Influence of hot rolling reduction rate on the microstructure, texture and magnetic properties of a strip-cast Fe-6.5 wt% Si grain-oriented electrical steel
Source abstract
Abstract
Abstract Grain-oriented electrical steel containing 6.5 wt% Si is a promising soft magnetic material with very low iron losses for high-frequency applications. However, due to the ordered phases formed in the microstructure, the room-temperature ductility (formability) of this material is extremely low. It is essentially not possible to process this steel by conventional cold rolling. In this study, an Fe-6.5 wt% Si grain-oriented electrical steel was processed through strip casting (also known as twin-roll casting), hot rolling, warm rolling, cold rolling, primary and secondary annealing. The effect of hot rolling reduction rate (12–40%) on the microstructure, crystallographic texture and magnetic properties of the final steel sheets was investigated. The results showed that hot rolling increased the area fraction of the Goss ({1 1 0}〈0 0 1〉) grains, reduced the grain size, and promoted the precipitation of fine second-phase particles. After warm rolling, cold rolling and primary annealing, the recrystallized microstructure was the finest if the hot-rolling reduction rate was the highest (40%). After secondary annealing, the steel with the largest hot rolling reduction rate (40%) showed the most apparent abnormal grain growth, leading to the formation of the Goss texture. As a result, the magnetic flux density and the magnetic Barkhausen noise (MBN) also showed the largest values among all the samples. On the other hand, those with lower hot-rolling reduction rates (12–32%) showed no or less abnormal grain growth during secondary recrystallization, which resulted in lower magnetic flux density and weaker magnetic Barkhausen noise. Increasing the amount of hot rolling reduction was thus able to promote abnormal grain growth during secondary recrystallization, and optimize the magnetic properties of the steel.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties and Applications · Microstructure and Mechanical Properties of Steels · Magnetic properties of thin films
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Ferromagnetism
2. Metallurgy of high-silicon steel parts produced using Selective Laser Melting10.1016/j.actamat.2016.03.037 ↗
3. Commercial scale production of Fe-6.5 wt.% Si sheet and its magnetic properties10.1063/1.342373 ↗
4. Ordering–disordering phenomena and micro-hardness characteristics of B2 phase in Fe–(5–6.5%) Si alloys10.1016/j.msea.2005.07.012 ↗
5. Magnetic properties of 6.5% Si-Fe sheet and its applications10.1016/0304-8853(90)90553-3 ↗
6. Magnetic properties evaluation of spray formed and rolled Fe–6.5 wt.% Si–1.0 wt.% Al alloy10.1016/j.msea.2006.02.318 ↗
7. Effect of silicon content on secondary recrystallization in grain-oriented electrical steel produced by single-stage cold rolling process10.2355/isijinternational.31.1007 ↗
8. Evolution of microstructure and texture in grain-oriented 6.5% Si steel processed by strip-casting10.1016/j.matchar.2017.02.022 ↗
9. Secondary recrystallization behaviors of grain-oriented 6.5 wt% silicon steel sheets produced by rolling and nitriding processes10.1007/s40195-016-0390-5 ↗
10. Effect of cooling rate on bending behavior of 6.5 wt.% Si electrical steel thin sheets fabricated by strip casting and rolling10.1016/j.matchar.2015.11.008 ↗
11. Characterization of microstructure, texture and magnetic properties in twin-roll casting high silicon non-oriented electrical steel10.1016/j.matchar.2013.11.014 ↗
12. Microstructure, texture evolution and magnetic properties of strip-casting non-oriented 6.5 wt.% Si electrical steel doped with cerium10.1016/j.matchar.2015.03.024 ↗
13. Development of λ-fiber recrystallization texture and magnetic property in Fe–6.5 wt% Si thin sheet produced by strip casting and warm rolling method10.1016/j.matlet.2012.09.046 ↗
14. Characterization of microstructure and texture in grain-oriented high silicon steel by strip casting10.1007/s40195-015-0338-1 ↗
15. Effect of hot rolling reduction on microstructure, texture and ductility of strip-cast grain-oriented silicon steel with different solidification structures10.1016/j.msea.2014.03.052 ↗
16. Effect of hot rolling on texture precipitation, and magnetic properties of strip-cast grain-oriented silicon steel10.1002/srin.201600009 ↗
17. Oxford Instruments, HKL Channel 5 EBSD System Manual, 2007, pp. 1–475.
18. Magnetic properties of (110)[001] grain oriented 6.5% silicon steel10.1063/1.349985 ↗
19. Takamiya · 2016
20. Recent development in grain-oriented electrical steel with low magnetostriction10.1007/s11665-997-0071-7 ↗
21. Posco Product Manual, Electrical Steel, 2011, pp. 1-34, http://www.posco.com/homepage/docs/eng5/dn/company/product/e_electrical_pdf_2011.pdf.10.1016/S1464-2859(11)70173-0 ↗
22. Evaluation of local anisotropy of magnetic response from non-oriented electrical steel by magnetic Barkhausen noise
23. Characterization of the magnetic easy axis in pipeline steel using magnetic Barkhausen noise10.1063/1.356561 ↗
24. Through-process characterization of local anisotropy of Non-oriented electrical steel using magnetic Barkhausen noise10.1016/j.jmmm.2018.01.023 ↗
25. Characterization of pure iron and (130 ppm) carbon–iron binary alloy by Barkhausen noise measurements: study of the influence of stress and microstructure10.1016/S1359-6454(98)00205-5 ↗
26. Correlation between AC core loss and surface magnetic barkhausen noise in electric motor steel10.1007/s10921-014-0260-x ↗
27. Correlation of magnetic Barkhausen noise with core loss in oriented 3% Si–Fe steel laminates10.1063/1.361258 ↗
28. Anisotropy study of grain oriented steels with magnetic Barkhausen Noise
29. Stresstech Group, Rollscan 350 Operating Instructions, V1.0b, 2013, pp. 1–39.
30. Stresstech Group, MicroScan 600 Operating Instructions, V.5.4b, 2015, pp. 1–37.
31. Deveci M, Stresstech Bulletin 2: The Properties of Barkhausen Noise, https://www.stresstech.com/download_file/view_inline/381/.
32. Texture control in the production of grain oriented silicon steels10.2355/isijinternational.29.809 ↗
33. Contribution of shear banding to origin of Goss texture in silicon iron10.1179/030634584790420258 ↗
34. Through process texture evolution and magnetic properties of high Si non-oriented electrical steels10.1016/j.matchar.2012.06.006 ↗
35. Texture control during the manufacturing of nonoriented electrical steels10.1155/2008/173083 ↗
36. Relative effect(s) of texture and grain size on magnetic properties in a low silicon non-grain oriented electrical steel10.1016/S0304-8853(03)00142-2 ↗
37. Strain-softening behavior of an Fe–6.5 wt%Si alloy during warm deformation and its applications10.1016/j.msea.2010.10.093 ↗
38. Barkhausen noise measurements give direct observation of magnetocrystalline anisotropy energy in ferromagnetic polycrystals10.1088/0022-3727/46/39/392001 ↗
39. Morphology and precipitation kinetics of MnS in low-carbon steel during thin slab continuous casting process10.1016/S1006-706X(06)60091-5 ↗
40. The impact of niobium on the microstructure, texture and magnetic properties of strip-cast grain oriented silicon steel10.1016/j.jmmm.2017.06.058 ↗
41. Precipitates in electrical steels10.1016/j.jmmm.2008.03.062 ↗
42. Fabrication of grain-oriented silicon steel by a novel way: Strip casting process10.1016/j.matlet.2014.09.075 ↗
43. A new model of Goss texture development during secondary recrystallization of electrical steel10.1016/S1359-6454(97)00111-0 ↗
44. Investigation of the stress-dependent magnetic easy axis in steel using magnetic Barkhausen noise10.1063/1.361878 ↗
45. Plastic versus elastic deformation effects on magnetic Barkhausen noise in steel10.1016/S1359-6454(00)00134-8 ↗