High anisotropic NdFeB submicro/nanoflakes prepared by surfactant-assisted ball milling at low temperature
Source abstract
Abstract
Abstract Hard magnetic NdFeB submicro/nanoflakes were successfully prepared by surfactant-assisted ball milling at low temperature (SABMLT) by specially using 2-methyl pentane and trioctylamine (TOA) as solvent and surfactant, respectively. Influences of the amount of TOA and milling temperature on the crystal structure, morphology and magnetic performances of the as-prepared NdFeB powders were investigated systematically. There is significant difference on morphology between the NdFeB powders milled at room and low temperature. The NdFeB powders with flaky morphology could be obtained even with a small amount of TOA by SABMLT, which could not be achieved by surfactant-assisted ball milling at room temperature (SABMRT). The better crystallinity, better grain alignment, higher coercivity, larger saturation magnetization and remanence ratio were achieved in the samples prepared by SABMLT. Furthermore, the final NdFeB powders prepared by SABMLT possessed a lower amount of residual TOA than those prepared by SABMRT. It was demonstrated that SABMLT is a promising way to fabricate rare-earth-transition metal nanoflakes with high anisotropy for permanent magnetic materials. The effective method of preparing NdFeB flakes by lowering temperature will be also useful to fabricate flakes of other functional materials.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties of Alloys · Magnetic properties of thin films · Metallic Glasses and Amorphous Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Effect of Cu and Ga additions on the anisotropy of R2Fe14B/α-Fe nanocomposite die-upset magnets (R=Pr, Nd)10.1016/j.jmmm.2005.09.013 ↗
2. Materials science: the pull of stronger magnets10.1038/472022a ↗
3. Ferromagnetic nanoparticles: synthesis, processing, and characterization10.1007/s11837-010-0060-4 ↗
4. Fabrication of ultrafine Nd-Fe-B powder by a modified reduction-diffusion process10.1016/S1001-0521(08)60086-8 ↗
5. Sol−gel based chemical synthesis of Nd2Fe14B hard magnetic nanoparticles10.1021/cm103148n ↗
6. Novel ferromagnetic materials of SmCo5 nanoparticles in single-nanometer size: chemical syntheses and characterizations10.1088/0957-4484/21/9/095603 ↗
7. Novel Nd2Fe14B nanoflakes and nanoparticles for the development of high energy nanocomposite magnets10.1088/0957-4484/21/29/295705 ↗
8. Single-crystal and textured polycrystalline Nd2Fe14B flakes with a submicron or nanosize thickness10.1016/j.actamat.2011.11.062 ↗
9. Magnetic nanoparticles produced by surfactant-assisted ball milling10.1063/1.2170593 ↗
10. Anisotropic PrCo5 Nanoparticles by Surfactant-Assisted Ball Milling10.1109/TMAG.2009.2022643 ↗
11. Strong textured SmCo5 nanoflakes with ultrahigh coercivity prepared by multistep (three steps) surfactant-assisted ball milling10.1038/srep13117 ↗
12. Preparation of PrCo5 bulk magnets using nanograin powders made by surfactant-assisted high energy milling10.1063/1.3339777 ↗
13. Hard magnetic Sm2Fe17N3 flakes nitrogenized at lower temperature10.1016/j.jallcom.2012.11.153 ↗
14. Niobium-complex-based syntheses of sodium niobate nanowires possessing superior photocatalytic properties10.1021/ic902107u ↗
15. Lead-free piezoceramics10.1038/nature03028 ↗
16. Effect of different surfactants on the formation and morphology of SmCo5 nanoflakes10.1016/j.actamat.2011.07.035 ↗
17. Anisotropic SmCo5 flakes and nanocrystalline particles by high energy ball milling10.1063/1.3562447 ↗
18. Influence of octanoic acid on SmCo5 nanoflakes prepared by surfactant-assisted high-energy ball milling10.1016/j.jallcom.2010.05.123 ↗
19. The microstructure and magnetic properties of anisotropic polycrystalline Nd2Fe14B nanoflakes prepared by surfactant-assisted cryomilling10.1088/2053-1591/1/1/016106 ↗
20. Sm2Fe17Nx nanoflakes prepared by surfactant assisted cryomilling10.1063/1.4861204 ↗
21. Highly anisotropic SmCo5 nanoflakes by surfactant-assisted ball milling at low temperature10.1016/j.jmmm.2014.07.049 ↗
22. PrCo5 nanoflakes prepared by surfactant-assisted ball milling at low temperature10.1063/1.4918342 ↗
23. Structure and size-dependent properties of NdFeB nanoparticles and textured nano-flakes prepared from nanocrystalline ribbons10.1088/0022-3727/46/24/245003 ↗
24. The effect of particle size on coercivity and crystallinity of SmCo510.1063/1.3607958 ↗
25. Anisotropic nanostructured magnets by magnetic-field-assisted processing10.1063/1.3337656 ↗
26. Formation of SmCo5 single-crystal submicron flakes and textured polycrystalline nanoflakes10.1016/j.actamat.2010.09.060 ↗
27. Ball milling in the presence of a fluid: results and perspectives
28. Rare earth-cobalt hard magnetic nanoparticles and nanoflakes by high-energy milling10.1088/0953-8984/22/16/164213 ↗
29. El-Eskandarany · 2001
30. Progress in research of cryomilling
31. Textured resin-bonded Sm(Co, Fe, Cu)5 nanostructured magnets exploiting magnetic field and surfactant-assisted milling10.1016/j.jallcom.2008.09.211 ↗