Abstract

With the wide application of Ce-contained rare earth (RE) permanent magnets, recycling of wasted Ce-contained magnets has drawn more and more attention. Hydrogenation-disproportionation-desorption-recombination (HDDR) method was used to prepare anisotropic magnetic powder from wasted (Ce, Pr, Nd)-Fe-B sintered magnet (N45 magnet). The influence of hydrogen pressure in disproportionation ( P dis) and desorption ( P des) and the disproportionation time ( t dis) on the magnetic properties and microstructures of HDDR powders was studied. The P dis, P des and t dis were optimized to be 50 kPa, 5 kPa and 5 h, respectively. The optimized anisotropic HDDR (Ce, Pr, Nd)-Fe-B powder possessed the coercivity of 10.15 kOe, remanence of 11.14kG and the degree of alignment of 0.77. This coercivity has reached 83 % of that of the recycled N45 magnet. Microstructure examination with scanning electron microscope revealed that the optimized HDDR powder is consisted of flake-shaped particles with hierarchical structure. The distribution of rE-rich phase has been significantly influenced by P dis, P des and t dis. The optimized HDDR particles exhibited the best homogeneous distribution of rE-rich phase. The result of transparent electron microscopy (TEM) and energy dispersive spectrometry demonstrated the nature of (Ce, Pr, Nd)-rich phase and (Ce, Pr, Nd) 2Fe 14B for the rE-rich phase and RE 2Fe 14B grain phase, respectively. Examination with high-resolution TEM revealed that the optimized t dis resulted in the largest thickness of (Ce, Pr, Nd)-rich phase at grain boundaries and the consequent maximum coercivity of HDDR particles. The orientation of the optimized HDDR particles was analyzed with X-ray diffractometer and electron back-scatter diffractometer. The result revealed well textured HDDR particles and the subordinate nanograins with preferred (0 0 1) orientation, suggesting the inherited texture of these HDDR particles from the initial (Ce, Pr, Nd) 2Fe 14B grains in N45 sintered magnet. This HDDR method was proved to be a prospective strategy in recycling of Ce-contained sintered magnets.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Hydrogen Storage and Materials · Rare-earth and actinide compounds

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Improving magnetic properties in mischmetal-based sintered composite magnets by regulating element distribution
2. Core–shell Y-substituted Nd–Ce–Fe–B sintered magnets with enhanced coercivity and good thermal stability10.1063/1.4982679 ↗
3. Special microstructure evolution and enhanced magnetic properties of Ce-Fe-B-based spark plasma sintered magnets with core-shell structure by NdCu addition10.1016/j.jallcom.2018.10.114 ↗
4. Magnetic properties of bulk, and rapidly solidified nanostructured (Nd1-xCex)2Fe14-yCoyB ribbons10.1016/j.actamat.2015.09.049 ↗
5. Microstructure and Magnetic Properties of Recycled Nd–Fe–B Magnets with Blending of Ce-Rich Alloy10.1109/TMAG.2017.2704091 ↗
6. Ralph, Cerium: an unlikely replacement of dysprosium in high performance Nd-Fe-B permanent magnets10.1002/adma.201404892 ↗
7. High performance (La, Ce, Pr, Nd)-Fe-B die-upset magnets based on misch-metal10.1016/j.jallcom.2017.06.290 ↗
8. Development of Ce-based sintered magnets: review and prospect10.1007/s42243-019-00287-x ↗
9. Recycling of rare earths: a critical review10.1016/j.jclepro.2012.12.037 ↗
10. Direct reuse of rare earth permanent magnets—coating integrity10.1109/TMAG.2016.2636804 ↗
11. The Hydrogen Ductilisation Process (HyDP) for shaping NdFeB magnets10.1016/j.jallcom.2016.12.177 ↗
12. Recovery of rare earth elements from NdFeB magnet by mono- and bifunctional mesoporous silica: Waste recycling strategies and perspectives10.1016/j.hydromet.2022.105855 ↗
13. A. Ikram, M.F. Mehmood, M. Podlogar, A. Eldosouky, R.S. Sheridan, M. Awais, A. Walton, M. Kržmanc, T. Tomse, S. Kobe, S. Sturm, K. Žužek Rožman, The sintering mechanism of fully dense and highly coercive Nd-Fe-B magnets from the recycled HDDR powders reprocessed by spark plasma sintering, J. Alloys Compd. 774 (2019) 1195, https://doi.org/10.1016/j.jallcom.2018.09.322.10.1016/j.jallcom.2018.09.322 ↗
14. The use of hydrogen to separate and recycle neodymium–iron–boron-type magnets from electronic waste10.1016/j.jclepro.2015.05.033 ↗
15. Magnetic properties and microstructures of the Nd-Fe-B magnet powder produced by hydrogen treatment10.1063/1.349232 ↗
16. Possible methods of recycling NdFeB-type sintered magnets using the HD/degassing process10.1016/j.jallcom.2007.01.134 ↗
17. Anisotropic powder from sintered NdFeB magnets by the HDDR processing route10.1016/j.jmmm.2011.07.043 ↗
18. Neutron-diffraction study of the insertion scheme of hydrogen in Nd2Fe14B10.1063/1.360720 ↗
19. Properties of hydrogenation-disproportionation-desorption-recombination NdFeB powders prepared from recycled10.1063/1.3677761 ↗
20. ChemInform Abstract: Disproportionation in Nd16Fe76B8-Type Hydrides.10.1002/chin.199045011 ↗
21. A systematic study of HDDR processing conditions for the recycling of end-of-life Nd-Fe-B magnets10.1016/j.jallcom.2017.06.319 ↗
22. Hydrogenation, disproportionation and desorption (HDD): An effective processing route for Nd-Fe-B-type magnets10.1016/0022-5088(90)90071-Q ↗
23. Recycling Used Nd-Fe-B Sintered Magnets via a Hydrogen-Based Route to Produce Anisotropic10.1002/aenm.201200337 ↗
24. Effect of hydrogen pressure on anisotropy of HDDR-treated Nd–Fe–B-type powder10.1016/j.jmmm.2006.01.145 ↗
25. Texture memory effect of Nd–Fe–B during hydrogen treatment, Journal of Magnetism and Magnetic Materials10.1016/j.jmmm.2004.11.423 ↗
26. O, Gutfleisch, HDDR treatment of Ce-substituted Nd2Fe14B-based permanent magnet alloys - phase structure evolution, intergranular processes and magnetic property development10.1016/j.jallcom.2019.152215 ↗
27. Anisotropic characteristic in HDDR Nd13Fe80B7
28. Effect of hydrogen pressure on disproportionation kinetics of Nd-Fe-B alloy10.1016/j.jallcom.2009.07.173 ↗
29. Effect of Processing Hydrogen Pressure on Magnetic Properties of HDDR Nd-Fe-B Magnet
30. Influence of RE-rich phase distribution in initial alloy on anisotropy of HDDR powders10.1088/1674-1056/24/9/097505 ↗
31. Magnetic property and microstructure of single crystalline Nd2Fe14B ultrafine particles ball milled from HDDR powders10.1016/j.jmmm.2013.02.044 ↗
32. Origin of anisotropy for the HDDR Nd13.5Fe79.5B7 magnetic powders
33. Texture in a ternary Nd16.2Fe78.2B5.6 powder using a modified hydrogenation–disproportionation–desorption–recombination process10.1016/S0304-8853(99)00702-7 ↗
34. The effect of Nd-Cu diffusion during hot pressing and hot deformation on the coercivity and the deformation ability of Nd-Fe-B HDDR magnets10.1016/j.jmmm.2017.04.031 ↗
35. Simultaneous enhancement in coercivity and remanence of Nd2Fe14B permanent magnet by grain boundary diffusion process using NdHx, Current
36. Mechanism of the texture development in hydrogen-disproportionation–desorption-recombination (HDDR) processed Nd-Fe-B powders10.1016/j.actamat.2014.11.003 ↗
37. Coercivity enhancement of hydrogenation–disproportionation–desorption–recombination processed Nd–Fe–B powders by the diffusion of Nd–Cu eutectic alloys10.1016/j.scriptamat.2010.08.021 ↗
38. Direct observation of texture memory in hydrogenation–disproportionation–desorption–recombination processed Nd-Fe-B magnets using electron backscatter diffraction10.1016/j.scriptamat.2015.12.023 ↗