Effects of milling-induced disorder on the lattice parameters and magnetic properties of hematite
Source abstract
Abstract
Abstract A ball-milling treatment in air for 30 min is enough to reduce anhydrous bulk hematite (α-Fe 2 O 3 ) grains to nanometric sizes. For milling times, t m , of 15, 30 min, 1 and 2 h, the crystals suffer an anisotropic lattice dilation, which is more pronounced for the smaller average grain sizes attained. Mossbauer and susceptibility results show that the process alters the effective Morin temperatures, T M . The transition occurs less sharply than for the non-milled material and spreads over a maximum extent of 50 K for t m =30 min. The susceptibility data indicate that the T M for the fraction of material undergoes the transition shifts toward values not lower than 235 K. For t m =10 h the transition is suppressed down to 12 K. Our results do not allow distinguishing bulk from surface regions of the grains. In addition, the disorder brought about by the milling reduces the magnetic response in the weak ferromagnetic state of α-Fe 2 O 3 . The modification of T M seems to depend mainly on the anisotropic dilation of the unit cell that affects the whole grain and it is related to the nanometric grain sizes achieved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Iron oxide chemistry and applications · Magnetic Properties and Synthesis of Ferrites · Minerals Flotation and Separation Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Morrish · 1994
2. Creer · 1975 · 664
3. Bruzzone · Phys. Rev. · 1983 · 28 · 243010.1103/PhysRevB.28.2430 ↗
4. Dang · Hyperfine Interactions · 1998 · 117 · 27110.1023/A:1012655729417 ↗
5. Kündig · Phys. Rev. · 1966 · 142 · 32710.1103/PhysRev.142.327 ↗
6. Amin · Phys. Rev. B · 1987 · 35 · 481010.1103/PhysRevB.35.4810 ↗
7. Sorescu · J. Appl. Phys. · 1999 · 85 · 554610.1063/1.369890 ↗
8. Vandenberghe · Hyperfine Interactions · 1990 · 53 · 17510.1007/BF02101046 ↗
9. Fujii · J. Magn. Magn. Mater. · 1994 · 135 · 23110.1016/0304-8853(94)90351-4 ↗
10. Nininger · J. Phys. Chem. Solids · 1978 · 39 · 13710.1016/0022-3697(78)90213-5 ↗
11. Koch · 1991 · 193
12. Suryanarayana · Progr. Mater. Sci. · 2001 · 46 · 110.1016/S0079-6425(99)00010-9 ↗
13. Kosmac · J. Mater. Res. · 1992 · 9 · 151910.1557/JMR.1992.1519 ↗
14. Mørup · Europhys. Lett. · 2001 · 56 · 44110.1209/epl/i2001-00538-7 ↗
15. Borzi · J. Magn. Magn. Mater. · 1999 · 205 · 23410.1016/S0304-8853(99)00495-3 ↗
16. Campbell · NanoStruct. Mater. · 1995 · 6 · 73510.1016/0965-9773(95)00163-8 ↗
17. Meillon · Phil. Mag. Lett. · 1995 · 72 · 10510.1080/09500839508241621 ↗
18. Zdujic · Mater. Sci. Eng. A · 1999 · 262 · 20410.1016/S0921-5093(98)01009-0 ↗
19. Randrianantoandro · Mater. Lett. · 2001 · 47 · 15010.1016/S0167-577X(00)00227-5 ↗
20. Rodrı́guez-Carvajal · Physica B · 1993 · 192 · 5510.1016/0921-4526(93)90108-I ↗
21. Brand · J. Phys. F · 1983 · 18 · 67510.1088/0305-4608/13/3/018 ↗
22. Williamson · Acta Metall. · 1953 · 1 · 2210.1016/0001-6160(53)90006-6 ↗
23. Del Bianco · Phys. Rev. B · 1997 · 56 · 889410.1103/PhysRevB.56.8894 ↗
24. Guérault · J. Phys.: Condens. Matter · 2000 · 12 · 949710.1088/0953-8984/12/45/311 ↗
25. Balogh · Phys. Rev. B · 2000 · 61 · 410910.1103/PhysRevB.61.4109 ↗
26. Zysler · J. Magn. Magn. Mater. · 2001 · 224 · 3910.1016/S0304-8853(00)01365-2 ↗
27. Liu · J. Phys.: Condens. Matter · 1994 · 6 · L49710.1088/0953-8984/6/34/001 ↗
28. Yu · J. Phys.: Condens. Matter · 1999 · 11 · 92710.1088/0953-8984/11/3/030 ↗