Annealing temperature effects on microstructure and magnetic properties of Fe-6.5wt. %Si alloy strips prepared by TSTRC process
Source abstract
Abstract
The Fe-6.5wt.%Si alloy exhibits remarkable soft magnetic characteristics, such as high magnetic permeability, low coercivity, high resistivity, and nearly zero magnetostriction. These attributes establish it as an ideal material for low-power, low-noise electric motors and transformers. This investigation aimed to assess the impact of annealing temperature (ranging from 800 to 1200 °C for 1 h) on the microstructure, texture, and magnetic properties of a 0.15 mm thick Fe-6.5wt.%Si alloy sheet, which was obtained by subjecting the strips produced through the top side-pouring twin-roll casting (TSTRC) process to multi-pass warm rolling in the temperature range of 600 ∼ 800 °C, avoiding hot rolling. Additionally, the recrystallization mechanism of the annealed sheet at 1100 °C for 1 h was explored. The findings indicate that enhancing the annealing temperature corresponded to a reduction in magnetic induction (B 8 and B 50) as well as iron losses (P 10/50, P 10/400, and P 2/1000). The annealed sheet at 1200 °C for 1 h demonstrated the most favorable magnetic properties, displaying iron losses of 0.486 W/kg, 6.895 W/kg, and 1.232 W/kg for P 10/50, P 10/400, and P 2/1000, respectively. These results illustrate excellent overall magnetic characteristics. The coercivity (Hc) of both B 8 and B 50 decreased as the annealing temperature increased in the hysteresis loop measurements. Specifically, for B 8, it decreased from 62.84 A/m to 24.50 A/m, and for B 50, it decreased from 78.10 A/m to 35.50 A/m. The average grain size of the samples gradually increased as the annealing temperature ranged from 800 to 1200 °C. The dominant texture observed was {1 1 1}, and the volume fraction of {1 1 1} texture increased while the volume fractions of {1 0 0} and {1 1 0} textures decreased. Upon annealing at 1100 °C for 8 s, the elongated and flattened deformed structures were mainly replaced by equiaxed grains, indicating the completion of the recrystallization process. However, there was a noticeable distinction in the coarsening degree of equiaxed grains based on their orientations. The presence of λ-oriented grains was less prominent, while α-oriented and γ-oriented grains were relatively more abundant. As the annealing time increased from 8 s to 1 h, there was a decrease in the presence of λ-oriented and α-oriented grains, while the presence of γ-oriented grains significantly increased.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties and Applications · Microstructure and Mechanical Properties of Steels · Metallic Glasses and Amorphous Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Recent developments of new soft magnetic materials10.1016/0304-8853(94)90534-7 ↗
2. Ordering-disordering phenomena and micro-hardness characteristics of B2 phase in Fe-(5–6.5%)Si alloys10.1016/j.msea.2005.07.012 ↗
3. Newly developed electrical steel for high-frequency use10.1016/S0304-8853(01)01164-7 ↗
4. Effect of annealing temperature on magnetic properties of cold rolled high silicon steel thin sheet10.1016/j.jallcom.2009.10.118 ↗
5. Strong <001> recrystallization texture component in 6.5wt% Si electrical steel thin sheets by secondary cold rolling and annealing10.1016/j.jmmm.2016.06.078 ↗
6. Improved plasticity and cold-rolling workability of Fe–6.5wt%Si alloy by warm-rolling with gradually decreasing temperature10.1016/j.jmst.2016.01.017 ↗
7. Deformation twinning feature and its effects on significant enhancement of tensile ductility in columnar-grained Fe-6.5wt.%Si alloy at intermediate temperatures10.1016/j.intermet.2011.12.011 ↗
8. Deformation twinning in an Fe-6.5wt.% Si alloy with columnar grains during intermediate temperature compression10.1016/j.msea.2012.01.050 ↗
9. Effects of boron on microstructure and mechanical properties of Fe-6.5 wt.%Si alloy fabricated by directional solidification10.1016/j.intermet.2012.12.005 ↗
10. Microstructure, texture evolution and magnetic properties of strip-casting non-oriented 6.5 wt.% Si electrical steel doped with cerium10.1016/j.matchar.2015.03.024 ↗
11. Effect of annealing on microstructure, texture and magnetic properties of Fe-6.5wt%Si-0.03wt%Nb alloy10.1016/j.jmmm.2020.166699 ↗
12. Magnetic properties and workability of 6.5% Si steel sheet10.1016/0304-8853(96)00128-X ↗
13. Basic Investigation of CVD method for manufacturing 6.5% Si steel sheet10.2355/isijinternational.36.706 ↗
14. Magnetic properties and workability of 6.5% silicon steel sheet manufactured in continuous CVD siliconizing line10.1016/0304-8853(94)90521-5 ↗
15. Rapidly quenched ribbon-form silicon-iron alloy with high silicon concentration10.1016/0304-8853(80)90352-2 ↗
16. Ordering influence on magnetic properties of rapidly quenched Fe-6.5wt%
17. Rapidly quenched ribbon-form silicon and silicon-iron10.1143/JJAP.18.207 ↗
18. Improvement of magnetic properties of an Fe–6.5wt.% Si alloy by directional solidification10.1016/j.matlet.2011.02.020 ↗
19. A study on magnetic properties of high Si steel obtained through powder rolling processing10.1016/j.jmmm.2007.05.008 ↗
20. Effects of warm temper rolling on microstructure, texture and magnetic properties of strip-casting 6.5wt% Si electrical steel10.1016/j.jmmm.2014.06.053 ↗
21. Effects of hot rolled microstructure after twin-roll casting on microstructure, texture and magnetic properties of low silicon non-oriented electrical steel10.1016/j.jmmm.2016.07.034 ↗
22. Effect of cooling rate on bending behavior of 6.5 wt.% Si electrical steel thin sheets fabricated by strip casting and rolling10.1016/j.matchar.2015.11.008 ↗
23. Effects of Fe-6.5wt.%Si alloys prepared by different cooling methods on ordered structure and mechanical properties
24. An investigation on the role of texture evolution and ordered phase transition in soft magnetic properties of Fe–6.5wt%Si electrical steel10.1016/j.jmmm.2017.01.054 ↗
25. The effects of recrystallization texture and grain size on magnetic properties of 6.5 wt% Si electrical steel10.1016/j.jmmm.2015.10.047 ↗
26. Development of λ-fiber recrystallization texture and magnetic property in Fe-6.5wt% Si thin sheet produced by strip casting and warm rolling method10.1016/j.matlet.2012.09.046 ↗
27. Microstructural evolution in warm-rolled and cold-rolled strip cast 6.5 wt.% Si steel thin sheets and its influence on magnetic properties10.1016/j.jmmm.2017.02.057 ↗
28. Production of high silicon steel for electrical applications by thermomechanical processing10.1016/j.jmatprotec.2003.10.002 ↗
29. Thermomechanical processing of high Si-steel (up to 6.3% Si)10.1109/20.951160 ↗
30. Effect of annealing temperature on soft magnetic properties of cold rolled 0.30 mm thick Fe-6.5wt.%Si foils10.4283/JMAG.2011.16.2.177 ↗
31. The evolution of the goss texture in silicon steel10.1016/S1359-6462(98)00022-0 ↗
32. Relative effect(s) of texture and grain size on magnetic properties in a low silicon non-grain oriented electrical steel10.1016/S0304-8853(03)00142-2 ↗