam · J. Magn. Magn. Mater. · 2013 · 329 · 5910.1016/j.jmmm.2012.10.008 ↗
22. Abo El Ata · J. Magn. Magn. Mater. · 2006 · 297 · 3310.1016/j.jmmm.2005.01.085 ↗
23. George · J. Phys. D: Appl. Phys. · 2006 · 39 · 90010.1088/0022-3727/39/5/002 ↗
24. Dar · J Alloys Compd. · 2010 · 493 · 55310.1016/j.jallcom.2009.12.154 ↗
25. Cheruku · Mater. Chem. Phys. · 2014 · 146 · 38910.1016/j.matchemphys.2014.03.043 ↗
26. Singhal · J. Sol–Gel Sci. Technol. · 2013 · 66 · 15510.1007/s10971-013-2980-2 ↗