Growth of defects around grain boundary and evolution of cellular structure during isothermal aging process in 2:17-type SmCo permanent magnets
Source abstract
Abstract
The cellular structure consisted of cell boundary phase (1:5H phase) and cell phase (2:17R phase) is crucial for 2:17-type SmCo magnets to obtain high performance. In this study, the growth of defects around grain boundary and the evolution of cellular structure during isothermal aging process are systematically investigated. Further analysis determines the effects of these microstructural changes on magnetic properties. With the isothermal aging time increasing from 0.5 to 12 h, the width of 1:5H phase-free zones (PFZs) around the grain boundary expands from approximately 100 to 200 nm. Simultaneously, the cellular structure inside the grain becomes more complete, and the Cu content in the 1:5H phase is increased. However, as the isothermal aging time further extends to 36 h, accompanied by the formation of substantial amounts of Cu-rich phases along the grain boundaries, the width of PFZs around the grain boundary increases to approximately 300 nm. Moreover, the width of the 1:5H phase widens, and it even disappears, leading to incomplete cellular structure and a low Cu content in the 1:5H phase. The broad PFZs and incomplete cellular structure negatively impacts the coercivity and squareness of the magnet. Finally, an optimal performance of B r = 10.8 kG, H cj = 29.7 kOe, ( BH) max = 26.7 MGOe, and SF = 49.9 % is obtained for the magnet aged 12 h. These findings indicate that the defects around the grain boundary can be effectively controlled and form complete cellular structure by adjusting the isothermal aging time, which may provide an important clue for developing high-performance and low-cost 2:17-type SmCo magnets.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties of Alloys · Magnetic and transport properties of perovskites and related materials · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. A Family of New Cobalt-Base Permanent Magnet Materials10.1063/1.1709459 ↗
2. C.H. Chen, M.S. Walmer, M.H. Walmer, A new class of Sm-TM magnets for operating temperatures up to 550°C, IEEE Trans. Magn. 36 (2000) 3376-3381, https://doi.org/ 10.1109/20.908807.10.1109/20.908807 ↗
3. Atomic structure and domain wall pinning in samarium-cobalt-based permanent magnets10.1038/s41467-017-00059-9 ↗
4. Attractive-domain-wall-pinning controlled Sm-Co magnets overcome the coercivity-remanence trade-off10.1016/j.actamat.2018.10.046 ↗
5. SmCo (2:17-type) magnets with high contents of Fe and light rare earths10.1063/1.355424 ↗
6. Magnetic materials and devices for the 21st century: stronger, lighter, and more energy efficient10.1002/adma.201002180 ↗
7. The microstructure of sintered Sm(Co0.72Fe0.20Cu0.055Zr0.025)7.5 permanent magnet studied by atom probe10.1016/j.actamat.2003.10.015 ↗
8. Direct evidence for Cu concentration variation and its correlation to coercivity in Sm(Co0.74Fe0.1Cu0.12Zr0.04)7.4 ribbons10.1016/j.scriptamat.2009.01.006 ↗
9. Optimization of microstructures and magnetic properties of Sm(CobalFe0.227Cu0.07Zr0.023)7.6 magnets by sintering treatment10.1016/j.jre.2018.04.014 ↗
10. Optimization of both coercivity and knee-point magnetic field of Sm2Co17-type magnets via solid solution process10.1016/j.jre.2019.11.009 ↗
11. Influence of intermediate-heat treatment on the structure and magnetic properties of iron-rich Sm(CoFeCuZr)Z sintered magnets10.1063/1.4906757 ↗
12. Identifications of SmCo5 and Smn+1Co5n-1-type phases in 2:17-type Sm-Co-Fe-Cu-Zr permanent magnets10.1016/j.scriptamat.2020.02.028 ↗
13. Effect of grain boundary on magnetization behaviors in 2:17 type SmCo magnet10.1016/j.jmmm.2019.165459 ↗
14. Study on the grain growth and the evolution of defects around grain boundaries during heat treatment process in Sm2Co17 permanent magnets10.1016/j.jallcom.2023.172444 ↗
15. Combination strategy for high-performance Sm(CoFeCuZr)z sintered permanent magnet: Synergistic improvement of the preparation process10.1016/j.actamat.2023.118901 ↗
16. Crystalline and magnetic microstructures of iron-rich Sm(Co0.65Fe0.26Cu0.07Zr0.02)7.8 sintered magnets: isothermal aging effect10.1016/j.jmmm.2018.06.047 ↗
17. Nanostructure short-range ordering induced cellular structure and microchemistry evolution in Sm2Co17-type magnets10.1016/j.actamat.2020.09.057 ↗
18. Atomic scale understanding of the defects process in concurrent recrystallization and precipitation of Sm-Co-Fe-Cu-Zr alloys10.1016/j.actamat.2020.10.067 ↗
19. Revisiting the pinning sites in 2:17-type Sm-Co-Fe-Cu-Zr permanent magnets10.1016/j.jre.2021.03.013 ↗
20. Magnetization reversal process in (SmGdDy)(Co, Fe, Cu, Zr)z magnets with different cellular structures
21. Exploring microstructural origin of squareness-coercivity trade-off in iron-rich Sm-Co-Fe-Cu-Zr magnets10.1016/j.scriptamat.2021.114418 ↗
22. Grain boundary optimization induced substantial squareness enhancement and high performance in iron-rich Sm-Co-Fe-Cu-Zr magnets10.1016/j.jmst.2020.12.067 ↗