The effect of grain size on the internal oxidation of Sm2Co17-type permanent magnets
Source abstract
Abstract
This work has examined the influence of grain size in sintered Sm2(Co,Fe,Cu,Zr)17-type permanent magnets on the growth of an internal oxidation zone (IOZ). Two magnets of similar composition but with average grain sizes of 46 μm and 170 μm respectively, were exposed to temperatures of 500 °C in air for times up to 1000 h. Overall, the smaller grained magnet showed a reduced growth rate of the IOZ (∼39.01 μm2h−1) compared to the larger grained magnet (∼48.95 μm2h−1) and a smaller irredeemable loss in Br (3.11%) after 1000 h. However, growth rate of the IOZ is shown to depend on the growth direction, in respect to the crystallographic c-axis of the matrix phase. The smaller grain size was shown to be most effective at retarding the growth of IOZ under surfaces parallel to the c-axis. It is proposed therefore, that a smaller grained sintered magnet may be the microstructure of choice for use in demanding, high temperature applications, where a protective coating is not always a possibility, such as a high-performance electrical machine with a surface mount PM rotor. Orientation of the exposed face must also be considered to minimise the resultant magnetic induction loss caused by oxidation.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Magnetic Properties of Alloys · Magnetic and transport properties of perovskites and related materials · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Corrosion of NdFeB permanent magnets in humid environments at temperatures up to 150°C10.1016/0304-8853(95)90037-3 ↗
2. Developments in the processing and properties of NdFeb-type permanent magnets10.1016/S0304-8853(02)00334-7 ↗
3. Sm2(Co, Fe, Cu, Zr)17 magnets for use at temperature >400 °C10.1063/1.367937 ↗
4. New rare-earth permanent magnets with an intrinsic coercivity of 10 kOe at 500 ° C10.1063/1.369832 ↗
5. Evolution and effects of surface degradation layer of Sm 2 Co 17 magnets at high temperatures10.1063/1.4862857 ↗
6. High temperature oxidation and its induced coercivity loss of a 2: 17 type SmCo-based magnet
7. Correlation of microchemistry of cell boundary phase and interface structure to the coercivity of Sm(Co0.784Fe0.100Cu0.088Zr0.028)7.19 sintered magnets10.1016/j.actamat.2016.12.050 ↗
8. The microstructure of sintered Sm(Co0.72Fe0.20Cu0.055Zr0.025)7.5 permanent magnet studied by atom probe10.1016/j.actamat.2003.10.015 ↗
9. Micromagnetism and the microstructure of high-temperature permanent magnets10.1063/1.1809250 ↗
10. High temperature 2:17 magnets: relationship of magnetic properties to microstructure and processing10.1109/20.908808 ↗
11. Effect of Zr on the microstructure and magnetic properties of Sm(Co bal, Fe 0.1, Cu 0.088, Zr x)8.5 magnets10.1063/1.371874 ↗
12. The oxidation morphology of SmCo alloys10.1016/j.jallcom.2009.07.115 ↗
13. The mechanism of high temperature oxidation of a SmCo-based magnetic alloy10.1016/j.corsci.2012.04.028 ↗
14. The oxidation of SmCo magnets10.1063/1.2830559 ↗
15. Surface reaction and Sm depletion at 550 °C for high temperature Sm-Tm magnets10.1109/20.951225 ↗
16. Thermal stability of surface modified Sm2Co17-type high temperature magnets10.1016/j.jmmm.2012.11.013 ↗
17. Oxidation protection of Sm 2 Co 17 -based alloys10.1016/j.jallcom.2011.12.031 ↗
18. The effect of a surface Cr film on the oxidation of SmCo-based magnetic alloy at 700 ° C10.1016/j.corsci.2013.07.033 ↗
19. The oxidation kinetics of SmCo alloys10.1016/j.jallcom.2008.05.083 ↗
20. Microstructure and high temperature magnetic properties of Sm(Co, Cu, Fe, Zr)[sub z] (z=6.7–9.1) permanent magnets10.1063/1.369597 ↗
21. Thermal stability of Sm-Tm high temperature magnets at 300–550°C10.1109/20.908773 ↗
22. Atomic scale understanding of the defects process in concurrent recrystallization and precipitation of Sm-Co-Fe-Cu-Zr alloys10.1016/j.actamat.2020.10.067 ↗
23. Decomposition behavior in the early-stage oxidation of Sm2Co17-type magnets10.1016/j.scriptamat.2021.113911 ↗
24. Model for calculating J(H) curves of Ni coated Nd-Fe-B magnets10.1016/S1006-706X(08)60164-8 ↗