journal article·2014

Investigation into the effect of Fe-site substitution on the performance of Sr 2 Fe 1.5 Mo 0.5 O 6−δ anodes for SOFCs

Jie Feng, Guoquan Yang, Ningning Dai, Zhenhua Wang, Wang Sun, David Rooney, Jinshuo Qiao, Kening Sun

J. Mater. Chem. A· Volume 2· Issue 41
Publisher page

Abstract

The unstable temperature for Sr 2 Fe 1.5−x Ni x Mo 0.5 O 6−δ materials in H 2 decreases with the increase of Ni content. Egressed Ni particles were detected in samples with a higher Ni content ( x > 0.1). Sr 2 Fe 1.4 Ni 0.1 Mo 0.5 O 6−δ shows the highest electronic conductivity of 20.6 S cm −1 at 800 °C.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Beijing Key Laboratory for Chemical Power Source and Green Catalysis

School of Chemical Engineering and Environment

Beijing Institute of Technology

Beijing, China

School of Chemistry and Chemical Engineering

Queen's University Belfast

Belfast, UK

References (34)

Show source-provided references
1. Zhan · Science · 2005 · 308 · 84410.1126/science.1109213 ↗
2. Ormerod · Chem. Soc. Rev. · 2003 · 32 · 1710.1039/b105764m ↗
3. Atkinson · Nat. Mater. · 2004 · 3 · 1710.1038/nmat1040 ↗
4. Yang · Science · 2009 · 326 · 12610.1126/science.1174811 ↗
5. Xie · Int. J. Hydrogen Energy · 2011 · 36 · 725710.1016/j.ijhydene.2011.03.075 ↗
6. Goodenough · J. Power Sources · 2007 · 173 · 110.1016/j.jpowsour.2007.08.011 ↗
7. Kan · Catal. Commun. · 2010 · 12 · 3610.1016/j.catcom.2010.07.014 ↗
8. Zha · Electrochem. Solid-State Lett. · 2005 · 8 · A40610.1149/1.1945370 ↗
9. Huang · Science · 2006 · 312 · 25410.1126/science.1125877 ↗
10. Vasala · J. Solid State Chem. · 2010 · 183 · 100710.1016/j.jssc.2010.03.004 ↗
11. Marrero-López · Mater. Res. Bull. · 2008 · 43 · 244110.1016/j.materresbull.2007.07.032 ↗
12. Kurokawa · J. Power Sources · 2007 · 164 · 51010.1016/j.jpowsour.2006.11.048 ↗
13. Jiang · J. Mater. Sci. · 2004 · 39 · 440510.1023/B:JMSC.0000034135.52164.6b ↗
14. Tao · J. Electrochem. Soc. · 2004 · 151 · A25210.1149/1.1639161 ↗
15. Wan · Solid State Ionics · 2006 · 177 · 121110.1016/j.ssi.2006.04.046 ↗
16. Huang · J. Electrochem. Soc. · 2006 · 153 · A126610.1149/1.2195882 ↗
17. Liu · Adv. Mater. · 2010 · 22 · 547810.1002/adma.201001044 ↗
18. He · J. Electrochem. Soc. · 2012 · 159 · B61910.1149/2.020206jes ↗
19. Xiao · Electrochem. Commun. · 2011 · 13 · 5710.1016/j.elecom.2010.11.012 ↗
20. Cho · Energy Environ. Sci. · 2013 · 6 · 185010.1039/c3ee23791e ↗
21. Dai · J. Power Sources · 2013 · 243 · 76610.1016/j.jpowsour.2013.05.168 ↗
22. Dai · J. Mater. Chem. A · 2013 · 1 · 1414710.1039/c3ta13607h ↗
23. Akbari-Fakhrabadi · J. Alloys Compd. · 2012 · 541 · 110.1016/j.jallcom.2012.06.036 ↗
24. Kobsiriphat · J. Electrochem. Soc. · 2010 · 157 · B27910.1149/1.3269993 ↗
25. Salerno · Appl. Clay Sci. · 2003 · 23 · 28710.1016/S0169-1317(03)00128-5 ↗
26. Xiao · J. Power Sources · 2012 · 201 · 4310.1016/j.jpowsour.2011.10.103 ↗
27. Klimova · Appl. Catal., A · 2003 · 240 · 2910.1016/S0926-860X(02)00417-9 ↗
28. Xiao · J. Power Sources · 2012 · 202 · 6310.1016/j.jpowsour.2011.11.021 ↗
29. Gu · J. Power Sources · 2008 · 183 · 47110.1016/j.jpowsour.2008.05.053 ↗
30. Lo Faro · Biomass Bioenergy · 2011 · 35 · 107510.1016/j.biombioe.2010.11.018 ↗
31. Biesinger · Appl. Surf. Sci. · 2011 · 257 · 271710.1016/j.apsusc.2010.10.051 ↗
32. Yamashita · Appl. Surf. Sci. · 2008 · 254 · 244110.1016/j.apsusc.2007.09.063 ↗
33. Zhang · J. Power Sources · 2010 · 195 · 635610.1016/j.jpowsour.2010.04.021 ↗
34. Muñoz-García · J. Am. Chem. Soc. · 2012 · 134 · 682610.1021/ja300831k ↗