journal article·2024-06-01

Effect of pulse electroplating parameters on the morphology and corrosion resistance of Ag plating coating

Guoliang Zhang, Qiu Li, De Sun, Xin Ye, Xiaolong Yi, Wei Fang, Zhitao Luo

Publisher page

Abstract

Abstract Pulse electroplating technology has the characteristics of fine grain and good corrosion resistance. In order to ensure the good application of electroplated silver cone cavity in solar radiation detector. The effects of three process parameters, including average current density (0.4–1 A dm−2), pulse on-time (0.2–1.8 ms) and pulse off-time (0.8–4.8 ms), on the deposition rate, appearance and corrosion resistance of silver coating were studied by control variates. The surface morphology and composition of silver coatings were studied by scanning electron microscope (SEM), laser confocal microscopy and energy dispersive x-ray spectrometer (EDX). The corrosion resistance of silver coating in 3.5 wt% NaCl solution (pH=5.5) was studied by polarisation curves and electrochemical impedance spectroscopy. The results show that pulse electroplating takes advantage of the dynamic change of current to influence the size of deposited particles and the degree of densification of the coating by precisely adjusting the pulse plating parameters, and ultimately obtains the coating with excellent morphology. The optimal parameters are: average current density 0.6 A dm−2, pulse on-time 1.2 ms, pulse off-time 1.8 ms. The silver coating prepared under process conditions has excellent corrosion resistance (7059 Ω cm−2). The surface crystal grain is dense, without obvious defects.
Source: crossref · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Copper Interconnects and Reliability · Electronic Packaging and Soldering Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. DMH and NA–based cyanide-free silver electroplating bath: a promising alternative to cyanide ones in microelectronics10.1007/s11581-020-03541-5 ↗
2. Microstructure-corrosion behaviour relationship of micro-alloyed Mg-0.5Zn alloy with the addition of Ca, Sr, Ag, In and Cu10.1016/j.matdes.2020.108980 ↗
3. Cyanide-free silver electroplating process in thiosulfate bath and microstructure analysis of Ag coatings (in English)10.1016/S1003-6326(13)62935-0 ↗
4. Experimental and theoretical studies of DMH as a complexing agent for a cyanide-free gold electroplating electrolyte10.1039/C5RA13140E ↗
5. Investigations on the corrosion properties of Sn–0.5Cu–Bi–xAg lead free solder alloys in 3.5% NaCl solution10.1007/s42341-020-00219-7 ↗
6. The effect of TiO2 concentration on morphology, wear and corrosion properties of NiB-TiO2 composite coatings by ultrasonic-assisted pulse electrodeposition10.1088/2051-672X/acaff9 ↗
7. Effect of current density on the texture, residual stress, microhardness and corrosion resistance of electrodeposited chromium coating10.1016/j.surfcoat.2023.129868 ↗
8. Antibacterial TaC-(Fe,Cr,Mo,Ni)-(Ag/Cu) composite coatings with high wear and corrosion resistance in artificial seawater10.3390/lubricants10110320 ↗
9. Growth and transformation mechanism of ternary CuAgSe dendrites from binary Ag2 Se dendrites10.1002/ejic.201100440 ↗
10. Electrochemical noise analysis for Nylon/Titanium hybrid materials10.1149/1.3660601 ↗
11. Electrochemical corrosion behavior of pulse and DC electrodeposited Co–P coatings10.1016/j.surfcoat.2011.09.063 ↗
12. Highly corrosion resistant bright silver metallization deposited from a neutral cyanide-free solution10.1016/j.mee.2011.04.016 ↗
13. Proposing a new complexing agent for cyanide-free silver electroplating through a comprehensive computational study of dimethyl hydantoin10.1080/08927022.2021.1895436 ↗
14. Role of polyethyleneimine as an additive in cyanide-free electrolytes for gold electrodeposition10.1039/C5RA12217A ↗
15. Pyrimidine derivative-based cyanide-free silver electroplating bath10.1080/00202967.2022.2070166 ↗
16. A composite additive used for a new cyanide-free silver plating bath (II): an insight by electrochemical measurements and quantum chemical calculation10.1039/c7nj02638b ↗
17. A combined theoretical and experimental study for silver electroplating10.1038/srep03837 ↗
18. Grain refinement by means of phase transformation and recrystallization induced by electropulsing (in English)10.1016/S1003-6326(11)61605-1 ↗
19. Pulse electrodeposition of nano-crystalline Ni-W alloy and the influence of tungsten composition on structure, microhardness and corrosion properties10.1016/j.jallcom.2021.158987 ↗
20. Influence of pulse current forward-reverse duty cycle on structure and performance of electroplated W–Cu composite coatings10.3390/MA14051233 ↗
21. Preparation of Co–P–TiO2 nanocomposite coatings via a pulsed electrodeposition process10.1080/02670844.2019.1693172 ↗
22. Pulse electroplating of Ni−W−P coating and its anti-corrosion performance (in English)10.1016/S1003-6326(18)64641-2 ↗
23. Effect of CeO2 on corrosion resistance of high-current pulsed electron beam treated pressureless sintering Al-20SiC composites10.3390/coatings11060707 ↗
24. Study of the electrodeposition of silver nanoparticles on glassy carbon by galvanostatic control10.1149/10101.0415ecst ↗
25. Nano-Grain Ni/ZrO2 functional gradient coating fabricated by double pulses electrodeposition with enhanced high temperature corrosion performance10.3390/coatings10040332 ↗
26. Green preparation of silver coating on AISI 304 stainless steel surface by Ag nanocrystalline in situ growth and the wear resistance10.1016/j.apsusc.2018.06.146 ↗
27. Galvanostatic pulse plating of Cu-Al alloy in a room-temperature chloroaluminate molten salt rotating ring-disk electrode studies10.1149/1.1366624 ↗
28. Pulse and pulse reverse plating—Conceptual, advantages and applications10.1016/j.electacta.2007.11.054 ↗
29. Effects and characterisations of pulse electrodeposition parameters of silver in terms of scattering parameter and surface roughness for waveguides operating at high frequencies10.1504/IJSURFSE.2021.116326 ↗
30. Corrosion and wear study of Ni–W–B/WC composite coatings electroplated by pulse plating10.1002/adem.202000426 ↗
31. Pulsed electrodeposition of ultrathin polyaniline films and mechanistic understanding of their anion-mediated electrochemical behavior10.1149/1945-7111/aba5d5 ↗
32. Electrochemical noise analysis of corrosion behaviour of asymmetric electrodes made of mild steel in NaHCO3 solutions at different NaCl concentrations10.1016/j.measurement.2020.107501 ↗
33. Identifying defect size in organic coatings by electrochemical noise, galvanostatic step and potentiostatic step techniques10.1016/j.jelechem.2019.113596 ↗
34. Impact of the confinement plate on the synthetic jet10.1063/5.0022813 ↗
35. Selective phase corrosion and cavitation erosion behaviors of various copper alloys in 3.5% NaCl solutions with different pH values10.1016/S1003-6326(23)66316-2 ↗
36. Unraveling crystal symmetry and strain effects on electronic band structures of SiC polytypes10.1063/5.0010512 ↗
37. Electrodeposited copper using direct and pulse currents from electrolytes containing low concentration of additives10.1016/j.surfcoat.2018.01.067 ↗
38. Electronucleation mechanism of copper in wastewater by controlled electrodeposition analysis10.1039/D0RA07380F ↗
39. Mechanisms of localized pulsed electrodeposition (L-PED) for microscale 3D printing of nanotwinned metals10.1149/2.0051910jes ↗
40. Potassium ferricyanide silver plating Material protection10.16577/j.cnki.42–1215/tb.1972.04.004 ↗
41. Effect of concentration of TiC on the properties of pulse electrodeposited Ni–P–TiC nanocomposite coatings10.1016/J.CERAMINT.2021.03.259 ↗
42. Pulse electrodeposition of nanocrystalline nickel using ultra narrow pulse width and high peak current density10.1016/S0257-8972(03)00014-8 ↗
43. The influence of different preparation methods on the erosion behavior of NiP-ZrO2 nanocomposite coating10.1016/j.triboint.2022.108014 ↗
44. Influence of pulse parameters on the mechanical properties and electrochemical corrosion behavior of electrodeposited Ni-W alloy coatings with high tungsten content10.1016/j.corsci.2019.108409 ↗
45. Study the effect of surface parameters variation on the corrosion behavior of thin chromium layer on modified titanium10.1134/S2070205122020186 ↗
46. Study the variation of surface topography & corrosion resistance of Cr-GO nanocomposite coatings by addition of GO nanoparticles
47. Surface morphology and crystal orientation of electrodeposited tungsten coatings with different pulse parameters10.1007/s12598-016-0825-1 ↗
48. Electroplating silver solution-discussion of cyanide-free formulations10.16577/j.cnki.42–1215/tb.1973.02.008. ↗