Texture and properties of a new Fe-Si-P solid solution strengthening high strength electrical steels
Source abstract
Abstract
In this study solid solution strengthening mechanism was introduced to increase the mechanical and magnetic properties of non-oriented silicon steel. Compared with the P-free steel, the annealed texture of 0.1P-containing steel whose γ orientation was almost completely eliminated consisted of strong η-fiber, near-Cube, and near-Goss orientation grains. The texture factor was increased from 1.25 to 4.27. Therefore, the magnetic properties of 0.1P steel was significantly improved and B 50 and P 10/400 were optimized to 1.712 T and 22.92 W/kg, respectively. When the frequency was 400 Hz, in the 0.1P steel core loss decrease was mainly because of hysteresis loss, which decreased by 38.6 %, and eddy current loss also decreased by 2.3 %. The addition of P resulted in a decrease in coercivity. Furthermore, the 0.1P steel had superior magnetic properties compared to P-free steel with yield strength and tensile strength of 581 MPa (increase of 8.1 %) and 692 MPa (increase of 7.8 %). Thus, it is underscored that the addition of 0.1 wt% P to 4.5 wt% Si steel can simultaneously improve both magnetic properties and mechanical properties.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties and Applications · Microstructure and Mechanical Properties of Steels · Electromagnetic Effects on Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Nonoriented electrical steels10.1007/s11837-012-0356-7 ↗
2. Progress on the research of high-strength non-oriented silicon steel sheets in traction motors of hybrid/electrical vehicles
3. Magnetic and mechanical properties of high strength non-oriented electrical steel
4. Magnetic and mechanical properties of newly developed high-strength nonoriented electrical steel10.1109/TMAG.2009.2033457 ↗
5. Sumitomo Metal Industries Ltd. Non-oriented electrical steel sheet and production process thereof. United States Patent: US 7,922,834 B2, 2011-04-12.
6. Production of high silicon steel for electrical applications by thermomechanical processing10.1016/j.jmatprotec.2003.10.002 ↗
7. Ordering-disordering phenomena and micro-hardness characteristics of B2 phase in Fe-(5–6.5%) Si alloys10.1016/j.msea.2005.07.012 ↗
8. Effect of coiling operation on strip quality of 4.5% Si steel in twin roll casting process10.2355/isijinternational.39.463 ↗
9. The effects of superheating on texture and microstructure of Fe-4.5 wt% Si steel strip by twin-roll strip casting10.2355/isijinternational.41.70 ↗
10. Investigation of Microstructure and Properties of Strip-Cast 4.5 wt% Si Non-oriented Electrical Steel by Different Rolling Processes
11. High-strength low-iron-loss silicon steels fabricated by cold rolling10.1016/j.jmmm.2018.10.143 ↗
12. Y. Hamada, I. Kono, M. Izawa, Manufacture method of non-oriented silicon steel sheets: Japan Patent, P2009-18535.
13. I. Tanaka, M. Fujisawa, K. Hitoshi, Manufacture method of non-oriented electrical steel sheets used in rotors: Japan Patent, P2007-16278.
14. Grain boundary segregation in electrical steels
15. M. Fujita, M. Kono, H. Ozaki, Manufacture method of non-oriented electrical steel sheets with excellent magnetic property: Japan Patent, 10-183244.
16. The effect of phosphorus on the core loss of lamination steels10.1016/0304-8853(92)91023-M ↗
17. Magnetic properties and recrystallization texture evolutions of phosphorus-bearing non-oriented electrical steel sheets10.2355/isijinternational.47.1666 ↗
18. Zhang · 2019
19. Influence of hot deformation on texture and magnetic properties of strip cast non-oriented electrical steel10.1016/j.jmmm.2018.05.015 ↗
20. 001}<120>-{113}<361>recrystallization textures induced by initial {001 grains and related microstructure evolution in heavily rolled electrical steel10.1016/j.matchar.2016.08.009 ↗
21. Through process texture evolution and magnetic properties of high Si non-oriented electrical steels10.1016/j.matchar.2012.06.006 ↗
22. Analysis of {411}<148>recrystallisation texture in twin-roll strip casting of 4.5 wt% Si nonoriented electrical steel10.1016/j.matlet.2016.04.091 ↗
23. Effects of warm temper rolling on microstructure, texture and magnetic properties of strip-casting 6.5 wt% Si electrical steel10.1016/j.jmmm.2014.06.053 ↗
24. Products and catalogs of Nippon Steel & Sumitomo Metals.
25. Mclean · 1957
26. Equilibrium segregation in a ternary solution: a model for temper embrittlement10.1016/0039-6028(75)90125-9 ↗
27. On Kinetics of Phosphorus Segregation in Cr-Mo-V Low Alloy Steel10.1016/0956-716X(94)90462-6 ↗
28. Phosphorus grain boundary segregation in polycrystalline low alloy steels
29. Effects of alloying elements, impurities, and carbon on temper embrittlement of steels10.1179/030634584790419683 ↗
30. Intergranular Segregation of Sulfur in the Fe-Ni36 Alloys10.1016/0956-716X(90)90240-H ↗
31. Peculiarities of intergranular internal adsorption of carbon and phosphorus in iron alloys
32. Determination of impurity-point defect binding energies in alloys10.1179/mst.1996.12.11.904 ↗
33. The influence of shear bands on final structure and magnetic properties of 3% Si non-oriented silicon steel10.1016/j.jmmm.2008.04.050 ↗
34. Park · 2002
35. Evolution of recrystallization texture in non-oriented electrical steels10.1016/S1359-6454(03)00115-0 ↗
36. Effect of initial grain size prior to cold rolling on annealing texture in non-oriented electrical steel10.4028/www.scientific.net/MSF.408-412.1257 ↗
37. The evolution of the Goss and Cube textures in electrical steel10.1016/j.matlet.2014.01.166 ↗
38. Humphreys · 2004 · 159
39. Recent development of non-oriented electrical steel in JFE steel
40. Research progress of high strength non-oriented electrical steels, mater
41. Influence of annealing process on microstructures, mechanical and magnetic properties of Nb-containing highstrength non-oriented silicon steel
42. Effect of copper precipitates on mechanical and magnetic properties of Cu-bearing non-oriented electrical steel processed by twin-roll strip casting10.1016/j.msea.2017.07.075 ↗
43. Effects of Cu precipitates on magnetic properties of nonoriented electrical steel10.1109/TMAG.2014.2365442 ↗