Effects of sintering temperature on properties of toroid cores using NiZnCu ferrites for power applications at >1 MHz
Source abstract
Abstract
Abstract The microstructures, magnetic and electronic performance of NiZnCu ferrites have been investigated at temperature from 850 °C to 1000 °C. X-ray diffraction (XRD) patterns showed that only single phase with spinel structure existed. Scanning electron microscopy (SEM) results showed that grain size increased with enhancement of sintering temperature and the most homogeneous, compact microstructure was obtained at 950 °C. Magnetic properties measurements revealed that both complex permeability and saturation magnetization increased with increasing of sintering temperature. The initial permeability was approximately linear within the scope of 850–1000 °C as well as the resonance frequency decreased from 70 MHz to 30 MHz. Power loss density tests demonstrated that the core sintered at 950 °C instead of the one sintered at 1000 °C had the lower power loss density at both 5 mT and 10 mT and the higher inductance under a certain exciting direct current at 1 MHz. Also the inductance of the sample sintered at the higher temperature dropped faster than that at the lower temperature. The results showed that the core sintered at 950 °C had better electrical performance and was suitable for wide usage.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties and Synthesis of Ferrites · Advancements in Battery Materials · Electromagnetic wave absorption materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Bai · 2011 · 249
2. Multipermeability inductors for increasing the inductance and improving the efficiency of high-frequency dc/dc converters10.1109/TPEL.2012.2228504 ↗
3. L. Wang, Y. Pei, X. Yang, Z. Wang, Y. Liu, A horizontal-winding multi-permeability distributed air-gap inductor, in Twenty-Seventh Annual IEEE Applied Power Electronics Conference and Exposition (APEC) 2012, 2012, PP. 994–1001.10.1109/APEC.2012.6165940 ↗
4. Soft magnetic alloy–polymer composite for high-frequency power electronics application10.1007/s11664-013-2866-7 ↗
5. Effect of average grain size and sintered relative density on the imaginary part-µ″ of the complex magnetic permeability of (Cu0.12Ni0.23Zn0.65)Fe2O4 system10.1016/j.ceramint.2015.11.101 ↗
6. Influence of microstructure on permeability dispersion and power loss of NiZn ferrite10.1063/1.2908202 ↗
7. Nickel–zinc ferrite fabricated by sol–gel route and application in high-temperature superconducting magnetic energy storage for voltage sag solving10.1016/j.matdes.2009.11.004 ↗
8. Submicrometer laminated Fe/SiO2 soft magnetic composites—an effective route to materials for high-frequency applications10.1002/adma.200401096 ↗
9. Effects of porosity and grain size on the magnetic properties of NiZn ferrite10.1111/j.1151-2916.1977.tb16092.x ↗
10. Synthesis and characterization of manganese ferrite nanoparticles obtained by electrochemical/chemical method10.1016/j.matdes.2016.09.031 ↗
11. Effect of sintering temperature on electromagnetic properties of NiCuZn ferrite10.1016/j.ceramint.2012.09.087 ↗
12. Characterization of low temperature sintered ferrite laminates for high frequency point-of-load (POL) converters10.1109/TMAG.2013.2273755 ↗
13. Influence of B2O3–MoO3 addition on microstructure and magnetic properties of low-temperature-fired NiCuZn ferrites10.1016/j.ceramint.2014.03.102 ↗
14. Influence of MoO3 and V2O5 co-doping on the magnetic properties and microstructure of a Ni–Zn ferrite10.1016/j.jallcom.2007.06.120 ↗
15. Effect of B2O3 on the densification and magnetic properties of Li–Zn ferrite10.1016/j.matdes.2011.04.019 ↗
16. Analysis of the complex permeability of NiCuZn ferrites up to 1 GHz with regard to Cu content and sintering temperature10.1016/j.ceramint.2013.06.010 ↗
17. Enhancement of initial permeability and reduction of loss factor in Zn substituted nanocrystalline Li0.35−0.5xNi0.3ZnxFe2.35−0.5xO410.1016/j.jmmm.2016.10.030 ↗
18. Frequency dispersion and temperature variation of complex permeability of Ni-Zn ferrite composite materials10.1063/1.359919 ↗
19. Contribution of magnetization mechanisms in nickel–zinc ferrites with different grain sizes and its temperature relationship10.1016/j.matchemphys.2016.03.002 ↗
20. Complex permeability of Fe-deficient Ni–Cu–Zn ferrites10.1016/j.jallcom.2012.09.037 ↗
21. The reluctance of some irregular magnetic fields10.1109/T-AIEE.1915.4765246 ↗
22. Rahaman · 2003
23. Properties of soft magnetic composite with evaporated MgO insulation coating for low iron loss10.4028/www.scientific.net/MSF.534-536.1361 ↗
24. DC bias effect on the magnetic properties in NiZn ferrite10.2497/jjspm.61.S245 ↗