journal article·2026-02Open access

Hydrogen decrepitation of Sm2TM17 sintered magnets from scrap rotor assemblies

J. Griffiths, O.P. Brooks, V. Kozak, W. Xia, H. Kitaguchi, D. Brown, A. Campbell, A. Lambourne, R.S. Sheridan

Abstract

Sm 2 TM 17 sintered magnets (TM = Co, Fe, Cu, Zr) have been utilised in high temperature electrical machine rotor applications as they have exceptionally stable magnetic properties at 200–350 °C. Sm and Co are critical elements and reliance on the virgin material supply chain must be reduced. Recycling Sm 2 TM 17 magnets from end-of-life applications (EoL) via a hydrogen decrepitation (HD) processing route could be a potential solution and was the focus of this study. Sm 2 TM 17 magnets were exposed to 2–10 bar pressure at 100 °C for 72 h either loose or constrained within a rotor assembly. The hydrogen absorption/desorption behaviour, unit cell expansion and magnetic properties of the resulting powders were investigated. Loose and constrained magnets absorbed similar amounts of hydrogen (0.195–0.233 Wt%), with unit cell volume increasing by 1.35–1.87 %, and all samples reached maximum hydrogen desorption at 180–210 °C. Magnets constrained within the rotor assembly were embrittled after HD but required further mechanical agitation to form a powder. Therefore, hydrogen uptake was not impeded by physical constraint, but crack propagation was hampered. Magnetised rotors did not demagnetise during HD but did exhibit reduced magnetic properties. Lattice strain caused by hydrogen uptake may have interfered with magnetic exchange coupling without destroying the domain wall pinning coercivity mechanism. This study illustrated that HD processing is a potentially viable recycling route for Sm 2 TM 17 sintered magnets, however a combination of mechanical agitation and a demagnetisation step will be required for the most efficient recovery of Sm 2 TM 17 sintered magnets from EoL applications.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Magnetic Properties of Alloys · Superconducting Materials and Applications · Magnetic Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. The hard-magnetic properties of rare earth-transition metal alloys10.1109/TMAG.1972.1067368 ↗
2. Recent progress in 2:17-type permanent magnets10.1007/BF02648616 ↗
3. New type rare earth cobalt magnets with an energy product of 30 MGOe10.1143/JJAP.16.671 ↗
4. Rare-earth magnets: properties, processing and applications, in
5. Atomic structure and domain wall pinning in samarium-cobalt-based permanent magnets10.1038/s41467-017-00059-9 ↗
6. Magnetization reversal of (Sm, Ce)2(co, Fe, cu, Zr)17 magnets as per soft x-ray magnetic circular dichroism microscopy10.1063/5.0005635 ↗
7. Chemical stability and hydrogen reaction behavior of SmCo 2:17-type permanent magnets10.1002/adem.202201934 ↗
8. Role of primary Zr-rich particles on microstructure and magnetic properties of 2 : 17-type Sm-Co-Fe-Cu-Zr permanent magnets10.1016/j.jmst.2020.04.018 ↗
9. European Commission
10. European Commission · 2014
11. European Commission
12. European Commission · 2020
13. European Commission · 2023
14. Department for Business Energy & Industrial Strategy
15. The potential of hydrogen in permanent magnet production10.1016/0022-5088(87)90524-8 ↗
16. The use of hydrogen to separate and recycle neodymium-iron-boron-type magnets from electronic waste10.1016/j.jclepro.2015.05.033 ↗
17. Recycling of SmCo5 magnets by HD process10.1016/j.jmmm.2018.01.064 ↗
18. Hydrogen decrepitation as a method of powder preparation of a 2:17-type, Sm(Co, Cu, Fe, Zr)8.92 magnetic alloy10.1007/BF01026543 ↗
19. Hydrogen reaction with SmCo compounds: literature review10.1007/s40831-018-0195-z ↗
20. Kinetic studies of hydrogen desorption in SmCo 2/17-type sintered magnets10.1016/j.tca.2008.12.021 ↗
21. Coercivity in hydrogen-decrepitated Sm2Co17-type compounds10.1016/0925-8388(92)90243-3 ↗
22. Hydrogen decrepitation of a 2/17 sintered magnet at room temperature10.1016/j.jallcom.2006.11.139 ↗
23. The effects of knife milling and ball milling on hydrogen decrepitated Sm2TM17 sintered magnet powder for short-loop recycling10.3390/met15111258 ↗
24. Large scale recycling of industrial scrap Sm (co, Fe, cu, Zr)z magnets into valuable permanent magnets
25. Sulfuric acid leaching of Sm–co alloy waste and separation of samarium from cobalt10.1016/j.hydromet.2017.09.014 ↗
26. Recovery of valuable metals from SmCo magnets through sulfation, selective oxidation, and water leaching
27. Leaching of Sm, Co, Fe, and Cu from Spent SmCo Magnets Using Organic Acid
28. The effects of temperature and pressure on the hydrogen decrepitation and hydrogen desorption of Sm 2 TM 17 sintered magnets10.1016/j.intermet.2025.108831 ↗
29. The juxtaposition of our future electrification solutions: a view into the unsustainable life cycle of the permanent magnet electrical machine
30. The extraction of NdFeB magnets from automotive scrap rotors using hydrogen10.1016/j.jclepro.2020.124058 ↗
31. Hydrogen assisted recycling of Nd-Fe-B magnets from the end-of-life audio products10.1016/j.jmmm.2024.172239 ↗
32. Processability and Separability of commercial anti-corrosion coatings produced by in situ hydrogen-processing of magnetic scrap (HPMS) recycling of NdFeB10.3390/ma17112487 ↗
33. Comparative evaluation of anti-corrosion coatings for NdFeB-type magnets with respect to performance and recyclability via hydrogen-assisted recycling (HPMS) mater
34. Efficient solvent-based removal of epoxy polymer coatings for the recycling of neodymium-iron-boron magnets10.1016/j.jclepro.2025.147053 ↗
35. Brooks · 2022
36. Use of Helmholtz coils for magnetic measurements10.1109/20.3411 ↗
37. Stelter
38. Preparation of highly heat ­ resistant SmFe ­N magnetic powder by reduction ­ diff usion process10.2320/matertrans.MT-M2020185 ↗
39. IEC
40. Simple and approximate expressions of demagnetizing factors of uniformly magnetized rectangular rod and cylinder10.1063/1.343481 ↗
41. Cui · 2022 · 1279