journal article·2024-12

High-performance anisotropic Sm2Co17/Fe(Co) bulk nanocomposite magnets fabricated by two-step high-pressure thermal compression deformation

Tiancong Li, Jieqiong Gao, Xiaohong Li, Jinyi wang, Li Lou, Yingxin Hua, Yiran Li, Wenyue Qin, Defeng Guo, Wei Li

Publisher page

Abstract

In the realm of Sm 2Co 17 nanocomposite magnetic materials, it remains a challenge to fabricate anisotropic magnets by forming nanocrystalline Sm 2Co 17 phases with strong texture, alongside soft phases of small size and high soft phase content. In this paper, we present a novel approach for fabricating anisotropic Sm 2Co 17/Fe(Co) nanocomposite bulk magnets with a prominent (00 l) texture of the Sm 2Co 17 phase, the 25 wt% content of the Fe(Co) phase, and a refined grain size of 25 nm. This fabrication is achieved using a two-step high-pressure thermal compression (HPTC) deformation process. The fabricated magnets exhibit a maximum energy product [( BH) max] of 20.0 MGOe with a pronounced magnetic anisotropy ( B r /// B r ⊥ = 1.23). This result is 53 % higher than the previously reported largest value [( BH) max = 13.1 MGOe] for Sm 2Co 17-based nanocomposites. The magnets also exhibit a low remanence temperature coefficient ( α = −0.014 %/°C) and a low coercivity temperature coefficient ( β = −0.23 %/°C), demonstrating exceptional thermal stability. Our findings may improve the fabrication of anisotropic bulk Sm 2Co 17 nanostructure magnets for practical applications.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Hydrogen Storage and Materials · Metallurgical and Alloy Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. The pull of stronger magnets10.1038/472022a ↗
2. Fabrication of bulk nanostructured permanent magnets with high energy density: challenges and approaches10.1039/C6NR09464C ↗
3. Influence mechanism of Fe content on the magnetic properties of Sm2Co17-type sintered magnets: microstructure and microchemistry10.1016/j.jallcom.2019.152908 ↗
4. Atomic structure and domain wall pinning in samarium-cobalt-based permanent magnets10.1038/s41467-017-00059-9 ↗
5. Optimization of both coercivity and knee-point magnetic field of Sm2Co17-type magnets via solid solution process10.1016/j.jre.2019.11.009 ↗
6. A family of new cobaltbase permanent magnet materials10.1063/1.1709459 ↗
7. A new class of Sm-TM magnets for operating temperatures up to 550 °C10.1109/20.908807 ↗
8. Attractive-domain-wall-pinning controlled Sm-Co magnets overcome the coercivity-remanence trade-off10.1016/j.actamat.2018.10.046 ↗
9. SmCo (2:17-type) magnets with high contents of Fe and light rare earths10.1063/1.355424 ↗
10. Strong magnets by self-assembly10.1038/420374a ↗
11. Meltspun permanent magnet materials containing Fe3B as the main phase10.1016/0304-8853(89)90333-8 ↗
12. The exchange-spring magnet: a new material principle for permanent magnets10.1109/20.102931 ↗
13. Heterostructures: new opportunities for functional materials10.1080/21663831.2019.1691668 ↗
14. Magnetic properties of hard/soft composites: SmCo5/Co1-xFex10.1103/PhysRevB.58.12071 ↗
15. Nanocomposite Sm2Co17/Co permanent magnets by mechanical alloying10.1063/1.362121 ↗
16. Fully dense bulk nanocomposites of (Sm1-xGdx)2(Co1-yFey)17+ (Co, Fe) with high coercivity and high curie temperature10.1109/TMAG.2004.830398 ↗
17. Fully dense anisotropic nanocomposite Sm (Co, Fe, Zr, Cu, B) z (z = 7.5–12) magnets10.1063/1.1851432 ↗
18. Sm2Co17 nanoparticles synthesized by surfactant-assisted high energy ball milling10.1016/j.jallcom.2012.06.011 ↗
19. Microstructure and magnetic properties of uncoupled Sm2Co17–Cu nanocomposites10.1063/1.1461070 ↗
20. Spark plasma sintered Sm2Co17-FeCo nanocomposite permanent magnets synthesized by high energy ball milling10.1088/0957-4484/19/33/335701 ↗
21. Hot-deformed Sm–Co/Co composite magnets fabricated from powder blends10.1063/1.3334493 ↗
22. Strong magnets with ordered structures10.1080/21663831.2021.2008541 ↗
23. Perspective and prospects for ordered functional materials10.1002/advs.202300193 ↗
24. Fast fabrication of a hierarchical nanostructured multifunctional ferromagnet10.1126/science.adp2328 ↗
25. Novel bimorphological anisotropic bulk nanocomposite materials with high energy products10.1002/adma.201606430 ↗
26. Development of crystallography texture in SmCo7/a-Fe nanocomposite magnets prepared by high-pressure thermal compression10.1016/j.jallcom.2018.03.363 ↗
27. Fabrication and magnetic properties of anisotropic SmCo3/Fe(Co) bulk nanocomposite magnets10.1063/5.0078533 ↗
28. Anisotropic bulk Nd2Fe14B/α-Fe nanohybrid magnets with an enhanced energy product10.1016/j.matlet.2018.01.104 ↗
29. Controllably manipulating three-dimensional hybrid nanostructures for bulk nanocomposites with large energy products10.1021/acs.nanolett.7b00264 ↗
30. Magnetism and phase stability of R(Co, M)7 pseudobinary intermetallics with TbCu7-type structure10.1063/1.2432103 ↗
31. Enhancement of anisotropy energy of SmCo5 by ceasing the coupling at 2c sites in the crystal lattice with Cu substitution10.1038/s41598-021-89331-z ↗
32. Nanocrystalline Sm12.5(Co, Zr)87.5 magnets: synthesis and magnetic properties10.1016/S0304-8853(01)00978-7 ↗
33. Effects of Zr, Nb, and Cu substitutions on magnetic properties of melt-spun and hot deformed bulk anisotropic nanocomposite SmCo type magnets10.1063/1.2831334 ↗
34. Concurrent ordering and phase transformation in SmCo7 nanograins10.1039/C5NR02592C ↗
35. Influence of intermediate-heat treatment on the structure and magnetic properties of iron-rich Sm(CoFeCuZr)Z sintered magnets10.1063/1.4906757 ↗
36. Magnetic materials and devices for the 21st century: stronger, lighter, and more energy efficient10.1002/adma.201002180 ↗
37. Fully dense Sm-Co-Fe-Cu and Sm-Co-Fe-Ga nanocomposite magnets by hot compaction10.1109/TMAG.2004.832162 ↗
38. Demagnetizing factors for cylinders10.1109/20.102932 ↗
39. Chikazumi · 1997 · 15