journal article·2020-03

Metal-coated Sm2Fe17N3 magnet powders with an oxide-free direct metal-metal interface

Wataru Yamaguchi, Rikio Soda, Kenta Takagi

Publisher page

Abstract

Abstract We successfully prepared Sm2Fe17N3 magnet powders uniformly coated with non-magnetic metals without oxides in the interface between the magnet phase and the coating layer. The whole process from powder preparation by jet milling to coating was undertaken in a low-oxygen atmosphere. Powder coating was investigated using two different dry thin-film preparation methods, arc-plasma deposition (APD) and DC magnetron sputtering. The powder was continuously stirred during coating in order to ensure the uniformity of the coating layer. Scanning electron microscopy with energy dispersive X-ray spectrometry (EDS) and X-ray photoelectron spectroscopy demonstrated that an arc-plasma deposited Zn layer on Sm2Fe17N3 powder had nearly 100% coverage and an oxide-free direct metal-metal interface with the underlying magnet phase. The effects of metal-coatings and coating methods on the coercivity of the magnet powder were evaluated with Zn, Ti, and Al as the coating materials and with APD and DC magnetron sputtering as the coating methods. With all three coating metals, the sputter-coated Sm2Fe17N3 powders showed higher coercivity than the raw powders. The APD powders had lower coercivity than the sputter-coated powders, and in the case of Ti, coercivity was even lower than that of the raw powder. Transmission electron microscopy with EDS and nano-beam electron diffraction suggested that the high energy particles deposited by APD damaged the magnetic phase. This study demonstrated that nanometer-thick coatings of non-magnetic metals without oxides in the interface with the magnet phase have the effect of enhancing the coercivity of Sm2Fe17N3 powders, provided the proper coating method is selected.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Hydrogen Storage and Materials · Rare-earth and actinide compounds

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. T. Iriyama, K. Kobayashi, H. Imai, European Patent, Appl. Pub. No. 0-369-097-Al, 1989.
2. Improved magnetic properties by treatment of iron-based rare earth intermetallic compounds in ammonia10.1016/0304-8853(90)90756-G ↗
3. Effect of nitrogen content on magnetic properties of Sm2Fe17Nx (0<x<6)10.1109/20.179482 ↗
4. Enhanced coercivity of spark plasma sintered Zn-bonded Sm-Fe-N magnets10.1016/j.scriptamat.2012.06.038 ↗
5. Magnetic properties of R2Fe17N2.7 compounds10.1016/0022-5088(91)90056-A ↗
6. Preparation of Sm2Fe17Nx powders and their bonded magnets with high-performance permanent magnetic characteristics10.1021/cm970036z ↗
7. Coercivity of Zn evaporation-coated Sm2Fe17Nx fine powder and its bonded magnets10.1016/S0925-8388(97)00155-2 ↗
8. High electrical resistance composite magnets of Sm2Fe17N3 powders coated with ferrite layer for high frequency applications10.1063/1.2832864 ↗
9. Increase of energy products of Zn-bonded Sm-Fe-N magnets with low oxygen content10.1016/j.jmmm.2018.07.064 ↗
10. Ozaki, Microstructural behavior on particle surfaces and interfaces in Sm2Fe17N3 powder compacts during low-temperature sintering10.1016/j.jmmm.2012.02.021 ↗
11. Role of surface iron oxides in coercivity deterioration of Sm2Fe17N3 magnet associated with low temperature sintering10.2320/matertrans.M2018358 ↗
12. Anisotropic Sm2Fe17N3 sintered magnets without coercivity deterioration10.1063/1.4967364 ↗
13. Comparison of the sputter rates of oxide films relative to the sputter rate of SiO210.1116/1.3456123 ↗
14. Metal bonded Sm2Fe17N3-δ magnets10.1063/1.348900 ↗
15. HIP sintering and magnetic properties of Sm2Fe17N3 with Zn additive10.1016/j.jmmm.2003.07.003 ↗
16. Magnetic properties of Sm-Fe-N anisotropic magnets produced by magnetic-field-assisted spark plasma sintering10.1016/j.mseb.2010.01.032 ↗
17. Enhanced coercivity of spark plasma sintered Zn-bonded Sm-Fe-N magnets10.1016/j.scriptamat.2012.04.001 ↗
18. Influence of swaging on the magnetic properties of Zn-bonded Sm-Fe-N magnets10.2320/matertrans.M2015190 ↗
19. Submicron Ag-coated Cu particles and characterization methods to evaluate their quality10.1016/j.jallcom.2016.08.009 ↗
20. Grain boundary complexions and pseudopartial wetting10.1016/j.cossms.2016.05.006 ↗
21. Influence of surface pretreatment and electrocoating parameters on the adhesion of cathodic electrocoat to the Al alloy surfaces10.1016/S0300-9440(98)00068-X ↗