Pre-annealing and magnetic induction in inhibitor-free 3% Si–Fe strips
Source abstract
Abstract
Abstract Effects of pre-annealing and hydrogen flow rate on final texture and magnetic induction have been investigated in inhibitor-free 100 μm thick 3% Si–Fe strips containing 18 ppm sulfur. Without any pre-annealing, the strip showed a low magnetic induction, due to various {1 1 0}, {1 0 0} and {1 1 1} final texture components. The number and the area fraction of {1 1 0} grains increased with increasing pre-annealing temperature and hydrogen flow rate. A pre-annealing temperature range that results in the sharp {1 1 0} 〈0 0 1〉 texture is observed, depending on the hydrogen flow rate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and interfaces · Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (5)
Show source-provided references
1. Vitos · Surf. Sci. · 1998 · 411 · 18610.1016/S0039-6028(98)00363-X ↗
2. Heo · Acta Mater. · 2000 · 48 · 290110.1016/S1359-6454(00)00084-7 ↗
3. Heo · Acta Mater. · 2003 · 51 · 495310.1016/S1359-6454(03)00258-1 ↗
4. Heo · J. Korean Phys. Soc. · 2004 · 44 · 1547
5. Heo · Mater. Lett. · 2005 · 59 · 282710.1016/j.matlet.2005.04.040 ↗