Ce and La as substitutes for Nd in Nd2Fe14B-based melt-spun alloys and hot-deformed magnets: a comparison of structural and magnetic properties
Source abstract
Abstract
Abstract Ce and La as very cheap rare-earth elements were used to substitute Nd in nanocrystalline melt-spun ribbons of nominal compositions (Nd1−xREx)13.6FebalCo6.6Ga0.6B5.6 (x = 0, 0.1, 0.2, … 1 for RE = Ce) and (x = 0, 0.1, 0.2, … 0.5 for RE = La). Ce substitution gradually decreased the Nd2Fe14B lattice constants and produced CeFe2 segregation from x = 0.7. La substitution led to lattice expansion along the c-axis and induced segregation of α-Fe and Nd2Fe17 at x = 0.5. Grain coarsening was observed in the Ce-substituted samples while La was found to suppress grain growth. Cerium worsened the magnetic properties of as-spun powders after an initial improvement in (Nd0.9Ce0.1)13.6FebalCo6.6Ga0.6B5.6 alloy which showed a coercivity (µ0Hc) of 1.54 T and a remanence (Br) of 0.81 T. Coercivity dropped with increasing La concentration but remanence increased from 0.73 T in the base composition to 0.88 T at x = 0.3. The Curie temperatures (TC) showed a slight decrease in both cases until x = 0.4. It then dropped abruptly for increasing Ce fractions and increased at x = 0.5 La. For x = 0.2 and 0.3 Ce and x = 0.2 La fractions, the melt-spun samples were further processed by hot-pressing and hot-deformation. The hot-pressed (Nd0.8La0.2)13.6FebalCo6.6Ga0.6B5.6 alloy measured lower coercivity but increased remanence comparing to the Ce-substituted alloys. However, this composition responded poorly to hot-deformation, severe cracking being induced in the process. Due to enhanced hot-workability, best magnetic properties were obtained after deformation for the (Nd0.7Ce0.3)13.6FebalCo6.6Ga0.6B5.6 alloy (µ0Hc = 1.09 T, Br = 0.97 T and energy product (BH)max = 170 kJ/m3).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties of Alloys · Rare-earth and actinide compounds · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Magnetic materials and devices for the 21st century: stronger, lighter, and more energy efficient10.1002/adma.201002180 ↗
2. REE recovery from end-of-life NdFeB permanent magnet scrap: a critical review10.1007/s40831-016-0090-4 ↗
3. Neodymium-iron-boron permanent magnets10.1016/0304-8853(91)90812-O ↗
4. Critical Materials Strategy, U. S. Department of Energy, December, 2011.
5. Critical Raw Materials Factsheets, European Commission, June 2017.
6. Recycling of rare earths: a critical review10.1016/j.jclepro.2012.12.037 ↗
7. Rare earths and the balance problem10.1007/s40831-014-0005-1 ↗
8. Rare earths and the balance problem: how to deal with the changing markets?10.1007/s40831-018-0162-8 ↗
9. Heavy rare earth free, free rare earth and rare earth free magnets - Vision and Reality10.1016/j.scriptamat.2018.01.032 ↗
10. Relationships between crystal structure and magnetic properties in Nd2Fe14B10.1103/PhysRevB.29.4176 ↗
11. Magnetic properties of ternary rare-earth compounds of the type R2Fe14B10.1016/0304-8853(84)90261-0 ↗
12. Crystal and magnetic structure of Ce2Fe14B and Lu2Fe14B10.1016/0304-8853(86)90712-2 ↗
13. Magnetic properties and microstructure of melt-spun Ce-Fe-B magnets10.1109/TMAG.2015.2447553 ↗
14. Magnetic hardening of Ce2Fe14B10.1063/1.3675175 ↗
15. Coercivity enhancement in Ce-Fe-B based magnets by core-shell grain structuring10.1063/1.4945040 ↗
16. Manipulating Ce valence in RE2Fe14B tetragonal compounds by La-Ce co-doping: resultant Crystallographic and magnetic anomaly
17. Preparation and microstructure of La-containing R-Fe-B permanent magnets10.1063/1.342711 ↗
18. Effect of composition on the magnetic properties of melt-spun (Ce1-xNdx)13.5(Fe1-y-zCoySiz)80B6.5 sintered magnets10.1063/1.347985 ↗
19. The effects of La-substitution on the microstructure and magnetic properties of nanocomposite NdFeB melt spun ribbons10.1016/S0304-8853(96)00632-4 ↗
20. Cerium: an unlikely replacement of dysprosium in high performance Nd-Fe-B permanent magnets10.1002/adma.201404892 ↗
21. Composition related magnetic properties and coercivity mechanism for melt spun [(La0.5Ce0.5)1−xREx]10Fe84B6 (RE = Nd or Dy) nanocomposite alloys10.1016/j.jmmm.2015.09.051 ↗
22. Effects of Ce-substitution on the magnetic properties and microstructure of Nd-Pr-Fe-B melt-spun powders10.1016/j.jmmm.2015.09.027 ↗
23. A novel approach for plastic-bonded magnets of the type MQU-F melt spun NdFeGaB-type alloys10.1109/TMAG.2017.2701842 ↗
24. Net-shape and crack-free production of Nd-Fe-B magnets by hot deformation10.1016/j.jallcom.2013.11.188 ↗
25. Coercivity enhancement in hot-pressed Nd-Fe-B permanent magnets with low-melting eutectics10.1063/1.4859097 ↗
26. Grain boundary diffusion in nanocrystalline Nd-Fe-B permanent magnets with low-melting eutectics10.1016/j.actamat.2016.05.048 ↗
27. The Fe-La (Iron-Lanthanum) system10.1007/BF02647859 ↗
28. Compilation of calculated data useful in predicting metallurgical behavior of the elements in binary alloy systems., Technical report
29. Solid-solution stability and preferential site-occupancy in (R-R')2Fe14B compounds10.1063/1.4953874 ↗
30. Site-preference and valency for rare-earth sites in (R-Ce)2Fe14B magnets10.1063/1.4789527 ↗
31. Flux growth and characterization of Ce-substituted Nd2Fe14B single crystals10.1016/j.jmmm.2016.10.127 ↗
32. The partitioning of La and Y in Nd-Fe-B magnets: a first-principles study10.1016/j.jallcom.2012.10.056 ↗
33. Effects of quench rate on the microstructure in melt-spun Nd-Fe-B alloys10.1557/JMR.1991.0724 ↗
34. Solidification, microstructural refinement and magnetism in Nd2Fe14B10.1016/S0304-8853(01)00955-6 ↗
35. Substitution of Nd with other rare earth elements in melt spun Nd2Fe14B magnets10.1063/1.4944080 ↗
36. Hot workability of melt spun Nd-Fe-Co-B magnets10.1063/1.347844 ↗
37. The dependence of magnetic properties and hot workability of rare earth-iron-boride magnets upon composition10.1109/TMAG.2004.832240 ↗
38. Effect of additives on hot deformation behavior of melt spun Nd-Fe-Co-B magnets10.1063/1.349943 ↗