journal article·2024-01

High magnetic performance ultra-thin Fe-6.5Si ribbons fabricated by planner flow casting and annealing

Ruxia Liu, Peiyun Qi, Feilong Sun, Jiawei Zhang, Guilin Wu, Shuize Wang, Zuoxin Zhu, Minghui Wang, Xinping Mao

Publisher page

Abstract

Fe-6.5 wt.%Si steel is one of the most attractive soft magnetic materials for making iron cores with low noise and low power loss. The planner flow casting method was regarded as a promising method to obtain ultra-thin ribbons of Fe-6.5Si alloy. In this study, Fe-6.5Si ribbons with a thickness of 0.03 mm were prepared by planner flow casting. Samples were heat-treated at various temperatures. It is revealed that the grain size on the wheel surface and free surface gradually increases with increasing annealing temperature. The initial {1 0 0} fiber texture of the wheel and free surfaces is weakened after annealing, transforming to {0 0 1} 〈5 1 0〉 on the wheel surface and to {2 2 9} < 11 2 2 > on the free surface after annealing at 1150 °C for 1 h. The texture parameter and dislocation density are the key factors affecting the magnetic induction intensity, showing an inverse correlation with the texture parameter and dislocation density. Furthermore, the iron loss is mainly influenced by the grain size, with an optimal grain size of 10 μm. Considering the magnetic induction intensity and iron loss, the optimal annealing temperature is determined to be 1100 °C, resulting in a magnetic induction intensity of B 8 = 1.26 T and B 50 = 1.65 T, and iron loss values of P 1/400 = 14.1 W/Kg and P 0.2/5000 = 11.1 W/Kg.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties and Applications · Metallic Glasses and Amorphous Alloys · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Effects of solidification cooling rates on microstructures and physical properties of Fe-6.5% Si alloys10.1016/j.actamat.2020.116575 ↗
2. Ductile-to-brittle transition behavior of Fe-6.5 wt% Si alloy with three-point bending testing10.1016/j.matchar.2023.112861 ↗
3. Improved ductility of Fe-6.5 wt% Si alloy under electropulsing tension10.1016/j.msea.2022.143639 ↗
4. Effect of annealing temperature on magnetic properties of cold rolled high silicon steel thin sheet10.1016/j.jallcom.2009.10.118 ↗
5. Ordering suppression and excellent ductility in soft-magnetic Fe-6.5 wt% Si sheet by Hf addition10.1016/j.jallcom.2018.06.343 ↗
6. Commercial scale production of Fe-6.5wt.%Si sheet and its magnetic properties10.1063/1.342373 ↗
7. Magnetic properties and workability of 6.5% Si steel sheet10.1016/0304-8853(96)00128-X ↗
8. Fabrication and magnetic properties of Fe-6.5% Si alloys by magnetron sputtering method10.1016/j.jallcom.2010.02.175 ↗
9. Production of high silicon steel for electrical applications by thermomechanical processing10.1016/S0924-0136(03)00247-4 ↗
10. Microstructure and properties of cost-effective Fe-6.5 wt% Si ribbons fabricated by melt-spinning10.1016/j.scriptamat.2019.01.002 ↗
11. Effect of wheel speed on magnetic and mechanical properties of melt spun Fe-6.5 wt.% Si high silicon steel10.1063/1.5006481 ↗
12. Thermodynamic and kinetic analysis of the melt spinning process of Fe-6.5 wt.% Si alloy10.1016/j.jallcom.2018.08.293 ↗
13. Magnetic properties of 6.5 percent silicon-iron ribbon formed by a melt spinning technique10.1109/TMAG.1982.1061959 ↗
14. W. Ciur yńska, J. Zbros czyk, J. Olszewski, J. Frackowiak, K. Narita. Order-disorder effect on magnetic properties of rapidly quenched Fe-6.5%Si alloy. Journal of Magnetism and Magnetic Materials, 1994, 133, 351-353.10.1016/0304-8853(94)90565-7 ↗
15. Fabrication of Fe-6.5 wt% Si ribbons by melt spinning method on large scale10.1155/2015/296197 ↗
16. Magnetic properties and core loss behavior of Fe-6.5 wt.% Si ribbons prepared by melt spinning
17. Influence of ejection temperature on structure and glass transition behavior for Zr-based rapidly quenched disordered alloys10.1016/j.actamat.2016.06.049 ↗
18. Characterization of microstructure, texture and magnetic properties in twin-roll casting high silicon non-oriented electrical steel10.1016/j.matchar.2013.11.014 ↗
19. Effects of warm temper rolling on microstructure, texture and magnetic properties of strip-casting 6.5 wt% Si electrical steel10.1016/j.jmmm.2014.06.053 ↗
20. Correlation between microstructure, texture, and magnetic induction in nonoriented electrical steels10.1109/TMAG.2009.2032425 ↗