Three-dimensional atom probe analysis and magnetic properties of Fe 85 Cu 1 Si 2 B 8 P 4 melt spun ribbons

S. Jafari, A. Beitollahi, B. Eftekhari Yekta, T. Ohkubo, Viktoria Budinsky, Mie Marsilius, S. Mollazadeh, Giselher Herzer, K. Hono

Publisher page

Abstract

Abstract The effect of phosphorous on the microstructure and magnetic properties of as-spun and flash annealed (389–535 °C for 7 s) Fe85Cu1Si2B8P4 melt spun ribbons were investigated by three-dimensional atom probe (3DAP) and high resolution transmission electron microscopy (HRTEM) techniques. The formation of quasi-amorphous α -Fe clusters of 3–5 nm size in an amorphous matrix were detected by HRTEM, despite the high quenching rate applied by high wheel speed used. Flash annealing of the as-spun ribbons gave rise to the formation of nanocrystalline α -Fe (Si) phase in amorphous matrix containing Fe, Si, B and P elements as detected by 3DAP. Comparing 3DAP analysis of the samples annealed at 445 °C and 535 °C revealed that the concentration of P and B in amorphous matrix were increased for the latter. Further, it was shown that P hardly solidified into nanocrystalline phase and partitioned in amorphous phase alongside B atoms leading to the further stabilization of amorphous matrix as confirmed by 3DAP analysis. The highest magnitude of saturation magnetic induction (Bs~1.85 T) and the lowest coercive field (~10–20 A/m) were obtained for the samples annealed above 445 °C, for which noticeable reduction of saturation magnetostriction ( λ s) were also detected.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Advanced Materials Characterization Techniques · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Grain size dependence of coercivity and permeability in nanocrystalline ferromagnets10.1109/20.104389 ↗
2. Grain structure and magnetism of nanocrystalline ferromagnets10.1109/20.42292 ↗
3. Amorphous and nanocrystalline materials for applications as soft magnets10.1016/S0079-6425(99)00002-X ↗
4. Magnetic properties of nanocrystalline Fe82.65Cu1.35SixB16−x alloys (x=0–7)10.1063/1.2769956 ↗
5. New high-Bs Fe-based nanocrystalline soft magnetic alloys10.1143/JJAP.46.L477 ↗
6. Modern soft magnets: amorphous and nanocrystalline materials10.1016/j.actamat.2012.10.040 ↗
7. Effect of super-heat treatment and quenching wheel speed on the structure and magnetic properties of Fe–Si–Nb–Cu–B–Al–Ge melt spun ribbons10.1016/j.jnoncrysol.2007.08.036 ↗
8. Structural characterization and magnetoimpedance effect in amorphous and nanocrystalline AlGe-substituted FeSiBNbCu ribbons10.1016/j.jmmm.2006.09.014 ↗
9. Soft magnetic metallic materials10.1016/S1574-9304(05)80103-8 ↗
10. New Fe-based soft magnetic alloys composed of ultrafine grain structure10.1063/1.342149 ↗
11. Magnetic properties of high Fe-based amorphous material10.1016/j.jmmm.2006.02.167 ↗
12. J.A. Vaccari, Des. Eng. 52 (1981).
13. New excellent soft magnetic FeSiBPCu nanocrystallized alloys with high Bs of 1.9T From nanohetero-amorphous phase10.1109/TMAG.2009.2023862 ↗
14. New Fe-metalloids based nanocrystalline alloys with high Bs of 1.9T and excellent magnetic softness10.1063/1.3058624 ↗
15. FeSiBPCu nanocrystalline soft magnetic alloys with high Bs of 1.9T produced by crystallizing hetero-amorphous phase10.2320/matertrans.MER2008306 ↗
16. Soft magnetic FeSiBPCu heteroamorphous alloys with high Fe content10.1063/1.3060579 ↗
17. Effect of P on crystallization behavior and soft-magnetic properties of Fe83.3Si4Cu0.7B12−xPx nanocrystalline soft-magnetic alloys10.1016/j.tsf.2011.03.110 ↗
18. Low core loss of Fe85Si2B8P4Cu1 nanocrystalline alloys with high Bs and B80010.1016/j.jallcom.2010.11.012 ↗
19. Low core losses and magnetic properties of Fe85–86Si1–2B8P4Cu1 nanocrystalline alloys with high B for power applications (invited)10.1063/1.3535169 ↗
20. Effect of P to B concentration ratio on soft magnetic properties in FeSiBPCu nanocrystalline alloys10.1063/1.3672082 ↗
21. Role of Si in high Bs and low core-loss Fe85.2B10−XP4Cu0.8SiX nano-crystalline alloys10.1063/1.4765718 ↗
22. Magnetic properties and structure of Fe83.3–85.8B7.0−4.5P9Cu0.7 nanocrystalline alloys10.1063/1.4794377 ↗
23. Fe-rich soft magnetic FeSiBPCu hetero-amorphous alloys with high saturation magnetization10.2320/matertrans.ME200831 ↗
24. In-situ Lorentz microscopy of Fe85Si2B8P4Cu1 nanocrystalline soft magnetic alloys10.1016/j.jmmm.2014.08.101 ↗
25. Direct imaging of structural heterogeneity of the melt-spun Fe85.2Si2B8P4Cu0.8 alloy10.1063/1.4923329 ↗
26. Nanocrystalline soft magnetic Fe–Si–B–P–Cu alloys with high B of 1.8–1.9T contributable to energy saving10.1109/TMAG.2011.2175210 ↗
27. Competition driven nanocrystallization in high Bs and low coreloss Fe–Si–B–P–Cu soft magnetic alloys10.1016/j.scriptamat.2014.08.023 ↗
28. S. Jafari, A. Beitollahi, B. Eftekhari, T. Yekta, V. Ohkubo, M. Budinsky, G. Marsilius, K. Herzer, Hono Atom probe analysis and magnetic properties of nanocrystalline Fe84.3Si4B8P3Cu0.7 2015, in preparation.10.1016/j.jallcom.2016.03.005 ↗
29. 〈http://www.foerstergroup.com/KOERZIMAT-CS-coercivity-field-strenght.157.0.html〉.
30. Measurement of saturation magnetostriction of a thin amorphous ribbon by means of small-angle magnetization rotation10.1109/TMAG.1980.1060610 ↗
31. Effect of stress annealing on the saturation magnetostriction of nanocrystalline Fe73.5Cu1Nb3Si15.5B710.1109/TMAG.2009.2031975 ↗
32. Broadening the applications of the atom probe technique by ultraviolet femtosecond laser10.1016/j.ultramic.2010.11.020 ↗
33. 3DAP analysis of (Ga,Mn)As diluted magnetic semiconductor thin film10.1016/j.ultramic.2008.11.011 ↗
34. Cu addition effect on soft magnetic properties in Fe–Si–B alloy system10.1063/1.2829240 ↗
35. Improvement of soft magnetic properties in (Fe0.85B0.15)100−xCux melt-spun alloys10.2320/matertrans.MAW200730 ↗
36. Nanoscale microstructural analysis of metallic materials by atom probe field ion microscopy10.1016/S0079-6425(01)00007-X ↗
37. The effect of grain-size distribution on coercivity in nanocrystalline soft magnetic alloys10.1016/j.jmmm.2003.12.368 ↗
38. Improvement of soft magnetic properties by simultaneous addition of P and Cu for nanocrystalline FeNbB alloys10.1063/1.2714676 ↗
39. Cu clustering and Si partitioning in the early crystallization stage of an Fe73.5Si13.5B9Nb3Cu1 amorphous alloy10.1016/S1359-6454(98)00392-9 ↗
40. Surface crysatllization and magnetic properties of Fe84.3Cu0.7Si4B8P3 soft magnetic ribbons10.1016/j.actamat.2015.05.051 ↗