Abstract

The present work investigates the structure, soft-magnetic and core-loss properties of 25 mm wide Fe 83Si 2B 9P 4Nb 1Cu 1 nanocrystalline ribbons. The melt-spun precursor ribbons of the thickness of 22 and 28 µm were prepared using commercial raw materials under ambient atmosphere. The XRD and DSC results show predominantly amorphous and hetero-amorphous structure for 22 and 28 µm ribbons in the as-quenched state. Further, the partial crystallization annealing leads to thickness dependent nanocrystallization process, wherein the thinner 22 µm ribbon shows sluggish primary(α-Fe(Si)) and delayed secondary(Fe 3(B 0.8P 0.2)) crystallization process compared to 28 µm ribbons. The difference is explained through as-quenched precursor matrix structure and selective solute re-distribution of the intergranular region during nanocrystallization. Moreover, the higher crystallite size (D) and volume fraction(V cr) of α-Fe(Si) nanocrystallites are observed for the 28 µm ribbon in the optimal annealing window. Under optimal annealing conditions, the 28 µm nanocrystalline ribbon (733 K) shows better AC soft-magnetic properties including B 800 of 1.62 T, H c of 15.7 A/m, B r/B s ratio ≥ 0.8 compared to B 800 of 1.59 T, H c of 17 A/m and B r/B s ratio ≥ 0.7 of 22 µm (743 K) ribbon. The 28 µm ribbon shows a low core loss ( P) of 0.34 W/kg under 50 Hz, 1.5 T compared to P > 0.65 W/kg for 22 µm ribbons. The lower core-loss behaviour of thicker 28 µm in the sub-kHz frequency regime has been explained based on the nanocrystalline microstructure and loss coefficients (hysteresis and eddy current). The work compares the AC core-loss properties with reported Fe-rich nanocrystalline alloys and also discusses the scope of improving B 800 beyond 1.65 T for the present alloys.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Magnetic Properties and Applications · Magnetic properties of thin films

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Advanced ferromagnetic materials in power electronic converters: A state of the art10.1109/ACCESS.2020.2982161 ↗
2. Applications of amorphous magnetic alloys10.1016/j.msea.2003.10.258 ↗
3. Review of Fe-6.5 wt%Si high silicon steel—A promising soft magnetic material for sub-kHz application10.1016/j.jmmm.2019.02.089 ↗
4. Soft magnetic properties of magnetic cores assembled with a high Bs Fe–based nanocrystalline alloy10.1109/TMAG.2016.2620118 ↗
5. Invar effects on some iron-base amorphous alloys10.1016/0304-8853(79)90194-X ↗
6. New Fe-based soft magnetic alloys composed of ultrafine grain structure10.1063/1.342149 ↗
7. Recent development of nanocrystalline soft magnetic alloys10.1016/0965-9773(95)00048-8 ↗
8. Modern soft magnets: Amorphous and nanocrystalline materials10.1016/j.actamat.2012.10.040 ↗
9. High Saturation Magnetization and Soft Magnetic Properties of bcc Fe-Zr-B and Fe-Zr-B-M (M = Transition Metal) Alloys with Nanoscale Grain Size10.2320/matertrans1989.32.93 ↗
10. Magnetic properties of nanocrystalline Fe82.65Cu1.35SixB16−x alloys (x=0–7)10.1063/1.2769956 ↗
11. New Fe-metalloids based nanocrystalline alloys with high Bs of 1.9 T and excellent magnetic softness10.1063/1.3058624 ↗
12. Three-dimensional atom probe analysis and magnetic properties of Fe85Cu1Si2B8P4melt spun ribbons10.1016/j.jmmm.2015.10.106 ↗
13. High B s Fe-based nanocrystalline alloy with high impurity tolerance10.1007/s10853-017-1557-9 ↗
14. Effects of Cu cluster evolution on soft magnetic properties of Fe83B10C6Cu1metallic glass in two-step annealing10.1016/j.jallcom.2016.08.150 ↗
15. Nanocrystalline soft magnetic materials from binary alloy precursors with high saturation magnetization10.1063/1.5079778 ↗
16. Effect of heating rate during primary crystallization on soft magnetic properties of melt-spun Fe-B alloys10.1016/j.scriptamat.2017.01.030 ↗
17. Structural Heterogeneity of the Melt-spun (Fe, Co)-Si-B-P-Cu Alloy with Excellent Soft Magnetic Properties10.1016/j.phpro.2015.12.154 ↗
18. Acta Materialia soft magnetic ribbons10.1016/j.actamat.2015.05.051 ↗
19. Crystallization and magnetic hardening behaviour of Fe-rich FeSiBNb(Cu) melt-spun alloys10.1016/j.jmmm.2020.166528 ↗
20. Role of P on amorphization, microstructure, thermo-physical and soft magnetic properties of Fe-rich FeB(P)SiNbCu melt-spun alloys10.1016/j.jmmm.2019.165723 ↗
21. Grain refinement in Fe-rich FeSiB(P)NbCu nanocomposite alloys through P compositional modulation10.1016/j.matlet.2021.129852 ↗
22. Magnetic properties of 120-mm wide ribbons of high Bs and low core-loss NANOMET® alloy10.1063/1.4913936 ↗
23. Fluxing purification and its effect on magnetic properties of high-BsFeBPSiC amorphous alloy10.1016/j.jmmm.2017.02.052 ↗
24. Vitrification and devitrification processes in metallic glasses10.1016/j.jallcom.2012.09.057 ↗
25. Surface oxidation of the Fe based amorphous ribbon annealed at temperatures below the glass transition temperature10.1016/j.jallcom.2014.08.160 ↗
26. Domains, domain walls and the coercive field of amorphous ferromagnets10.1051/jphys:019810042090128500 ↗
27. Enhanced magnetic softness of surface-crystallized Fe-Si-B-Nb-Mo-Cu amorphous alloys via competitive growth of surface pre-crystals/clusters10.1016/j.mseb.2021.115277 ↗
28. Competition driven nanocrystallization in high Bs and low coreloss Fe-Si-B-P-Cu soft magnetic alloys10.1016/j.scriptamat.2014.08.023 ↗
29. Cu clustering stage before the crystallization in Fe-Si-B-Nb-Cu amorphous alloys10.1016/S0965-9773(99)00219-6 ↗
30. Heating rate dependence of coercivity and microstructure of Fe–B–P–Cu nanocrystalline soft magnetic materials10.1016/j.jallcom.2020.157832 ↗
31. Nanocrystalline soft magnetic materials10.1016/0304-8853(95)01126-9 ↗
32. Magnetic-field-induced anisotropies and exchange softening in Fe-rich nanocrystalline soft magnetic alloys10.1016/j.scriptamat.2012.03.006 ↗
33. Anisotropies in soft magnetic nanocrystalline alloys10.1016/j.jmmm.2005.03.020 ↗
34. The impact of bending stress on magnetic properties of Finemet type microwires and ribbons10.1016/j.jallcom.2018.02.015 ↗
35. Interplay of uniform and random anisotropy in nanocrystalline soft magnetic alloys10.1016/j.actamat.2005.03.008 ↗
36. Magnetic Domains, Springer, Berlin Heidelberg, Berlin
37. Local random magnetocrystalline and macroscopic induced anisotropies in magnetic nanostructures10.1016/j.jnoncrysol.2008.06.118 ↗
38. Grain refinement mechanism of soft-magnetic alloys with nanocrystals embedded in amorphous matrix10.1016/j.jmrt.2020.01.093 ↗
39. Power-law behavior of coercivity in nanocrystalline magnetic alloys with grain-size distribution10.1016/j.scriptamat.2018.04.008 ↗
40. Design parameters for nanostructured soft magnetic alloys10.1109/TMAG.2013.2259149 ↗
41. Influence of microstructure on soft magnetic properties of low coreloss and high Bs Fe85Si2B8P 4Cu1 nanocrystalline alloy10.1063/1.4868188 ↗
42. General Properties of Power Losses in Soft Ferromagnetic Materials10.1109/20.43994 ↗
43. Connection between microstructure and magnetic properties of soft magnetic materials10.1016/j.jmmm.2008.04.001 ↗
44. Magnetostriction and magnetic core loss at high frequency in amorphous Fe-Nb-Si-B alloys10.1063/1.331888 ↗
45. Effect of latent heat during primary crystallization on the nanostructural formation process in nanocrystalline soft magnetic materials10.1063/1.5130427 ↗
46. Nano-crystallization of amorphous alloys by ultra-rapid annealing: An effective approach to magnetic softening10.1016/j.jallcom.2017.11.110 ↗
47. Microstructure, soft magnetic properties and applications of amorphous Fe-Co-Si-B-Mo-P alloy10.1063/1.5007781 ↗
48. Improvement of magnetic properties, microstructure and magnetic structure of Fe73.5Cu1Nb3Si15.5B7 nanocrystalline alloys by two-step annealing process10.1007/s10854-015-4216-4 ↗