Microstructure refinement and significant improvements of magnetic properties in Pr2Fe14B/α-Fe nanocomposites
Source abstract
Abstract
Abstract Exchange coupled (Pr,Tb) 2 (Fe,Nb,Zr) 14 B/α-Fe nanocomposites have been produced by melt spinning. A trend for perpendicular and planar c -axis orientation of the 2:14:1 phase was observed in the free surface of ribbons spun at speeds below 10 m/s and at optimal speeds, respectively. Higher wheel speeds led to the formation of an amorphous phase that transformed to 2:14:1 phase around 680°C. Optimum magnetic properties were found in samples spun at 14–17 m/s and annealed at 700°C for 20 min. The loop squareness was also found to depend mainly on the microstructure that is very sensitive to the sample composition. A few percentage of Nb and Zr suppressed the grain growth, resulting in a drastic improvement of magnetic properties, with approximate 50% enhancement in the intrinsic coercivity and an increase in maximum energy product from 5.6 kOe and 14.7 MGOe for the (Nb,Zr)-free sample to 8.2 kOe and 20.3 MGOe for the (Nb,Zr)-substituted samples, respectively. The significant improvement in magnetic properties originated from a much finer and homogeneous nanocomposite microstructure with an average grain size of 20 nm, leading to a high remanence of 0.73 M s . Henkel plots indicate the enhancement of exchange coupling between hard and soft magnetic phases.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties of Alloys · Magnetic properties of thin films · Rare-earth and actinide compounds
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Skomski · Phys. Rev. B · 1993 · 48 · 1581210.1103/PhysRevB.48.15812 ↗
2. Withanawasam · J. Appl. Phys. · 1994 · 76 · 706510.1063/1.358028 ↗
3. Wu · J. Appl. Phys. · 2000 · 87 · 865810.1063/1.373593 ↗
4. Chen · J. Appl. Phys. · 2001 · 89 · 229910.1063/1.1344221 ↗
5. Neu · J. Appl. Phys. · 2001 · 90 · 154010.1063/1.1380223 ↗
6. Jin · IEEE Trans. Magn. · 2001 · 37 · 256410.1109/20.951236 ↗
7. Zhang · J. Appl. Phys. · 2001 · 89 · 150910.1063/1.1335637 ↗
8. Yin · J. Alloys Compounds · 2001 · 316 · 29610.1016/S0925-8388(00)01497-3 ↗
9. Schrefl · Phys. Rev. B · 1994 · 49 · 610010.1103/PhysRevB.49.6100 ↗
10. Chen · J. Alloys Compounds · 2001 · 327 · 20110.1016/S0925-8388(01)01418-9 ↗
11. Chen · J. Appl. Phys. · 2001 · 85 · 590810.1063/1.369910 ↗
12. McComrmick · J. Appl. Phys. · 1998 · 83 · 625610.1063/1.367772 ↗
13. Zhang · Appl. Phys. Lett. · 2001 · 79 · 242610.1063/1.1409269 ↗
14. Shima · Appl. Phys. Lett. · 2001 · 78 · 204910.1063/1.1360234 ↗
15. Jin · J. Magn. Magn. Mater. · 2002 · 242–245 · 130710.1016/S0304-8853(01)01273-2 ↗
16. Fischer · J. Magn. Magn. Mater. · 1996 · 153 · 3510.1016/0304-8853(95)00494-7 ↗
17. Chen · J. Magn. Magn. Mater. · 1999 · 195 · 42010.1016/S0304-8853(99)00132-8 ↗
18. Chen · J. Appl. Phys. · 1999 · 85 · 591710.1063/1.369913 ↗
19. Garcı́a-Otero · J. Appl. Phys. · 2000 · 87 · 737610.1063/1.372996 ↗
20. Kelly · IEEE Trans. Magn. · 1989 · 25 · 388110.1109/20.42466 ↗