Microstructural and magnetic studies of L10 FePt–SiO2 nano-composite thin film with columnar structure for perpendicular magnetic recording
Source abstract
Abstract
Abstract (Fe 50 Pt 50 ) 100− x -(SiO 2 ) x films ( x =0–30 vol%) were grown on a textured Pt(0 0 1)/CrRu(0 0 2) bilayer at 420 °C using glass substrates. FePt(0 0 1) preferred orientation was obtained in the films. Interconnected microstructure with an average grain size of about 30 nm is observed in the binary FePt film. As SiO 2 is incorporated, it precipitates as particles are dispersed at FePt grain boundaries. When the content of SiO 2 is increased to 13 vol%, columnar FePt with (0 0 1) texture separated by SiO 2 is attained. The FePt columns have a length/radius ratio of 2:1. Additionally, the mean grain size is reduced to about 13 nm. The development of this well-isolated columnar structure leads to an enhancement in coercivity by about 44% from 210 to 315 kA/m. As the SiO 2 content exceeds 20 vol%, a significant ordering reduction is found accompanied by a transformation of preferred orientation from (0 0 1) to (2 0 0) and the columnar structure disappears, resulting in a drastic degradation in magnetism. The results of our study suggest that isolated columnar, grain refined, (0 0 1)-textured FePt film can be achieved via the fine control of SiO 2 content. This may provide useful information for the design of FePt perpendicular recording media.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic properties of thin films · Magnetic Properties and Applications · Metallic Glasses and Amorphous Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. Shun-ichi Iwasaki, Proceeding of the Eighth Perpendicular Magnetic Recording Conference, Tokyo, Japan, 2007.
2. Dutson · IEEE Trans. Magn. · 2007 · 43 · 81410.1109/TMAG.2006.888437 ↗
3. Piramanayagam · IEEE Trans. Magn. · 2007 · 43 · 63310.1109/TMAG.2006.888206 ↗
4. 〈http://www.hitachigst.com/hdd/research/recording_head/pr/index.html〉.
5. Honda · J. Appl. Phys. · 1994 · 75 · 598410.1063/1.355533 ↗
6. Luo · Appl. Phys. Lett. · 2000 · 77 · 222510.1063/1.1314289 ↗
7. Li · Appl. Phys. Lett. · 2007 · 91 · 15250210.1063/1.2798584 ↗
8. Luo · Appl. Phys. Lett. · 1999 · 75 · 316210.1063/1.125264 ↗
9. Watanabe · Appl. Phys. Lett. · 2000 · 76 · 397110.1063/1.126838 ↗
10. Kuo · J. Appl. Phys. · 2000 · 87 · 41910.1063/1.371878 ↗
11. Peng · J. Appl. Phys. · 2006 · 99 · 08F90710.1063/1.2176306 ↗
12. Suzuki · J. Magn. Magn. · 2005 · 286 · 30610.1016/j.jmmm.2004.09.084 ↗
13. Chen · Appl. Phys. Lett. · 2007 · 91 · 13250610.1063/1.2789790 ↗
14. Lee · Appl. Phys. Lett. · 2007 · 90 · 25251110.1063/1.2748326 ↗
15. Wu · Appl. Phys. Lett. · 2007 · 91 · 07250210.1063/1.2770652 ↗
16. Sun · Thin Solid Films · 2008 · 516 · 115510.1016/j.tsf.2007.06.128 ↗