journal article·2017-01

Impact of moisture content on dynamic mechanical properties and transition temperatures of wood

Oleg V. Startsev, Alexey Makhonkov, Vladimir Erofeev, Sergei Gudojnikov

Publisher page

Abstract

The dynamic shear modulus and the loss modulus of Betula alba, Ulmus parvifolia, Quercus robur, Acer platanoides, Tilia cordata, Fraxinus excelsior and Pinus sylvestris wood were measured using an inverted torsion pendulum within a wide temperature range. The glass transition temperature of the lignin–carbohydrate complex and the decomposition temperature of the wood cellulose were estimated. The temperature band from 170°C to 240°С shows the transition of the lignin–cellulose complex from the glassy to the rubbery state. Mechanical properties of different types of wood are affected by moisture and anatomical differences, but glass transition and decomposition temperatures are the same. More than 5% of moisture in the wood stored at normal conditions were found. After drying, the increase of dynamic shear modulus of wood over the entire region of the glassy state was observed. The intensity of maximum peak of dynamic loss modulus is also increased due to activation of the segmental motion of macromolecules of the ligno-carbon complex. The decomposition temperature of the cellulose crystallites was unchanged for specimens containing moisture and for dried specimens.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Bamboo properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. ASTM E1640-09. · 2009
2. 10.1023/A:101798611955910.1023/A:1017986119559 ↗
3. 10.1080/17480272.2012.70166610.1080/17480272.2012.701666 ↗
4. Behzad, M. · IJE Transactions B · 2004 · 17 · 95-104
5. Beusheva O. S. · Polzunovsky Vestnik · 2009 · 3 · 297-300
6. Birkinshaw, C. · Journal of Material Science · 1986 · 5 · 89
7. 10.1021/bm400080f10.1021/bm400080f ↗
8. 10.1515/hf-2011-016710.1515/hf-2011-0167 ↗
9. 10.1007/s00226-012-0514-710.1007/s00226-012-0514-7 ↗
10. 10.1134/1.159131910.1134/1.1591319 ↗
11. Filistovich D. V. · Pribory & Tekhnika Eksperimenta · 2003 · 46 · 163
12. Horvath, B. · BioResources · 2011 · 6 · 212510.15376/biores.6.2.2125-2134 ↗
13. 10.1016/j.compositesa.2012.01.00710.1016/j.compositesa.2012.01.007 ↗
14. 10.1016/j.compositesa.2011.11.00110.1016/j.compositesa.2011.11.001 ↗
15. 10.1080/17480272.2013.86925610.1080/17480272.2013.869256 ↗
16. Lisperguer, J. · Wood Research · 2009 · 54 · 31
17. 10.1080/17480272.2012.70768610.1080/17480272.2012.707686 ↗
18. Ornaghi H. L., · Journal of Applied Polymer Science · 2010 · 118 · 88710.1002/app.32388 ↗
19. 10.1515/HF.2007.09310.1515/HF.2007.093 ↗
20. 10.1007/BF0036650110.1007/BF00366501 ↗
21. Shakhzadyan E. A. · 1992 · 34 · 3
22. 10.1002/pc.1007610.1002/pc.10076 ↗
23. Startsev O. V. · Polymer Composites · 1998 · 6 · 48110.1177/147823919800600707 ↗
24. 10.1080/0091403970803148310.1080/00914039708031483 ↗
25. 10.1007/s00226005010010.1007/s002260050100 ↗
26. Tabet T. A. · Journal of Nuclear and Related Technologies · 2009 · 6 · 71
27. Tamer, A. · 2013 · 113
28. 10.4236/msa.2012.3504710.4236/msa.2012.35047 ↗
29. 10.1080/0277381080234697610.1080/02773810802346976 ↗